# US 9,356,110 B2 · Semiconductor device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,110 B2
- Document ID: US9356110B2
- Status: Granted
- Kind: B2
- Application number: 14/173,074
- Filed: 2014-02-05
- Published: 2014-10-23
- Granted: 2016-05-31
- Earliest claimed: 2013-02-26
- Assignees: Renesas Electronics Corporation
- Applicants: Renesas Electronics Corporation
- Inventors: Masao Inoue; Yoshiki Maruyama; Akio Nishida; Yorinobu Kunimune; Kota Funayama
- Web page: https://patentgrep.com/patent/US9356110B2

## CPC

- H10D 64/662: {the conductor further comprising additional layers, e.g. multiple silicon layers having different crystal structures}
- H10D 30/0411: {of FETs having floating gates}
- H10D 30/6891: {characterised by the shapes, relative sizes or dispositions of the floating gate electrode}
- H10D 64/01306: {the conductor comprising a layer of silicon contacting the insulator, e.g. polysilicon}
- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10D 64/661: {the conductor comprising a layer of silicon contacting the insulator, e.g. polysilicon having vertical doping variation (having lateral variation in the gate structure H10D64/671)}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3238: {being insulating materials}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

To control a grain growth on laminated polysilicon films, a method of manufacturing a semiconductor device is provided. The method includes: forming a first polysilicon film (21) on a substrate (10); forming an interlayer oxide layer (22) on a surface of the first polysilicon film (21); forming a second polysilicon film (23) in contact with the interlayer oxide layer (22) above the first polysilicon film (21); and performing annealing at a temperature higher than a film formation temperature of the first and second polysilicon films in a gas atmosphere containing nitrogen, after formation of the second polysilicon film (23).

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
forming a first polysilicon film on a substrate;
forming an oxide layer on a surface of the first polysilicon film;
forming a second polysilicon film above the first polysilicon film, the second polysilicon film being in contact with the oxide layer; and
performing annealing at a temperature higher than a film formation temperature of the first and second polysilicon films in a gas atmosphere containing at least one of N2, NO or N2O, after the formation of the second polysilicon film, such that nitrogen is introduced to the oxide layer to suppress grain growth inside the polysilicon films.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the annealing in the gas atmosphere containing nitrogen is performed at a pressure equal to or higher than an atmospheric pressure.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the annealing in the gas atmosphere containing at least one of N2, NO or N2O is performed in a first annealing step after the formation of the second polysilicon film.

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the step of annealing in the gas atmosphere containing at least one of N2, NO or N2O is a step to be performed at a maximum temperature after formation of the second polysilicon film.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
after the annealing in the gas atmosphere containing at least one of N2, NO or N2O, an impurity is introduced into the second polysilicon film, and
the second polysilicon film in which the impurity is introduced is annealed.

### Claim 6 (depends on 5)

The method of manufacturing a semiconductor device according to claim 5, wherein
the annealing of the second polysilicon film in which the impurity is introduced is performed at a temperature lower than the temperature at which the annealing in the gas atmosphere containing at least one of N2, NO or N2O is performed.

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
the first polysilicon film is formed on a gate insulating film, and
laminated polysilicon films including the first polysilicon film and the second polysilicon film serve as a gate of a transistor.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein
the semiconductor device is a floating gate type transistor, and
at least one of a control gate and a floating gate of the floating gate type transistor comprises the laminated polysilicon films.

### Claim 9 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein
the semiconductor device is a split gate type transistor, and
a control gate of the split gate type transistor comprises the laminated polysilicon films.

### Claim 10

A method of manufacturing a semiconductor device, comprising:
forming a first polysilicon film on a substrate;
forming an oxide layer on a surface of the first polysilicon film;
forming a second polysilicon film above the first polysilicon film, the second polysilicon film being in contact with the oxide layer; and
annealing the first and second polysilicon films in a gas atmosphere containing nitrogen at a pressure equal to or higher than an atmospheric pressure, after the formation of the second polysilicon film, wherein
after the annealing in the gas atmosphere containing nitrogen, an impurity is introduced into the second polysilicon film, and
the second polysilicon film in which the impurity is introduced is annealed.

### Claim 11 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein the annealing in the gas atmosphere containing nitrogen is performed in a first annealing step after the formation of the second polysilicon film.

### Claim 12 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein the annealing in the gas atmosphere containing nitrogen is performed at a temperature higher than a film formation temperature of the second polysilicon film.

### Claim 13 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein the annealing of the second polysilicon film in which the impurity is introduced is performed at a temperature lower than the temperature at which the annealing in the gas atmosphere containing nitrogen is performed.

### Claim 14 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein the gas containing nitrogen includes one of an N2 gas, an NO gas, and an N2O gas.

### Claim 15 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein
the first polysilicon film is formed on a gate insulating film, and
laminated polysilicon films including the first polysilicon film and the second polysilicon film serve as a gate of a transistor.

### Claim 16 (depends on 15)

The method of manufacturing a semiconductor device according to claim 15, wherein
the semiconductor device is a floating gate type transistor, and
at least one of a control gate and a floating gate of the floating gate type transistor comprises the laminated polysilicon films.

### Claim 17 (depends on 15)

The method of manufacturing a semiconductor according to claim 15, wherein
the semiconductor device is a split gate type transistor, and
a control gate of the split gate type transistor comprises the laminated polysilicon films.

### Claim 18 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the annealing is performed for 60 seconds.