# US 9,355,874 B2 · Silicon nitride etching in a single wafer apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,874 B2
- Document ID: US9355874B2
- Status: Granted
- Kind: B2
- Application number: 13/244,337
- Filed: 2011-09-24
- Published: 2013-03-28
- Granted: 2016-05-31
- Earliest claimed: 2011-09-24
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Weibo Yu; Hsueh-Chin Lu; Han-Guan Chew; Kuo Bin Huang; Chao-Cheng Chen; Syun-Ming Jang
- Inventors: Weibo Yu; Hsueh-Chin Lu; Han-Guan Chew; Kuo Bin Huang; Chao-Cheng Chen; Syun-Ming Jang
- Web page: https://patentgrep.com/patent/US9355874B2

## CPC

- H10P 72/0424: {using mainly spraying means, e.g. nozzles}
- H10P 50/283: {by chemical means}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A single wafer etching apparatus and various methods implemented in the single wafer etching apparatus are disclosed. In an example, etching a silicon nitride layer in a single wafer etching apparatus includes: heating a phosphoric acid to a first temperature; heating a sulfuric acid to a second temperature; mixing the heated phosphoric acid and the heated sulfuric acid; heating the phosphoric acid/sulfuric acid mixture to a third temperature; and etching the silicon nitride layer with the heated phosphoric acid/sulfuric acid mixture.

## Claims

### Claim 1

A method comprising:
etching a silicon nitride layer in a single wafer etching apparatus, wherein the etching the silicon nitride layer includes:
heating a phosphoric acid to a first temperature;
heating a sulfuric acid to a second temperature;
mixing the heated phosphoric acid and the heated sulfuric acid in a volume ratio of phosphoric acid to sulfuric acid equal to about 1:9;
heating the phosphoric acid/sulfuric acid mixture to an etching temperature; and
etching the silicon nitride layer with the heated phosphoric acid/sulfuric acid mixture;
wherein mixing the heated phosphoric acid and the heated sulfuric acid occurs simultaneously with heating the phosphoric acid/sulfuric acid mixture to the etching temperature.

### Claim 2 (depends on 1)

The method of claim 1 further comprising mixing a heated water vapor with the phosphoric acid/sulfuric acid mixture.

### Claim 3 (depends on 1)

The method of claim 1 wherein mixing the heated phosphoric acid and the heated sulfuric acid includes using an exothermic reaction between the sulfuric acid and water vapor or hot water.

### Claim 4 (depends on 1)

The method of claim 1 wherein the etching the silicon nitride layer with the heated phosphoric acid/sulfuric acid mixture includes dispensing the heated phosphoric acid/sulfuric acid mixture onto a spinning wafer surface, wherein the wafer includes the silicon nitride layer.

### Claim 5 (depends on 1)

The method of claim 1 wherein the phosphoric acid/sulfuric acid mixture contains a larger proportion of sulfuric acid relative to phosphoric acid, by volume.

### Claim 6

A method comprising:
etching a material layer in a single wafer etching apparatus, wherein the etching the material layer includes:
mixing phosphoric acid and sulfuric acid in a volume ratio of phosphoric acid to sulfuric acid equal to about 1:9;
heating the phosphoric acid/sulfuric acid mixture to an etching temperature, wherein the heating includes injecting water vapor into the phosphoric acid/sulfuric acid mixture, and wherein mixing the phosphoric acid and the sulfuric acid occurs simultaneously with heating the phosphoric acid/sulfuric acid mixture to the etching temperature; and
etching the material layer with the heated phosphoric acid/sulfuric acid mixture.

### Claim 7 (depends on 6)

The method of claim 6 further comprising, before mixing the phosphoric acid and the sulfuric acid:
heating the phosphoric acid to a first temperature; and
heating the sulfuric acid to a second temperature.

### Claim 8 (depends on 6)

The method of claim 6 wherein the heating the phosphoric acid/sulfuric acid mixture to the etching temperature includes using an exothermic reaction between the sulfuric acid and the water vapor or hot water.

### Claim 9 (depends on 6)

The method of claim 6 wherein etching the material layer with the heated phosphoric acid/sulfuric acid mixture includes etching a material layer that includes silicon-containing portions and silicon nitride portions, wherein the heated phosphoric acid/sulfuric acid mixture selectively etches the silicon nitride portions.

### Claim 10 (depends on 9)

The method of claim 9 wherein the silicon-containing portions are silicon oxide portions of the material layer.

### Claim 11 (depends on 1)

The method of claim 1 wherein the etching temperature is greater than or equal to about 120° C.

### Claim 12 (depends on 6)

The method of claim 6 wherein the etching temperature is greater than or equal to about 120° C.

### Claim 13 (depends on 1)

The method of claim 1 wherein the phosphoric acid/sulfuric acid mixture has a lower viscosity than the phosphoric acid.

### Claim 14 (depends on 13)

The method of claim 13 wherein the lower viscosity of the phosphoric acid/sulfuric acid mixture results in at least one of improved etch selectivity, improved etch uniformity, and improved defectivity performance.

### Claim 15 (depends on 6)

The method of claim 6 wherein the phosphoric acid/sulfuric acid mixture has a lower viscosity than the phosphoric acid.

### Claim 16 (depends on 15)

The method of claim 15 wherein the lower viscosity of the phosphoric acid/sulfuric acid mixture results in at least one of improved etch selectivity, improved etch uniformity, and improved defectivity performance.