# US 9,356,239 B2 · Method for manufacturing high resolution AMOLED backplane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,239 B2
- Document ID: US9356239B2
- Status: Granted
- Kind: B2
- Application number: 14/390,026
- Filed: 2014-08-21
- Published: 2016-02-11
- Granted: 2016-05-31
- Earliest claimed: 2014-08-07
- Assignees: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Applicants: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Inventors: Yuanjun Hsu
- Web page: https://patentgrep.com/patent/US9356239B2

## CPC

- H10D 86/481: {integrated with passive devices, e.g. auxiliary capacitors}
- H10D 30/6719: {having significant overlap between the lightly-doped drains and the gate electrodes, e.g. gate-overlapped LDD [GOLDD] TFTs}
- H10D 86/0221: {comprising manufacture, treatment or patterning of TFT semiconductor bodies}
- H10D 86/60: wherein the TFTs are in active matrices
- H10K 59/1213: {the pixel elements being TFTs}
- H10K 71/30: Doping active layers, e.g. electron transporting layers
- H10K 59/1201: {Manufacture or treatment}
- H10K 71/00: Manufacture or treatment specially adapted for the organic devices covered by this subclass
- H10K 71/233: {by photolithographic etching}
- H10K 71/60: Forming conductive regions or layers, e.g. electrodes
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present invention relates to a method for manufacturing a high resolution AMOLED backplane. The method includes: step 10: forming a first buffer layer on a substrate; step 20: forming a low temperature poly-silicon layer on the first buffer layer; step 30: patternizing the low temperature poly-silicon layer; step 40: forming a gate insulation layer, arranging a proper photoresist mask on the gate insulation layer to correspond to TFT source/drain areas and a storage capacitor area, and subjecting the patternized low temperature poly-silicon layer to a first P+ ion doping operation; step 50: forming a gate terminal and subjecting the patternized low temperature poly-silicon layer to a second P+ ion doping operation by using the gate terminal as a hard mask; and step 60: forming a first insulation layer on the gate terminal and forming source/drain terminals on the first insulation layer so that the source/drain terminals are in contact with portions of the TFT source/drain areas that are subjected to both the first P+ ion doping operation and the second P+ ion doping operation through a contact window. The method for manufacturing a high resolution AMOLED backplane of the present invention improves the design rules so as to increase panel resolution and reduce the contact resistance of source/drain terminals and P+ doping zones.

## Claims

### Claim 1

A method for manufacturing a high resolution active matrix organic light emitting diode (AMOLED) backplane, comprising:
Step 10: forming a first buffer layer on a substrate;
Step 20: forming a low temperature poly-silicon layer on the first buffer layer;
Step 30: patternizing the low temperature poly-silicon layer to form a patternized low temperature poly-silicon layer that include a storage capacitor area and TFT source/drain areas and channel areas;
Step 40: forming a gate insulation layer on the patternized low temperature poly-silicon layer, arranging a proper photoresist mask on the gate insulation layer to correspond to the TFT source/drain areas and the storage capacitor area, and subjecting the patternized low temperature poly-silicon layer to a first P+ ion doping operation through the proper photoresist mask to form a first concentration doped portion at each of TFT source/drain areas and the storage capacitor area;
Step 50: forming a gate metal layer on the gate insulation layer, patternizing the gate metal layer to form a gate terminal, subjecting the first concentration doped portions of the TFT source/drain areas of the patternized low temperature poly-silicon layer to a second P+ ion doping operation by using the gate terminal as a hard mask so as to form a second, higher concentration doped portion in a portion of each of the first concentration doped portions of the TFT source/drain areas, wherein the second concentration portions are subjected to both the first and second P+ ion doping operations; and
Step 60: forming a first insulation layer on the gate terminal, forming source/drain terminals on the first insulation layer, wherein the source/drain terminals are in contact with the second concentration doped portions of the TFT source/drain areas through a contact window.

### Claim 2 (depends on 1)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 1, wherein the second P+ ion doping operation implant P+ ions in the patternized low temperature poly-silicon layer to a depth greater than that of the first P+ ion doping operation.

### Claim 3 (depends on 1)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 1 further comprising forming a second buffer layer between the first buffer layer and the low temperature poly-silicon layer.

### Claim 4 (depends on 1)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 1 further comprising forming a second insulation layer between the first insulation layer and the source/drain terminals.

### Claim 5 (depends on 1)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 1 further comprising forming a planarization layer on the source/drain terminals.

### Claim 6 (depends on 5)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 5 further comprising forming an electrode layer on the planarization layer.

### Claim 7 (depends on 6)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 6 further comprising forming an organic layer on the electrode layer.

### Claim 8 (depends on 7)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 7 further comprising forming spacers on the organic layer.

### Claim 9 (depends on 1)

The method for manufacturing a high resolution AMOLED backplane as claimed in claim 1, wherein the gate terminal comprises molybdenum.

### Claim 10

A method for manufacturing a high resolution active matrix organic light emitting diode (AMOLED) backplane, comprising:
Step 10: forming a first buffer layer on a substrate;
Step 20: forming a low temperature poly-silicon layer on the first buffer layer;
Step 30: patternizing the low temperature poly-silicon layer to form a patternized low temperature poly-silicon layer that include a storage capacitor area and TFT source/drain areas and channel areas;
Step 40: forming a gate insulation layer on the patternized low temperature poly-silicon layer, arranging a proper photoresist mask on the gate insulation layer to correspond to the TFT source/drain areas and the storage capacitor area, and subjecting the patternized low temperature poly-silicon layer to a first P+ ion doping operation through the proper photoresist mask to form a first concentration doped portion at each of TFT source/drain areas and the storage capacitor area;
Step 50: forming a gate metal layer on the gate insulation layer, patternizing the gate metal layer to form a gate terminal, subjecting the first concentration doped portions of the TFT source/drain areas of the patternized low temperature poly-silicon layer to a second P+ ion doping operation by using the gate terminal as a hard mask so as to form a second, higher concentration doped portion in a portion of each of the first concentration doped portions of the TFT source/drain areas, wherein the second concentration portions are subjected to both the first and second P+ ion doping operations; and
Step 60: forming a first insulation layer on the gate terminal, forming source/drain terminals on the first insulation layer, wherein the source/drain terminals are in contact with the second concentration doped portions of the TFT source/drain areas that are subjected to both the first P+ ion doping operation and the second P+ ion doping operation through a contact window;
wherein the second P+ ion doping operation implant P+ ions in the patternized low temperature poly-silicon layer to a depth greater than the first P+ ion doping operation;
the method for manufacturing a high resolution AMOLED backplane further comprising forming a second buffer layer between the first buffer layer and the low temperature poly-silicon layer;
the method for manufacturing a high resolution AMOLED backplane further comprising forming a second insulation layer between the first insulation layer and the source/drain terminals;
the method for manufacturing a high resolution AMOLED backplane further comprising forming a planarization layer on the source/drain terminals;
the method for manufacturing a high resolution AMOLED backplane further comprising forming an electrode layer on the planarization layer;
the method for manufacturing a high resolution AMOLED backplane further comprising forming an organic layer on the electrode layer;
the method for manufacturing a high resolution AMOLED backplane further comprising forming spacers on the organic layer; and
wherein the gate terminal comprises molybdenum.