# US 9,356,162 B2 · High efficiency group III-V compound semiconductor solar cell with oxidized window layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,162 B2
- Document ID: US9356162B2
- Status: Granted
- Kind: B2
- Application number: 12/695,671
- Filed: 2010-01-28
- Published: 2010-07-29
- Granted: 2016-05-31
- Earliest claimed: 2009-01-28
- Assignees: MicroLink Devices, Inc.
- Applicants: Noren Pan; Christopher Youtsey; David S. McCallum; Victor C. Elarde; John M. Dallesasse
- Inventors: Noren Pan; Christopher Youtsey; David S. McCallum; Victor C. Elarde; John M. Dallesasse
- Web page: https://patentgrep.com/patent/US9356162B2

## CPC

- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 10/142: comprising multiple PN homojunctions, e.g. tandem cells
- H10F 10/163: comprising only Group III-V materials, e.g. GaAs/AlGaAs or InP/GaInAs photovoltaic cells
- H10F 71/129: {Passivating}
- Y02E 10/52: PV systems with concentrators
- Y02E 10/544: Solar cells from Group III-V materials
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present application utilizes an oxidation process to fabricating a Group III-V compound semiconductor solar cell device. By the oxidation process, a window layer disposed on a cell unit is oxidized to enhance the efficiency of the solar cell device. The oxidized window has an increased band gap to minimize the surface recombination of electrons and holes. The oxidized window also improves transparency at the wavelengths that were absorbed in the conventional window layer.

## Claims

### Claim 1

A method for fabricating a Group III-V compound semiconductor solar cell device, the method comprising the steps of:
forming at least one cell unit from a Gallium Indium Phosphide (Ga1-xInxP) compound semiconductor material, the cell unit being configured to absorb predetermined wavelengths of a solar spectrum;
forming an unoxidized window layer on the cell unit to prevent recombination of photo-generated carriers at a top surface of the solar cell device, wherein the unoxidized window layer thickness is about 2500 Angstroms;
providing a cap layer on the window layer to enhance an electrical contact with a metal conductive material;
etching the cap layer to expose at least a portion of the window layer; and
oxidizing the window layer to convert the window layer to an oxidized window layer, wherein the step of oxidizing includes the further steps of:
once the cell unit is formed, subjecting the cell unit to a post-processing wet oxidation technique including placing the cell unit with the unoxidized window layer in a chamber of a furnace having a temperature in the range of 350° C. to 550° C. and a pressure of generally atmospheric pressure, and
placing the cell unit in the chamber for a time in a range between about 1.0 hour and about 3.0 hours; and then
oxidizing the exposed portion of the window layer using the wet oxidation technique after the device is formed, the exposed portion corresponding to an etched portion of the cap layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the oxidized window layer has a larger band gap than the window layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein a band gap of the oxidized window layer is about 4.0 eV.

### Claim 4 (depends on 1)

The method of claim 1, wherein the window layer is an Al-containing Group III-V compound semiconductor material.

### Claim 5 (depends on 1)

The method of claim 1, wherein the window layer is an InAlP window layer or an AlGaAs window layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the oxidized window transmits a second range of wavelengths of the solar spectrum to the cell unit to increase a photoluminescence (PL) intensity of the cell unit, the second range of wavelengths being absorbed in the window layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein the second range of wavelengths are wavelengths of a far blue end of the solar spectrum.

### Claim 8 (depends on 1)

The method of claim 1, wherein a second cell unit is formed from any of Gallium Arsenide (GaAs), Gallium Iridium Phosphide (Ga1-xInxP), Gallium Indium Arsenide (Ga1-xInxAs), Indium Phosphide (InP) and Gallium Indium Arsenide Phosphide (Ga1-xInxAs1−yPy), and Aluminum Gallium Iridium Phosphide ((AlxGa1-x)1-yInyP).

### Claim 9 (depends on 1)

The method of claim 1, wherein the solar cell device comprises a plurality of cell units, wherein each cell unit is configured to absorb different wavelengths of the solar spectrum.

### Claim 10 (depends on 1)

The method of claim 1, further comprising the step of:
providing a substrate on which the cell is formed, wherein the substrate is formed of Gallium Arsenide (GaAs), Indium Phosphide (InP) or Germanium (Ge).

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
removing the cell unit with the oxidized window layer from the furnace,
providing the metal conductive material on the cap layer; and
applying an antireflection coating to the oxidized window layer.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
providing a backside contact on a bottom surface of the substrate.

### Claim 13 (depends on 1)

The solar cell device of claim 1, wherein the window layer has a thickness, comprising the step of oxidizing only a top portion of the window layer.

### Claim 14 (depends on 1)

The solar cell device of claim 1, wherein the window layer has a thickness, comprising the step of oxidizing the entire thickness of the window layer.

### Claim 15 (depends on 1)

The solar cell device of claim 1, wherein prior to oxidation the window layer has a first thickness, and after oxidation the window layer has a second thickness that is greater than the first thickness.

### Claim 16 (depends on 1)

The method of claim 1, further comprising the steps of providing the metal conductive material on the cap layer prior to introducing the cell unit to the furnace,
removing the cell unit with the oxidized window layer from the furnace, and then
applying an antireflection coating to the oxidized window layer.

### Claim 17 (depends on 1)

The method of claim 1, further comprising adjusting the temperature of the chamber based on the material composition of the window layer.

### Claim 18 (depends on 1)

The method of claim 1, further comprising adjusting the time the unit cell is placed in the chamber based on the material composition of the window layer.

### Claim 19

A method for fabricating a Group III-V compound semiconductor solar cell device, the method comprising the steps of:
forming at least one cell unit from a Gallium Indium Phosphide (Ga1-xInxP) compound semiconductor material, the cell unit being configured to absorb predetermined wavelengths of a solar spectrum;
forming an unoxidized window layer on the cell unit to prevent recombination of photo-generated carriers at a top surface of the solar cell device;
providing a cap layer on the window layer to enhance an electrical contact with a metal conductive material;
etching the cap layer to expose at least a portion of the window layer; and
oxidizing the window layer to convert the window layer to an oxidized window layer, wherein the step of oxidizing includes the further steps of:
once the cell unit is formed, subjecting the cell unit to a post-processing wet oxidation technique including placing the cell unit with the unoxidized window layer in a chamber of a furnace having a temperature in the range of 350° C. to 550° C. and a pressure of generally atmospheric pressure, and
placing the cell unit in the chamber for a time in a range between about 1.0 hour and about 3.0 hours; and then
oxidizing the exposed portion of the window layer using the wet oxidation technique after the device is formed, the exposed portion corresponding to an etched portion of the cap layer,
wherein the oxidized window layer is an A1GaAs window layer, and
wherein the oxidized window layer transmits a second range of wavelengths of the solar spectrum to the cell unit to increase a photoluminescence (PL) intensity of the cell unit, the second range of wavelengths being absorbed in the window layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the oxidized window layer has a larger band gap than the window layer and wherein a band gap of the oxidized window layer is about 4.0 eV.