# US 9,356,124 B2 · Method for fabricating multi-gate structure device with source and drain having quasi-SOI structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,124 B2
- Document ID: US9356124B2
- Status: Granted
- Kind: B2
- Application number: 14/764,155
- Filed: 2013-09-30
- Published: 2016-03-03
- Granted: 2016-05-31
- Earliest claimed: 2013-03-28
- Assignees: Peking University
- Applicants: Peking University
- Inventors: Ru Huang; Jiewen Fan; Jia Li; Xiaoyan Xu; Ming Li
- Web page: https://patentgrep.com/patent/US9356124B2

## CPC

- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0223: {having source and drain regions or source and drain extensions self-aligned to sides of the gate}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 62/116: {adjoining the input or output regions of field-effect devices, e.g. adjoining source or drain regions}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 50/242: {of Group IV materials}
- H10P 50/283: {by chemical means}
- H10P 52/403: {of conductive or resistive materials}
- H10P 95/064: {the removal being chemical etching}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating a multi-gate structure device with a source and a drain having a quasi-SOI structure, comprising forming an active region in a shape of a fin bar, forming an oxide isolation layer for shallow trench isolation (STI), forming a polysilicon dummy gate, forming source and drain extension regions, forming the source and the drain with the quasi-SOI structure, and forming a high-K metal gate. Solution(s) consistent with the present innovations may be achieved by using a process method compatible with the conventional bulk silicon CMOS processes and can be easily integrated into the process flow. Moreover, innovations here may provide a small leakage current even in a case of having a short channel length, thereby reducing the power consumption of the device.

## Claims

### Claim 1

A method for fabricating a multi-gate structure device with a source and a drain having a quasi-SOI structure, wherein the method comprises:
forming an active region in a shape of a fin bar, comprising:
depositing a silicon oxide layer and a silicon nitride layer on a surface of a silicon wafer to be used as materials for a hard mask;
defining a pattern of the fin bar in a fine strip shape by a photolithography process;
transferring the pattern onto the hard mask by using a dry etching process;
transferring the pattern onto the silicon wafer by using the hard mask and removing a photoresist;
forming an oxide isolation layer for shallow trench isolation (STI), comprising:
depositing a silicon oxide layer as a material for STI;
performing a CMP process to the silicon oxide layer until stopping at a surface of the silicon nitride layer, so that the surface of the silicon nitride layer and a surface of the silicon oxide layer are flattened;
removing the silicon nitride layer used as the hard mask by using a wet corrosion process;
etching back the silicon oxide layer in a region of STI by using a dry etching process so as to form STI;
performing a well implantation process and a well annealing process; and
performing an implantation process and an annealing process for inhibiting a substrate parasite transistor from being formed;
forming a polysilicon dummy gate, comprising:
forming a silicon oxide layer through a dry oxygen oxidation process to be used as a dummy gate dielectric layer;
depositing a polysilicon layer as a gate material layer;
performing a CMP process to flatten the polysilicon layer until stopping at a certain height from a top of the fin bar;
depositing a silicon oxide layer as a hard mask layer for a gate line; and
performing a photolithography process and an etching process to form a hard mask line and the gate line;
forming source and drain extension regions, comprising:
depositing a silicon oxide layer as an offset material layer;
performing an implantation process for the source and drain extension regions; and
depositing a silicon oxide layer and etching back it by using a dry etching process so as to form silicon oxide sidewalls;
forming the source and the drain with the quasi-SOI structure, comprising:
etching the silicon wafer in the source and the drain until stopping under a surface of the region of STI;
depositing a silicon nitride layer and etching back it by using a dry etching process to form silicon nitride sidewalls, which are formed only at outer surfaces of the silicon oxide sidewalls, while the silicon nitride layer within a trench between regions of STI in the source and the drain is completely removed;
etching the silicon wafer within the trench of the source and the drain once again to a certain depth by using an anisotropic dry etching process;
forming a silicon oxide layer in the trench of the source and the drain through a wet oxidation process to be used as an isolation layer in the quasi-SOI structure;
performing a wet corrosion process to remove the silicon nitride sidewalls;
doping an epitaxial monocrystalline silicon layer in situ to form a highly-doped lifted source and drain; and
performing an implantation process and an annealing process for the source and drain;
forming a high-k metal gate, comprising:
depositing a silicon oxide layer as a dielectric layer;
performing a CMP process to the silicon oxide layer until stopping at the surface of the polysilicon layer, so that a surface of the silicon oxide layer and the surface of the polysilicon layer are flattened;
removing the polysilicon dummy gate through a wet corrosion process;
removing the dummy gate dielectric layer of silicon oxide through a wet corrosion process;
forming a transition layer of silicon oxide and a high-k gate dielectric layer of HfO2 through an atomic layer deposition process;
forming a metal work function adjusting layer of TiN through an atomic layer deposition process;
forming a metal gate material layer of Al through a physical vapor deposition process;
performing a CMP process to the metal gate material layer of Al until stopping at the surface of the silicon oxide layer, so that the surface of the silicon oxide layer and a surface of Al are flattened;
forming contact holes by using a photolithography process and an etching process; and
forming metal contacts and performing an alloying process.

### Claim 2 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing the materials for the hard mask, the silicon oxide layer has a thickness of about 200 Å and the silicon nitride layer has a thickness of about 500 Å.

### Claim 3 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing a polysilicon layer as a gate material layer, the silicon oxide layer has a thickness more than about 1000 Å higher than a height of the fin bar.

### Claim 4 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing a silicon oxide layer as a hard mask layer for a gate line, the silicon oxide layer has a thickness of about 300 Å.

### Claim 5 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing a silicon oxide layer as an offset material layer, the silicon oxide layer has a thickness of about 50 Å.

### Claim 6 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing and etching a silicon oxide layer to form silicon oxide sidewalls, the silicon oxide layer has a thickness of about 100 Å.

### Claim 7 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing and etching a silicon nitride layer to form silicon nitride sidewalls, the silicon nitride layer has a thickness of about 150 Å.

### Claim 8 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of etching using an anisotropic dry etching process, the depth is 20-30 nm.

### Claim 9 (depends on 1)

The method for fabricating the multi-gate structure device with the source and the drain having the quasi-SOI structure of claim 1, wherein in the step of depositing and etching a silicon oxide layer to form silicon oxide sidewalls, the silicon oxide layer has a thickness of about 4000 Å.

### Claim 10

A method for fabricating a multi-gate structure device with a source and a drain having a quasi-SOI structure, wherein the method comprises:
forming an active region in a shape of a fin bar, comprising:
depositing a silicon oxide layer and a silicon nitride layer on a surface of a silicon wafer to be used as materials for a hard mask;
defining a pattern of the fin bar in a fine strip shape by a photolithography process;
transferring the pattern onto the hard mask by using a dry etching process;
transferring the pattern onto the silicon wafer by using the hard mask and removing a photoresist;
forming an oxide isolation layer for shallow trench isolation (STI), comprising:
depositing a silicon oxide layer as a material for STI;
forming a polysilicon dummy gate, comprising:
forming a silicon oxide layer through a dry oxygen oxidation process to be used as a dummy gate dielectric layer;
depositing a polysilicon layer as a gate material layer;
performing a CMP process to flatten the polysilicon layer until stopping at a certain height from a top of the fin bar;
depositing a silicon oxide layer as a hard mask layer for a gate line; and
performing a photolithography process and an etching process to form a hard mask line and the gate line;
forming source and drain extension regions, comprising:
depositing a silicon oxide layer as an offset material layer;
performing an implantation process for the source and drain extension regions; and
depositing a silicon oxide layer and etching back it by using a dry etching process so as to form silicon oxide sidewalls;
forming the source and the drain with the quasi-SOI structure, comprising:
etching the silicon wafer in the source and the drain until stopping under a surface of the region of STI;
depositing a silicon nitride layer and etching back it by using a dry etching process to form silicon nitride sidewalls, which are formed only at outer surfaces of the silicon oxide sidewalls, while the silicon nitride layer within a trench between regions of STI in the source and the drain is completely removed;
etching the silicon wafer within the trench of the source and the drain once again to a certain depth by using an anisotropic dry etching process;
forming a silicon oxide layer in the trench of the source and the drain through a wet oxidation process to be used as an isolation layer in the quasi-SOI structure;
performing a wet corrosion process to remove the silicon nitride sidewalls;
doping an epitaxial monocrystalline silicon layer in situ to form a highly-doped lifted source and drain; and
performing an implantation process and an annealing process for the source and drain;
forming a high-k metal gate.

### Claim 11 (depends on 10)

The method of claim 10, wherein in the step of depositing the materials for the hard mask, the silicon oxide layer has a thickness of 200 Å and the silicon nitride layer has a thickness of about 500 Å.

### Claim 12 (depends on 11)

The method of claim 11, wherein in the step of depositing a polysilicon layer as a gate material layer, the silicon oxide layer has a thickness more than about 1000 521 higher than a height of the fin bar.

### Claim 13 (depends on 12)

The method of claim 12, wherein in the step of depositing a silicon oxide layer as a hard mask layer for a gate line, the silicon oxide layer has a thickness of about 300 Å.

### Claim 14 (depends on 13)

The method of claim 13, wherein in the step of depositing a silicon oxide layer as an offset material layer, the silicon oxide layer has a thickness of about 50 Å.

### Claim 15 (depends on 14)

The method of claim 14, wherein in the step of depositing and etching a silicon oxide layer to form silicon oxide sidewalls, the silicon oxide layer has a thickness of about 100 Å.

### Claim 16 (depends on 15)

The method of claim 15, wherein in the step of depositing and etching a silicon nitride layer to form silicon nitride sidewalls, the silicon nitride layer has a thickness of 150 Å.

### Claim 17 (depends on 16)

The method of claim 16, wherein in the step of etching using an anisotropic dry etching process, the depth is about 20 nm to about 30 nm.

### Claim 18 (depends on 10)

The method of claim 10, wherein in the step of depositing and etching a silicon oxide layer to form silicon oxide sidewalls, the silicon oxide layer has a thickness of about 4000 Å.

### Claim 19 (depends on 10)

The method of claim 10 wherein the step of forming the high-k metal gate comprises:
depositing a silicon oxide layer as a dielectric layer;
performing a CMP process to the silicon oxide layer until stopping at the surface of the polysilicon layer, so that a surface of the silicon oxide layer and the surface of the polysilicon layer are flattened;
removing the polysilicon dummy gate through a wet corrosion process;
removing the dummy gate dielectric layer of silicon oxide through a wet corrosion process;
forming a transition layer of silicon oxide and a high-k gate dielectric layer of HfO2 through an atomic layer deposition process;
forming a metal work function adjusting layer of TiN through an atomic layer deposition process;
forming a metal gate material layer of Al through a physical vapor deposition process;
performing a CMP process to the metal gate material layer of Al until stopping at the surface of the silicon oxide layer, so that the surface of the silicon oxide layer and a surface of Al are flattened;
forming contact holes by using a photolithography process and an etching process; and
forming metal contacts and performing an alloying process.

### Claim 20 (depends on 12)

The method of claim 12, wherein in the step of depositing and etching a silicon nitride layer to form silicon nitride sidewalls, the silicon nitride layer has a thickness of 150 Å.