# US 9,355,845 B2 · Light induced nanowire assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,845 B2
- Document ID: US9355845B2
- Status: Granted
- Kind: B2
- Application number: 14/216,452
- Filed: 2014-03-17
- Published: 2014-09-18
- Granted: 2016-05-31
- Earliest claimed: 2013-03-15
- Assignees: University of Notre Dame du Lac
- Applicants: Nattasamon Petchsang; Masaru Kuno; Vladimir Plashnitsa
- Inventors: Nattasamon Petchsang; Masaru Kuno; Vladimir Plashnitsa
- Web page: https://patentgrep.com/patent/US9355845B2

## CPC

- H10P 14/265: {using solutions}
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/06: Silicon
- C30B 29/08: Germanium
- C30B 29/16: Oxides
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B 29/46: Sulfur-, selenium- or tellurium-containing compounds
- C30B 29/48: AIIBVI compounds {wherein A is Zn, Cd or Hg, and B is S, Se or Te}
- C30B 29/50: Cadmium sulfide
- C30B 29/60: characterised by shape
- C30B 33/04: using electric or magnetic fields or particle radiation
- H10P 14/3402: {characterised by the chemical composition}
- H10P 14/3424: {being Group IIB-VIA materials}
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10P 14/3461: {Nanoparticles}
- H10P 14/3462: {Nanowires}
- B82Y 40/00: Manufacture or treatment of nanostructures
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The invention provides a method for assembling semiconducting nanowires, which method can include providing a mixture comprising a dielectric solvent and two or more semiconducting nanowires, wherein the semiconducting nanowires can be the same or different; exposing the mixture to an electrostatic charge under lighting conditions; and allowing macroscopic nanowire alignment to occur, wherein each nanowire is substantially oriented along the direction of the applied electric field.

## Claims

### Claim 1

A method for assembling semiconducting nanowires into yarns, said method comprising:
providing a mixture, wherein the mixture comprises a dielectric solvent and at least two semiconducting nanowires;
loading said mixture into a conduit;
applying an electrostatic charge to a substrate;
depositing said mixture from said conduit on top of said charged substrate under lighting conditions; and
pulling said conduit away from said substrate in a direction along the surface normal.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the alignment area is from about 1 cm2 to 100 square feet.

### Claim 3 (depends on 1)

A method as set forth in claim 1, wherein said conduit is pulled away from said substrate in a direction along the surface normal at a rate of about 0.5 millimeters per second to about 50 mm/second.

### Claim 4 (depends on 1)

A method as set forth in claim 1, wherein said conduit is a pipette or a syringe.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said electrostatic charge is selected from (1) a unipolar charge of a positive sign applied to said substrate; or (2) a unipolar charge of a negative sign applied to said substrate.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said nanowires are selected from zinc oxide, zinc sulfide, zinc selenide, zinc telluride, cadmium sulfide, cadmium selenide, cadmium telluride, mercury sulfide, mercury selenide, mercury telluride, germanium sulfide, germanium selenide, germanium telluride, tin sulfide, tin selenide, tin telluride, lead sulfide, lead selenide, lead telluride, and lead selenium sulfide, Si, Ge, GaP, GaAs, InP, InAs, or a combination thereof.

### Claim 7 (depends on 1)

The method according to claim 1, wherein said substrate is selected from borosilicate, copper, or polytetrafluoroethylene, and wherein said dielectric solvent is selected from hexane, toluene, or a mixture thereof.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said substrate is charged by an electrostatic generator to deposit charges onto the substrate.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said nanowires are first washed to remove any excess ligand.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the source of said nanowires are nanowire solutions having concentrations from about 10−12 to about 10−11M.

### Claim 11 (depends on 1)

The method according to claim 1, wherein said lighting conditions are broad band illumination.

### Claim 12 (depends on 1)

The method according to claim 1, wherein said electrostatic charge ranges from about 10 V/cm to about 100 V/cm.

### Claim 13

A method for assembling semiconducting nanowires into segmented yarns, said method comprising:
providing more than one mixture, each more than one mixture comprising a dielectric solvent and at least two semiconducting nanowires;
depositing more than one of said mixtures on top of a polytetrafluoroethylene substrate;
applying an electrostatic charge to said substrate using a tissue or an electrostatic generator;
introducing a conduit into one of said more than one mixture and then removing said conduit, wherein a first yarn of at least two semiconducting nanowires is formed;
removing said conduit from said one of said more than one mixtures and placing the bottom of said first yarn of at least two semiconducting nanowires into a second of the other said more than one mixture,
wherein at least one yarn of at least two semiconducting nanowires is formed, the method characterized by assembling nanowires using LINA (light induced nanowire assembly), the LINA comprising applying lighting conditions to said at least two semiconducting nanowires; wherein said at least two semiconducting nanowires alligate into said first yarn during the removing of said conduit from one of said more than one mixture and said placing of the bottom of said first yarn of at least two semiconducting nanowires into said second of the other said more than one mixture to form segmented yarns.