# US 9,356,282 B2 · Method of manufacture of homodispersed silicon carbide-derived carbon composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,282 B2
- Document ID: US9356282B2
- Status: Granted
- Kind: B2
- Application number: 13/822,951
- Filed: 2011-09-13
- Published: 2013-09-19
- Granted: 2016-05-31
- Earliest claimed: 2010-09-13
- Assignees: OÜ Skeleton Technologies Group
- Applicants: Jaan Leis; Mati Arulepp
- Inventors: Jaan Leis; Mati Arulepp
- Web page: https://patentgrep.com/patent/US9356282B2

## CPC

- C01B 32/984: Preparation from elemental silicon
- C04B 35/62834: {Silicon carbide}
- C04B 35/62839: {Carbon}
- C04B 35/62892: {with a coating layer consisting of particles}
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/587: for inserting or intercalating light metals
- C04B 2235/428: Silicon
- H01B 1/04: mainly consisting of carbon-silicon compounds, carbon or silicon
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention concerns a method of manufacture of the homodispersed composite of the synthetic carbon material derived from carbide and silicon where the powder of the carbon material is first dispersed mechanically with the powder of silicon to homodispersed mixture, then the homodispersed mixture of the carbon material and silicon is sintered in an inert environment at a temperature between 1200 to 1500° C. to synthetic homodispersed composite of the silicon carbide and silicon. The homodispersed composite of the silicon carbide and silicon is heated in an inert environment at a temperature between 800 to 1100° C. and then the homodispersed composite of the silicon carbide and silicon is chlorinated at a temperature from 800 to 100° C.

## Claims

### Claim 1

A method for preparing a carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon that comprises stages, comprising:
heating a homogeneous composite comprising silicon particles encapsulated in a metal carbide or non-metal carbide case in an inert environment at temperatures between 300 to 1100° C.; and thereafter
chemically processing the homogeneous composite comprising silicon particles encapsulated in a metal carbide or non-metal carbide case at temperatures between 300 to 1100° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the step of chemical processing is used for extraction of atoms of a metal or non-metal from a metal carbide or non-metal carbide case surrounding silicon particles in said homogenous composite and is conducted in a gaseous halogen environment at temperatures between 300 to 1100° C.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the step of chemical processing in a gaseous halogen environment is chlorination of a homogeneous composite comprising silicon particles encapsulated in a metal carbide or non-metal carbide case at temperatures at 300 to 1100° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the inert environment is argon.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the homogeneous composite comprising silicon particles encapsulated in a non-metal carbide case is a composite that is prepared through stages, comprising:
mechanically dispersing a powder of carbon material with silicon powder into a homogeneous mixture; thereafter
sintering the homogeneous mixture of carbon material and silicon in inert environment at 1200 to 1500° C. to obtain the composite comprising silicon particles encapsulated in a silicon carbide case.

### Claim 6 (depends on 1)

The method for preparing a carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon according to claim 1, wherein:
the step of heating a homogeneous composite comprising silicon particles encapsulated in silicon carbide in an inert environment occurs at temperatures between 800 to 1100° C.; and thereafter
the step of chemically processing comprises chlorinating the homogeneous composite comprising silicon particles encapsulated in silicon carbide at 800 to 1100° C.

### Claim 7 (depends on 6)

The method according to claim 6, further comprising preparing the homogeneous composite, comprising:
mechanically dispersing a carbon material powder into a homogeneous mixture with silicon powder; and thereafter
sintering the homogeneous mixture of carbon material and silicon in an inert environment at 1200 to 1500° C. to obtain a homogeneous composite comprising silicon particles encapsulated in synthetic carbide.

### Claim 8 (depends on 6)

The method according to claim 6, further comprising after chlorination, processing the carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon in a reducing environment at 600 to 900° C.

### Claim 9 (depends on 7)

The method according to claim 7, further comprising after chlorination, processing the carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon in a reducing environment at 800° C.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the reducing environment is hydrogen or ammonia.

### Claim 11 (depends on 6)

The method according to claim 6, further comprising after chlorination, treating the carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon in an inert environment at least at 1000° C.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the inert environment is argon.

### Claim 13 (depends on 6)

The method according to claim 6, further comprising after chlorination, processing the carbon-encapsulated silicon composite of carbide derived synthetic carbon material and silicon in an oxidative environment at 550 to 1000° C.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the oxidative environment is oxygen, water, air, or carbon dioxide.