# US 9,355,980 B2 · Three-dimensional chip stack and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,980 B2
- Document ID: US9355980B2
- Status: Granted
- Kind: B2
- Application number: 14/016,966
- Filed: 2013-09-03
- Published: 2015-03-05
- Granted: 2016-05-31
- Earliest claimed: 2013-09-03
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Wei-Ming Chen; Cheng-Hsien Hsieh; Sung-Hui Huang; Kuo-Ching Hsu
- Web page: https://patentgrep.com/patent/US9355980B2

## CPC

- B23K 1/0016: {Soldering of electronic components}
- H10W 70/611: {for connecting multiple chips together}
- H10W 70/65: Shapes or dispositions of interconnections
- H10W 90/00: Package configurations
- B23K 2101/40: Semiconductor devices
- H10W 72/01223: {in liquid form, e.g. by dispensing droplets or by screen printing}
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01238: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01255: {by using masks}
- H10W 72/019: {of bond pads}
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01953: {by etching}
- H10W 72/0198: {batch processes}
- H10W 72/072: {of bump connectors}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/07255: {changes in materials}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/2528: {Intermetallic compounds}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/722: {between stacked chips}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A three-dimensional chip stack includes a first chip bonded to a second chip to form a bonded interconnection therebetween. The bonded interconnection includes a first conductive pillar overlying a first substrate of the first chip, a second conductive pillar overlying a second substrate of the second chip, and a joint structure between the first conductive pillar and the second conductive pillar. The joint structure includes a first IMC region adjacent to the first conductive pillar, a second IMC region adjacent to the second conductive pillar, and a metallization layer between the first IMC region and the second IMC region.

## Claims

### Claim 1

A three-dimensional chip stack, comprising:
a first chip comprising a first substrate;
a first conductive pillar overlying the first substrate;
a second chip comprising a second substrate;
a second conductive pillar overlying the second substrate; and
a metallization layer between the first conductive pillar and the second conductive pillar, the metallization layer having a first surface and a second surface;
wherein the first chip is bonded to the second chip to form a bonded interconnection between the first substrate and the second substrate,
wherein the bonded interconnection comprises a first joint structure between the first conductive pillar and the first surface of the metallization layer, and a second joint structure between the second conductive pillar and the second surface of the metallization layer;
wherein the first joint structure comprises a first intermetallic compound (IMC) and the second joint structure comprises a second IMC; and
wherein the metallizaton layer has a higher melting point than the first joint structure or the second joint structure.

### Claim 2 (depends on 1)

The three-dimensional chip stack of claim 1, wherein the metallization layer comprises at least one of copper or a layer of elemental copper.

### Claim 3 (depends on 1)

The three-dimensional chip stack of claim 1, wherein at least one of the first IMC or the second IMC comprises copper and tin.

### Claim 4 (depends on 1)

The three-dimensional chip stack of claim 1, wherein:
the metallization layer comprises a first material having a first melting point;
the first IMC comprises a second material having a second melting point, the second melting point lower than the first melting point; and
the second IMC comprises a third material having a third melting point, the third melting point lower than the first melting point.

### Claim 5 (depends on 1)

The three-dimensional chip stack of claim 1, wherein the first conductive pillar comprises a copper pillar.

### Claim 6 (depends on 5)

The three-dimensional chip stack of claim 5, wherein the first conductive pillar comprises a metal capping layer on the copper pillar.

### Claim 7 (depends on 6)

The three-dimensional chip stack of claim 6, wherein the metal capping layer comprises a nickel layer.

### Claim 8 (depends on 7)

The three-dimensional chip stack o of claim 7, wherein the first IMC region comprises copper, tin and nickel.

### Claim 9 (depends on 1)

The three-dimensional chip stack of claim 1, wherein the second conductive pillar comprises a copper pillar.

### Claim 10 (depends on 9)

The three-dimensional chip stack of claim 9, wherein the second conductive pillar comprises a metal capping layer on the copper pillar.

### Claim 11 (depends on 10)

The three-dimensional chip stack of claim 10, wherein the metal capping layer comprises a nickel layer.

### Claim 12 (depends on 11)

The three-dimensional chip stack o of claim 11, wherein the second IMC region comprises copper, tin and nickel.

### Claim 13

A method of forming a three-dimensional chip stack, the method comprising:
forming a first bump structure on a first semiconductor substrate, wherein the first bump structure comprises a first conductive pillar and a first solder layer on top of the first conductive pillar;
forming a second bump structure on a second semiconductor substrate, wherein the second bump structure comprises a second conductive pillar, a second solder layer on top of the second conductive pillar, and a metallization layer on the second solder layer;
attaching the first bump structure to the second bump structure; and
performing a thermal reflow process to form a first joint structure comprising a first intermetallic compound (IMC) region between the first conductive pillar and a first surface of the metallization layer, and a second joint structure comprising a second IMC region between the second conductive pillar and a second surface of the metallization layer, wherein the metallization layer has a higher melting point than the first IMC or the second IMC.

### Claim 14 (depends on 13)

The method of claim 13, wherein the metallization layer comprises a copper layer, and the first IMC region comprises copper and tin.

### Claim 15 (depends on 13)

The method of claim 13, wherein the first conductive pillar comprises a copper pillar.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first conductive pillar comprises a metal capping layer between the copper pillar and the first solder layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal capping layer comprises a nickel layer.

### Claim 18 (depends on 13)

The method of claim 13, further comprising forming the first solder layer as a hemisphere-shaped solder layer before attaching the first bump structure to the second bump structure.

### Claim 19

A method of forming a three-dimensional chip stack, the method comprising:
receiving a first chip comprising a first bump structure formed on a first semiconductor substrate, wherein the first bump structure comprises a first conductive pillar and a first solder layer on top of the first conductive pillar;
receiving a second chip comprising a second bump structure on a second semiconductor substrate, wherein the second bump structure comprises a second conductive pillar, a second solder layer on top of the second conductive pillar, and a metallization layer on the second solder layer, the metallization layer having a higher melting point than that of the first solder layer or the second solder layer; and
bonding the first chip to the second chip by attaching the first bump structure to the second bump structure, wherein a first joint structure comprising a first intermetallic compound (IMC) region comprising copper and tin is formed between the first conductive pillar and the first surface of the metallization layer, and a second joint structure comprising a second IMC region comprising copper and tin is formed between the second conductive pillar and a second surface of the metallization layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the metallization layer comprises a copper layer.