# US 9,355,890 B2 · Method of manufacturing semiconductor device and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,890 B2
- Document ID: US9355890B2
- Status: Granted
- Kind: B2
- Application number: 13/748,873
- Filed: 2013-01-24
- Published: 2013-08-15
- Granted: 2016-05-31
- Earliest claimed: 2012-02-15
- Assignees: Renesas Electronics Corporation
- Applicants: Renesas Electronics Corporation
- Inventors: Tetsuya Iida
- Web page: https://patentgrep.com/patent/US9355890B2

## CPC

- H10D 30/657: {having substrates comprising insulating layers, e.g. SOI-LDMOS transistors}
- H10D 30/603: {having asymmetry in the channel direction, e.g. lateral high-voltage MISFETs having drain offset region or extended drain IGFETs [EDMOS]}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 86/01: Manufacture or treatment
- H10D 87/00: Integrated devices comprising both bulk components and either SOI or SOS components on the same substrate
- H10P 52/402: {of semiconductor materials}
- H10P 90/1906: {Preparing SOI wafers}
- H10P 90/1908: {using silicon implanted buried insulating layers, e.g. oxide layers [SIMOX]}
- H10P 90/1912: {using selective deposition, e.g. epitaxial lateral overgrowth [ELO] or selective deposition of single crystal silicon}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/061: {using SOI processes together with lateral isolation, e.g. combinations of SOI and shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10W 20/021: {of interconnections within wafers or substrates}
- H10W 20/023: {the interconnections being through-semiconductor vias}
- H10W 20/0245: {comprising use of blind vias during the manufacture}
- H10W 20/20: Interconnections within wafers or substrates, e.g. through-silicon vias [TSV]
- H10W 20/2134: {TSVs extending from the semiconductor wafer into back-end-of-line layers}
- H10W 20/218: {in silicon-on-insulator [SOI] wafers}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed is a miniaturized semiconductor device having an SOI layer, in which: a silicon layer is formed over a semiconductor substrate via an BOX film; after the silicon layer is patterned by using a nitride film as a mask, an insulating film covering the surface of each of the nitride film, the silicon layer, and the BOX film is formed; subsequently, an opening, which penetrates the insulating film and the BOX film and which exposes the upper surface of the semiconductor substrate, is formed, and an epitaxial layer is formed in the opening; subsequently, the SOI region and a bulk silicon layer are formed over the semiconductor substrate by flattening the upper surface of the epitaxial layer with the use of the nitride film as an etching stopper film.

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising:
providing a semiconductor substrate that is comprised of: a supporting substrate; a first insulating film formed over the supporting substrate; and a semiconductor layer formed over the first insulating film, and that includes a first region and a second region over the upper surface of the semiconductor layer;
exposing the upper surface of the first insulating film in the second region by forming a second insulating film over the semiconductor layer and by processing the semiconductor layer with the use of the second insulating film as a mask;
forming a third insulating film so as to cover the semiconductor layer, the second insulating film, and the first insulating film;
exposing the upper surface of the supporting substrate by opening the third insulating film and the first insulating film in the second region;
forming a first epitaxial layer in the opening of the first insulating film and the third insulating film;
exposing the upper surface of the semiconductor layer by polishing the first epitaxial layer, the third insulating film, and the second insulating film; and
after the exposing of the upper surface of the semiconductor layer, forming a semiconductor element over each of the semiconductor layer in the first region and the first epitaxial layer in the second region.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein, in the exposing of the upper surface of the semiconductor layer, the second insulating film is used as a stopper film for polishing.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the semiconductor layer and the first epitaxial layer are spaced apart from each other by 5 μm or more.

### Claim 4 (depends on 3)

The method of manufacturing a semiconductor device according to claim 3,
wherein a digital circuit and an analog circuit are formed in the first region, and
wherein a high-frequency analog circuit of 10 kHz or more is formed in the second region.

### Claim 5 (depends on 4)

The method of manufacturing a semiconductor device according to claim 4,
wherein the semiconductor element formed in the second region includes an LDMOSFET (Laterally Diffused Metal Oxide Semiconductor Field Effect Transistor) in which impurities are diffused in the direction along the upper surface of the first epitaxial layer.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein, in the exposing of the upper surface of the supporting substrate, the upper surface of the supporting substrate is exposed by forming a plurality of grooves around the opening of the third insulating film and the first insulating film in the second region, and
wherein, in the forming of the first epitaxial layer, the first epitaxial layer is formed in the opening of the first insulating film and the third insulating film and a second epitaxial layer is formed in the grooves.

### Claim 7

A method of manufacturing a semiconductor device comprising:
providing a semiconductor substrate that is comprised of: a supporting substrate; a first insulating film formed over the supporting substrate; and a semiconductor layer formed over the first insulating film, and that includes a first region and a second region over the upper surface of the semiconductor layer, and forming a second insulating film over the semiconductor layer;
flattening the upper surface of each of the second insulating film and a third insulating film, after the third insulating film is embedded in a groove formed by removing both the semiconductor layer and the second insulating film between the first region and the second region;
after the flattening of the upper surface of each of the second insulating film and the third insulating film, exposing the upper surface of the supporting substrate by opening, in the second region, the second insulating film, the semiconductor layer, and the first insulating film such that both ends of the semiconductor layer in the second region are left;
forming an epitaxial layer in the opening of the first insulating film and the semiconductor layer;
exposing the upper surface of the semiconductor layer by polishing the epitaxial layer, the third insulating film, and the second insulating film; and
after the exposing of the upper surface of the semiconductor layer, forming a semiconductor element over each of the semiconductor layer in the first region and the epitaxial layer in the second region.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7 further comprising of, before the flattening of the upper surface of each of the second insulating film and the third insulating film, forming a fourth insulating film over the second insulating film,
wherein, in the exposing of the upper surface of the supporting substrate by opening, the upper surface of the supporting substrate is exposed by opening, in the second region, the fourth insulating film, the second insulating film, the semiconductor layer, and the first insulating film such that both ends of the semiconductor layer in the second region are left, and
wherein, in the forming of the epitaxial layer, the upper surface of the epitaxial layer reaches the height of the fourth insulating film.

### Claim 9 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7,
wherein, in the exposing the upper surface of the semiconductor layer, the second insulating film is used as a stopper film for polishing.

### Claim 10 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7,
wherein the semiconductor layer and the epitaxial layer are spaced apart from each other by 5 μm or more.

### Claim 11 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10,
wherein a digital circuit and an analog circuit are formed in the first region, and
wherein a high-frequency analog circuit of 10 kHz or more is formed in the second region.

### Claim 12 (depends on 11)

The method of manufacturing a semiconductor device according to claim 11,
wherein the semiconductor element formed in the second region includes an LDMOSFET (Laterally Diffused Metal Oxide Semiconductor Field Effect Transistor) in which impurities are diffused in the direction along the upper surface of the epitaxial layer.

### Claim 13

A method of manufacturing a semiconductor device comprising:
providing a semiconductor substrate that is formed by: a supporting substrate; a first insulating film formed over the supporting substrate; and a semiconductor layer formed over the first insulating film, and that includes a first region and a second region over the upper surface of the semiconductor layer;
forming an element isolation region in a groove formed by removing the semiconductor layer between the first region and the second region;
forming a third insulating film, which has a first opening in the second region, over each of the semiconductor layer and the element isolation region;
exposing the upper surface of the supporting substrate by providing a second opening in the second region with the use of the third insulating film as a mask;
forming an epitaxial layer in the second opening;
exposing the upper surface of the semiconductor layer by polishing the epitaxial layer and the third insulating film; and
after the exposing of the upper surface of the semiconductor layer, forming a semiconductor element over each of the semiconductor layer in the first region and the epitaxial layer in the second region.

### Claim 14 (depends on 13)

The method of manufacturing a semiconductor device according to claim 13 further comprising, after the forming of the element isolation region and before the forming of the third insulating film, forming a second insulating film over each of the semiconductor layer and the element isolation region,
wherein, in the forming of the third insulating film, the third insulating film is formed over the second insulating film.

### Claim 15 (depends on 13)

The method of manufacturing a semiconductor device according to claim 13,
wherein the semiconductor layer and the epitaxial layer are spaced apart from each other by 5 μm or more.

### Claim 16 (depends on 15)

The method of manufacturing a semiconductor device according to claim 15,
wherein a digital circuit and an analog circuit are formed in the first region, and
wherein a high-frequency analog circuit of 10 kHz or more is formed in the second region.

### Claim 17 (depends on 16)

The method of manufacturing a semiconductor device according to claim 16,
wherein the semiconductor element formed in the second region includes an LDMOSFET (Laterally Diffused Metal Oxide Semiconductor Field Effect Transistor) in which impurities are diffused in the direction along the upper surface of the epitaxial layer.

### Claim 18 (depends on 13)

The method of manufacturing a semiconductor device according to claim 13,
wherein both ends of the first opening of the third insulating film, which is formed in the forming the third insulating film, are located immediately over the element isolation region, and
wherein the element isolation region is exposed to the internal wall of the second opening formed in the exposing of the upper surface of the supporting substrate.

### Claim 19 (depends on 13)

The method of manufacturing a semiconductor device according to claim 13,
wherein both ends of the first opening of the third insulating film formed in the forming of the third insulating film are located immediately over the semiconductor layer, and
wherein the semiconductor layer is exposed to the internal wall of the second opening formed in the exposing of the upper surface of the supporting substrate.