# US 9,356,123 B2 · Manufacturing method of low temperature polycrystalline silicon thin film and manufacturing method of thin film transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,123 B2
- Document ID: US9356123B2
- Status: Granted
- Kind: B2
- Application number: 14/355,137
- Filed: 2013-06-06
- Published: 2015-06-04
- Granted: 2016-05-31
- Earliest claimed: 2013-03-29
- Assignees: Boe Technology Group Co., Ltd.
- Applicants: Huijuan Zhang
- Inventors: Huijuan Zhang
- Web page: https://patentgrep.com/patent/US9356123B2

## CPC

- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6731: {Top-gate only TFTs}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3454: {Amorphous}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10P 30/20: into semiconductor materials, e.g. for doping
- H10P 70/10: {Cleaning before device manufacture, i.e. Begin-Of-Line process}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A manufacturing method of a low temperature polycrystalline silicon thin film and a manufacturing method of a thin film transistor are provided. The manufacturing method of the low temperature polycrystalline silicon thin film comprises: forming an amorphous silicon thin film on a substrate; and performing a rapid thermal annealing (RTA) process on the amorphous silicon thin film for several times at a predetermined temperature to form the low temperature polycrystalline silicon thin film, wherein the predetermined temperature is lower than a conventional RTA crystallization temperature.

## Claims

### Claim 1

A manufacturing method of a low temperature polycrystalline silicon thin film, comprising:
forming an amorphous silicon thin film on a substrate; and
performing a first thermal treatment on the amorphous silicon thin film under a temperature range of 400-500° C.;
performing a rapid thermal annealing (RTA) process on the amorphous silicon thin film for several times at a predetermined temperature followed by a cooling process to cool the substrate to a room temperature each cycle, so as to form the low temperature polycrystalline silicon thin film, wherein the predetermined temperature is lower than 750° C; and
performing a second thermal treatment on the low temperature polycrystalline silicon thin film under a temperature range of 400-500° C. for at least 3 hours.

### Claim 2 (depends on 1)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 1, wherein the forming the amorphous silicon thin film on the substrate comprises:
forming a buffer layer on the substrate; and
forming the amorphous silicon thin film on the buffer layer.

### Claim 3 (depends on 2)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 2, wherein before the forming the buffer layer on the substrate, the method further comprises: cleaning the substrate.

### Claim 4 (depends on 1)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 1, wherein
the RTA process performed on the amorphous silicon thin film is under a temperature range of 600-670° C. for no more than 30 s.

### Claim 5 (depends on 4)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 4, wherein the first thermal treatment performed on the amorphous silicon thin film is lasted for 1-2 hours.

### Claim 6 (depends on 5)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 5, wherein the first thermal treatment is performed to remove hydrogen from the amorphous silicon thin film.

### Claim 7 (depends on 1)

A manufacturing method of a thin film transistor, comprising:
forming a buffer layer on a substrate;
forming a low temperature polycrystalline silicon thin film on the buffer layer by using a method according to claim 1;
patterning the low temperature polycrystalline silicon thin film to form an active layer comprising a source region, a drain region and a channel region;
forming a gate insulation layer on the channel region, and forming a gate electrode on the gate insulation layer;
doping impurities into the source region and the drain region by an ion implantation method, and forming an interlayer insulation layer on the gate electrode; and
forming a source electrode and a drain electrode on the substrate on which the interlayer insulation layer has been formed.

### Claim 8 (depends on 1)

A manufacturing method of a thin film transistor, comprising:
forming a buffer layer on a substrate;
forming a gate electrode on the buffer layer, and forming a gate insulation layer on the gate electrode;
forming a low temperature polycrystalline silicon thin film on the gate insulation layer by using a method according to claim 1;
patterning the low temperature polycrystalline silicon thin film to form an active layer comprising a source region, a drain region and a channel region;
doping impurities into the source region and the drain region by an ion implantation method, and forming an interlayer insulation layer on the active layer; and
forming a source electrode and a drain electrode on the substrate on which the interlayer insulation layer has been formed.

### Claim 9 (depends on 1)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 1, wherein before the forming the amorphous silicon thin film on the substrate, the method further comprises: cleaning the substrate.

### Claim 10 (depends on 1)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 1, wherein the first thermal treatment is performed to remove hydrogen from the amorphous silicon thin film.

### Claim 11 (depends on 1)

The manufacturing method of the low temperature polycrystalline silicon thin film according to claim 1, wherein the second thermal treatment is performed so that a growth of crystal grains of the low temperature polycrystalline silicon thin film is promoted.