# US 9,356,156 B2 · Stable high mobility MOTFT and fabrication at low temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,156 B2
- Document ID: US9356156B2
- Status: Granted
- Kind: B2
- Application number: 13/902,514
- Filed: 2013-05-24
- Published: 2014-11-27
- Granted: 2016-05-31
- Earliest claimed: 2013-05-24
- Assignees: Cbrite Inc.
- Applicants: Chan-Long Shieh; Gang Yu; Fatt Foong; Juergen Musolf
- Inventors: Chan-Long Shieh; Gang Yu; Fatt Foong; Juergen Musolf
- Web page: https://patentgrep.com/patent/US9356156B2

## CPC

- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10D 30/031: {of thin-film transistors [TFT]}
- H10D 30/6704: {having supplementary regions or layers in the thin films or in the insulated bulk substrates for controlling properties of the device}
- H10D 30/6713: {characterised by the properties of the source or drain regions, e.g. compositions or sectional shapes}
- H10D 30/673: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 30/6756: {Amorphous oxide semiconductors}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 30/6758: {characterised by the insulating substrates}
- H10D 62/402: {Amorphous materials}
- H10D 62/80: characterised by the materials
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10W 20/0698: {Local interconnections}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/083: {the openings being via holes penetrating underlying conductors}
- H10D 86/021: {of multiple TFTs}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a stable high mobility amorphous MOTFT includes a step of providing a substrate with a gate formed thereon and a gate dielectric layer positioned over the gate. A carrier transport structure is deposited by sputtering on the gate dielectric layer. The carrier transport structure includes a layer of amorphous high mobility metal oxide adjacent the gate dielectric and a relatively inert protective layer of material deposited on the layer of amorphous high mobility metal oxide both deposited without oxygen and in situ. The layer of amorphous metal oxide has a mobility above 40 cm2/Vs and a carrier concentration in a range of approximately 1018 cm−3 to approximately 5×1019 cm−3. Source/drain contacts are positioned on the protective layer and in electrical contact therewith.

## Claims

### Claim 1

A method of fabricating a stable high mobility amorphous MOTFT comprising the steps of:
providing a substrate with a gate formed thereon and a gate dielectric layer positioned over the gate;
depositing a carrier transport structure on the gate dielectric layer, the carrier transport structure including a layer of amorphous high mobility metal oxide adjacent the gate dielectric and a protective layer of material relatively inert compared to the layer of metal oxide;
forming an oxygen-rich zone adjacent a top surface of the protective layer at approximately room temperature, including coating with an oxygen-rich self-assembled layer comprising one of 4-chlorophenyl trichlorosilane (4-CPTS), chloromethyl trichlorosilane (CMTS), 4-chlorophenyl phosphoric acid (4-CPPA), 3-nitrophenyl phosphonic acid (3-NPPA), 2-chloroethyl phosphonic acid (2-CEPA), or their combination; and
driving oxygen into the protective layer at an elevated temperature below approximately 350° C.

### Claim 2 (depends on 1)

The method as claimed in claim 1 further including the steps of:
defining a channel area overlying the gate in the layer of amorphous high mobility metal oxide;
forming an etch-stop layer overlying the channel area subsequent to the driving oxygen step;
defining source/drain contact areas on opposed sides of the channel area;
performing a cleaning and/or treatment and/or etching step on the surface of the source/drain contact areas; and
depositing and patterning source/drain contacts on the protective layer in the source/drain contact areas.

### Claim 3 (depends on 1)

The method as claimed in claim 1 further including, prior to the step of forming an oxygen-rich zone, the steps of:
defining a channel area overlying the gate in the layer of amorphous high mobility metal oxide;
defining source/drain contact areas on opposed sides of the channel area;
depositing a blanket metal layer on the protective layer; and
patterning the blanket metal layer to form source/drain electrodes in the source/drain areas and to open an area between the source/drain electrodes overlying the channel area.

### Claim 4 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing a layer of amorphous high mobility metal oxide includes depositing a layer of amorphous metal oxide with a mobility above 40 cm2/Vs.

### Claim 5 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing a layer of amorphous high mobility metal oxide includes depositing a layer of amorphous metal oxide with a carrier concentration in a range of approximately 1018 cm−3 to approximately 5×1019 cm−3.

### Claim 6 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the layer of amorphous high mobility metal oxide includes depositing one of indium-tin-oxide (ITO), indium oxide (InO), tin oxide (SnO), cadmium oxide (CdO), zinc oxide (ZnO) indium-zinc-oxide (IZO), or zinc oxide (ZnO), or a composite film including more than one of the above metal-oxides.

### Claim 7 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the layer of amorphous high mobility metal oxide includes depositing a layer with a thickness in a range of equal to or less than approximately 5 nm.

### Claim 8 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the protective layer includes depositing a layer including metal oxides that are more inert than the amorphous high mobility metal oxide layer.

### Claim 9 (depends on 8)

The method as claimed in claim 8 wherein the step of depositing the more inert metal oxide includes depositing a layer of one of M-Zn—O, M-In—O, or their combination, where M includes at least one of Al, Ga, Ta, Ti, Si, Ge, Sn, Mo, W, Cu, V, or Zr.

### Claim 10 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the protective layer includes depositing a layer with a thickness in a range of 20 nm-50 nm.

### Claim 11 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the carrier transport structure includes depositing the layer of amorphous high mobility metal oxide and the protective layer in situ, without a vacuum break.

### Claim 12 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the carrier transport structure includes depositing the layer of amorphous high mobility metal oxide and the protective layer at a temperature below 160° C.

### Claim 13 (depends on 1)

The method as claimed in claim 1 wherein the step of depositing the carrier transport structure includes depositing the layer of amorphous high mobility metal oxide and the protective layer by sputtering.

### Claim 14 (depends on 13)

The method as claimed in claim 13 wherein the step of depositing the layer of amorphous high mobility metal oxide and the protective layer by sputtering without oxygen.

### Claim 15 (depends on 1)

The method as claimed in claim 1 wherein the step of forming the oxygen-rich zone further includes using oxygen plasma, N2O plasma, a UV-ozone process, surface treatment with hydrogen-peroxide or a dichromate solution, or a combination process thereof.

### Claim 16 (depends on 15)

The method as claimed in claim 15 wherein the step of forming the oxygen-rich zone is performed at a temperature below 160° C.

### Claim 17 (depends on 15)

The method as claimed in claim 15 wherein the step of forming the oxygen-rich zone is performed at a pressure below 100 mtorr.

### Claim 18 (depends on 1)

The method as claimed in claim 1 wherein the step of driving oxygen from the oxygen source into the protective layer includes using an elevated temperature equal to or greater than 160° C.

### Claim 19 (depends on 1)

The method as claimed in claim 1 wherein the step of providing the substrate includes providing a substrate including one of glass, plastic film, and stainless steel film each in one of rigid, conformable, or flexible form.

### Claim 20 (depends on 1)

The method as claimed in claim 1 wherein the step of providing the gate dielectric layer includes providing a layer including SiO2, SiN, Al2O3, AlN, Ta2O5, TiO2, ZrO, HfO, SrO, or their combinations in blend or multiple layer form.

### Claim 21 (depends on 20)

The method as claimed in claim 20 wherein the step of providing the gate dielectric layer includes forming the gate dielectric layer by anodization, by heating under oxygen-rich ambient, or combinations thereof in sequence from the corresponding metal.

### Claim 22

A method of fabricating a stable high mobility amorphous MOTFT comprising the steps of:
providing a substrate with a gate formed thereon and a gate dielectric layer positioned over the gate;
depositing by sputtering a carrier transport structure on the gate dielectric layer without intentional substrate heating or with intentional cooling, the carrier transport structure including a layer of amorphous high mobility metal oxide adjacent the gate dielectric and a protective layer of material deposited on the layer of amorphous high mobility metal oxide both deposited without oxygen and in situ, the protective layer being relatively inert compared to the layer of amorphous high mobility metal oxide;
forming an oxygen-rich zone at the upper surface of the protective layer at a temperature below 160° C.
driving oxygen into the protective layer from the oxygen-rich zone at an elevated temperature; and
the resulting layer of amorphous metal oxide having a mobility above 40 cm2/Vs and a carrier concentration in a range of approximately 1018 cm−3 to approximately 5×1019 cm−3.

### Claim 23 (depends on 22)

The method as claimed in claim 22 further including the steps of:
defining a channel area overlying the gate in the layer of amorphous high mobility metal oxide;
forming an etch-stop layer overlying the channel area subsequent to the driving oxygen step;
defining source/drain contact areas on opposed sides of the channel area;
performing a cleaning and/or treatment and/or etching step on the surface of the source/drain contact areas; and
depositing and patterning source/drain contacts on the protective layer in the source/drain contact areas.

### Claim 24 (depends on 22)

The method as claimed in claim 22 further including, prior to the step of forming an oxygen-rich zone, the steps of:
defining a channel area overlying the gate in the layer of amorphous high mobility metal oxide;
defining source/drain contact areas on opposed sides of the channel area;
depositing a blanket metal layer on the protective layer; and
patterning the blanket metal layer to form source/drain electrodes in the source/drain areas and to open an area between the source/drain electrodes overlying the channel area.

### Claim 25 (depends on 22)

The method as claimed in claim 22 wherein the step of depositing the layer of amorphous high mobility metal oxide includes depositing a layer with a thickness in a range of equal to or less than approximately 5 nm.

### Claim 26 (depends on 22)

The method as claimed in claim 22 wherein the step of depositing the protective layer includes depositing a layer with a thickness in a range of 20 nm-50 nm.