# US 9,355,886 B2 · Conformal film deposition for gapfill

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,886 B2
- Document ID: US9355886B2
- Status: Granted
- Kind: B2
- Application number: 14/074,596
- Filed: 2013-11-07
- Published: 2014-05-15
- Granted: 2016-05-31
- Earliest claimed: 2010-04-15
- Assignees: Novellus Systems, Inc.
- Applicants: Novellus Systems, Inc.
- Inventors: Shankar Swaminathan; Bart van Schravendijk; Adrien LaVoie; Sesha Varadarajan; Jason Daejin Park; Michal Danek; Naohiro Shoda
- Web page: https://patentgrep.com/patent/US9355886B2

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/56: After-treatment
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 72/0402: {Apparatus for fluid treatment (H10P72/0441, H10P72/0448 take precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method and apparatus for conformally depositing a dielectric oxide in high aspect ratio gaps in a substrate is disclosed. A substrate is provided with one or more gaps into a reaction chamber where each gap has a depth to width aspect ratio of greater than about 5:1. A first dielectric oxide layer is deposited in the one or more gaps by CFD. A portion of the first dielectric oxide layer is etched using a plasma etch, where etching the portion of the first dielectric oxide layer occurs at a faster rate near a top surface than near a bottom surface of each gap so that the first dielectric oxide layer has a tapered profile from the top surface to the bottom surface of each gap. A second dielectric oxide layer is deposited in the one or more gaps over the first dielectric oxide layer via CFD.

## Claims

### Claim 1

A method of conformally depositing a dielectric oxide in high aspect ratio gaps in a substrate, the method comprising:
(a) providing a substrate with one or more gaps into a reaction chamber, wherein each gap has a depth to width aspect ratio of greater than about 5:1;
(b) depositing a first dielectric oxide layer in the one or more gaps via conformal film deposition (CFD), wherein depositing the first dielectric oxide layer in the one or more gaps via CFD includes:
introducing a first reactant in vapor phase into the reaction chamber under conditions allowing the first reactant to adsorb onto the substrate surface;
introducing a second reactant in vapor phase into the reaction chamber while the first reactant is adsorbed on the substrate surface, wherein the second reactant is introduced without sweeping the first reactant out of the reaction chamber; and
exposing the substrate surface to plasma to drive a reaction between the first and the second reactants on the substrate surface to form the first dielectric oxide layer;
(c) etching a portion of the first dielectric oxide layer using a plasma etch, wherein etching the portion of the first dielectric oxide layer occurs at a faster rate near a top surface than near a bottom surface of each gap so that the first dielectric oxide layer has a tapered profile from the top surface to the bottom surface of each gap; and
(d) depositing a second dielectric oxide layer in the one or more gaps over the first dielectric oxide layer via CFD.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
repeating steps (b)-(d) to substantially fill the one or more gaps.

### Claim 3 (depends on 1)

The method of claim 1, wherein depositing the second dielectric oxide layer includes substantially filling the one or more gaps.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
flowing a fluorine-containing species into a remote plasma to generate a plasma-activated etchant; and
flowing the plasma-activated etchant into the reaction chamber to react with the first dielectric oxide layer to perform the etch.

### Claim 5 (depends on 4)

The method of claim 4, wherein the fluorine-containing species includes nitrogen trifluoride (NF3).

### Claim 6 (depends on 4)

The method of claim 4, further comprising:
flowing hydrogen (H2) into the reaction chamber while etching the portion of the first dielectric oxide layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein a flow rate ratio of hydrogen to the fluorine-containing species is between about 1:1 and about 5:1.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first dielectric oxide layer and the second dielectric oxide layer each include silicon dioxide (SiO2).

### Claim 9 (depends on 1)

The method of claim 1, wherein a thickness of the first dielectric oxide layer is between about 100 Å and about 500 Å.

### Claim 10

An apparatus for conformally depositing a dielectric oxide in high aspect ratio gaps in a substrate, the apparatus comprising:
a reaction chamber;
a plasma source coupled to the reaction chamber; and
a controller comprising instructions for performing the following operations:
(a) providing a substrate into the reaction chamber, wherein the substrate comprises one or more gaps, each gap having a depth to width aspect ratio of greater than about 5:1;
(b) depositing a first dielectric oxide layer in the one or more gaps via conformal film deposition (CFD), wherein depositing the first dielectric oxide layer in the one or more gaps via CFD includes:
introducing a first reactant in vapor phase into the reaction chamber under conditions allowing the first reactant to adsorb onto the substrate surface;
introducing a second reactant in vapor phase into the reaction chamber while the first reactant is adsorbed on the substrate surface, wherein the second reactant is introduced without sweeping the first reactant out of the reaction chamber; and
exposing the substrate surface to plasma to drive a reaction between the first and the second reactants on the substrate surface to form the first dielectric oxide layer:
(c) etching a portion of the first dielectric oxide layer using a plasma etch, wherein etching the portion of the first dielectric oxide layer occurs at a faster rate near a top surface than near a bottom surface of each gap so that the first dielectric oxide layer has a tapered profile from the top surface to the bottom surface of each gap; and
(d) depositing a second dielectric oxide layer in the one or more gaps over the first dielectric oxide layer via CFD.

### Claim 11 (depends on 10)

The apparatus of claim 10, wherein the controller further comprises instructions to perform:
repeating steps (b)-(d) to substantially fill the one or more gaps.

### Claim 12 (depends on 10)

The apparatus of claim 10, wherein the controller comprising instructions for depositing the second dielectric oxide layer comprises instructions for substantially filling the one or more gaps.

### Claim 13 (depends on 10)

The apparatus of claim 10, wherein the controller further comprises instructions to perform:
flowing a fluorine-based species into the plasma source to generate a plasma-activated etchant; and
flowing the plasma-activated etchant into the reaction chamber to react with the first dielectric oxide layer to perform the etch.

### Claim 14 (depends on 13)

The apparatus of claim 13, wherein the controller further comprises instructions to perform:
flowing hydrogen (H2) into the reaction chamber while etching the portion of the first dielectric oxide layer.