# US 9,356,235 B2 · Structure and formation method of memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,235 B2
- Document ID: US9356235B2
- Status: Granted
- Kind: B2
- Application number: 14/474,931
- Filed: 2014-09-02
- Published: 2015-10-01
- Granted: 2016-05-31
- Earliest claimed: 2014-03-25
- Assignees: Winbond Electronics Corp.
- Applicants: Winbond Electronics Corp.
- Inventors: Po-Yen Hsu; Hsiu-Han Liao; Shuo-Che Chang; Chia Hua Ho
- Web page: https://patentgrep.com/patent/US9356235B2

## CPC

- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N 70/023: {by chemical vapor deposition, e.g. MOCVD, ALD}
- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Structures and formation methods of memory devices are provided. The memory device includes a first electrode, a second electrode, and a resistive layer positioned between the first electrode and the second electrode. The resistive layer has a crystalline portion. A volume ratio of the crystalline portion to the resistive layer is in a range from about 0.2 to about 1.

## Claims

### Claim 1

A memory device, comprising:
a first electrode;
a second electrode; and
a resistive layer positioned between the first electrode and the second electrode, wherein the resistive layer has a crystalline portion, and a volume ratio of the crystalline portion to the resistive layer is in a range from about 0.2 to about 1.

### Claim 2 (depends on 1)

The memory device as claimed in claim 1, wherein the crystalline portion comprises a plurality of crystalline grains.

### Claim 3 (depends on 2)

The memory device as claimed in claim 2, wherein an average grain size of the crystalline grains is in a range from about 2 nm to about 50 nm.

### Claim 4 (depends on 1)

The memory device as claimed in claim 1, wherein the resistive layer comprises hafnium oxide.

### Claim 5 (depends on 1)

The memory device as claimed in claim 1, wherein the crystalline portion comprises a plurality of crystalline grains, and the crystalline grains have a crystalline phase of monoclinic phase.

### Claim 6 (depends on 1)

The memory device as claimed in claim 1, wherein the crystalline portion comprises a plurality of crystalline grains, and the crystalline grains are surrounded by an amorphous portion of the resistive layer.

### Claim 7 (depends on 6)

The memory device as claimed in claim 6, wherein the crystalline grains are separated from each other.

### Claim 8 (depends on 6)

The memory device as claimed in claim 6, wherein some of the crystalline grains connect with each other.

### Claim 9 (depends on 6)

The memory device as claimed in claim 6, wherein some of the crystalline grains are separated from each other.

### Claim 10 (depends on 1)

The memory device as claimed in claim 1, wherein the resistive layer comprises aluminum oxide, zirconium oxide, titanium oxide, tantalum oxide, tungsten oxide, zinc oxide, nickel oxide, copper oxide, or a combination thereof.

### Claim 11

A memory device, comprising:
a first electrode;
a second electrode; and
a resistive layer positioned between the first electrode and the second electrode, wherein the resistive layer has a crystalline portion, and an area ratio of the crystalline portion to the resistive layer is in a range from about 0.2 to about 1.

### Claim 12 (depends on 11)

The memory device as claimed in claim 11, wherein the crystalline portion comprises a plurality of crystalline grains.

### Claim 13 (depends on 11)

The memory device as claimed in claim 11, wherein an average grain size of the crystalline grains is in a range from about 2 nm to about 50 nm.

### Claim 14 (depends on 11)

The memory device as claimed in claim 11, wherein the crystalline portion comprises a plurality of crystalline grains, and the crystalline grains are surrounded by an amorphous portion of the resistive layer.