# US 9,355,669 B2 · Perpendicularly magnetized thin film structure and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,669 B2
- Document ID: US9355669B2
- Status: Granted
- Kind: B2
- Application number: 13/678,856
- Filed: 2012-11-16
- Published: 2013-05-23
- Granted: 2016-05-31
- Earliest claimed: 2011-11-18
- Assignees: Korea Institute of Science and Technology
- Applicants: Korea Institute of Science and Technology
- Inventors: Gyung Min Choi; Byoung Chul Min; Kyung Ho Shin
- Web page: https://patentgrep.com/patent/US9355669B2

## CPC

- G11B 5/72: Protective coatings, e.g. anti-static {or antifriction}
- G11B 5/657: {containing inorganic, non-oxide compound of Si, N, P, B, H or C, e.g. in metal alloy or compound (containing oxygen G11B5/658)}
- G11B 5/674: {having differing macroscopic or microscopic structures, e.g. differing crystalline lattices, varying atomic structures or differing roughnesses}
- G11B 5/84: Processes or apparatus specially adapted for manufacturing record carriers
- H01F 10/123: {having a L10 crystallographic structure, e.g. [Co,Fe][Pt,Pd] thin films}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H01F 41/32: for applying conductive, insulating or magnetic material on a magnetic film {, specially adapted for a thin magnetic film}
- H10N 50/85: Materials of the active region
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H10N 50/01: Manufacture or treatment
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A perpendicularly magnetized thin film structure and a method of manufacturing the perpendicularly magnetized thin film structure are provided. The perpendicularly magnetized thin film structure includes i) a base layer, ii) a magnetic layer located on the base layer and having an L10-crystalline structure, and iii) a metal oxide layer located on the magnetic layer.

## Claims

### Claim 1

A perpendicularly magnetized thin film structure comprising:
a base layer;
a magnetic layer located on the base layer and having an L10-crystalline structure; and
a metal layer located on the magnetic layer, wherein only a surface of the metal layer is oxidized into a metal oxide layer and a part of the metal layer adjacent to the magnetic layer remains in a metal state without being oxidized, and wherein the metal oxide layer contains at least one metal oxide selected from a group of Cr2O3, ZrO2, ZnO, Cu2O, and NiO,
wherein the magnetic layer contains boron above 0 and not more than 50 at % and the metal oxide layer contains B2O3.

### Claim 2 (depends on 1)

The perpendicularly magnetized thin film structure of claim 1, wherein the metal oxide layer further contains at least one of metal oxide selected from a group of TiO2, Ta2O5, and Al2O3.

### Claim 3 (depends on 1)

The perpendicularly magnetized thin film structure of claim 1, wherein the magnetic layer contains a compound having a chemical formula of A100-xBx, the A is at least one element selected from a group of Fe(iron), Co(cobalt), Ni(nickel), Mn(manganese) or Cr(chromium), the B is at least one element selected from a group of Pt(platinum), Pd(palladium), Ni(nickel), Rh(rhodium), Au(gold), Hg(mercury) or Al(aluminum), and the x is 25 at % to 75 at %.

### Claim 4 (depends on 3)

The perpendicularly magnetized thin film structure of claim 3, wherein the x is 40 at % to 60 at %.

### Claim 5 (depends on 1)

The perpendicularly magnetized thin film structure of claim 1, further comprising an insulating layer located between the base layer and the magnetic layer.

### Claim 6 (depends on 5)

The perpendicularly magnetized thin film structure of claim 5, wherein the insulating layer includes an MgO layer and the thickness of the MgO layer is 2 nm or less.

### Claim 7 (depends on 5)

The perpendicularly magnetized thin film structure of claim 5, wherein the base layer includes a magnetic layer.

### Claim 8 (depends on 7)

The perpendicularly magnetized thin film structure of claim 7, wherein the magnetic layer of the base layer is made of at least one compound selected from a group of FePtB and CoPtB.

### Claim 9 (depends on 5)

The perpendicularly magnetized thin film structure of claim 5, further comprising another magnetic layer located between the insulating layer and the magnetic layer, having a BCC (Body Centered Cubic) crystalline structure, and containing at least one material selected from a group of CoFeB, CoFe and Fe.

### Claim 10 (depends on 5)

The perpendicularly magnetized thin film structure of claim 5, further comprising an electrode layer located on the metal oxide layer and the thickness of the metal oxide layer s smaller than the thickness of the magnetic layer.

### Claim 11

A method of manufacturing a perpendicularly magnetized thin film structure, comprising:
providing a base layer;
providing a magnetic layer on the base layer;
providing a metal layer on the magnetic layer; and
annealing the base layer, the magnetic layer, and the metal layer in a partial oxygen pressure,
wherein the annealing temperature is 400° C. to 900° C. and wherein the partial oxygen pressure in the annealing is 10−10 bar to 1 bar, wherein, in the annealing, the magnetic layer is transformed to have an L10-crystalline structure by tensile stress applied in parallel with the surface of the magnetic layer by the metal layer which is transformed into a metal oxide, the c axis of the magnetic layer is aligned perpendicular to the direction in which the film plane of the magnetic layer is extended, and the metal layer is transformed into a metal oxide layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein only a surface of the metal layer is oxidized into the metal oxide layer and a part of the metal layer adjacent to the magnetic layer remains in a metal state without being oxidized.

### Claim 13 (depends on 11)

The method of claim 11, further comprising:
providing an insulating layer between the base layer and the magnetic layer,
wherein, in the annealing, the insulating layer is annealed together with the base layer, the magnetic layer, and the metal layer.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
providing another magnetic layer between the insulating layer and the metal layer,
wherein, in the annealing, the magnetic layer is annealed together with the base layer, the insulating layer, the magnetic layer, and the metal layer.

### Claim 15 (depends on 11)

The method of claim 11, further comprising
reducing the thickness of the metal oxide layer after the annealing; and
providing an electrode layer on the metal oxide layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the reducing of the thickness of the metal oxide layer partially removes the metal oxide layer by performing argon on milling, reactive ion etching, or chemical-mechanical planarization on the metal oxide layer.

### Claim 17

A method of manufacturing a perpendicularly magnetized thin film structure, the method comprising:
forming a magnetic layer on a base layer such that the magnetic layer exhibits a magnetic easy direction in parallel to a surface between the magnetic layer and the base layer;
depositing a metal layer on the magnetic layer; and
annealing in a partial oxygen pressure the base layer, the magnetic layer, and the metal layer which oxidizes only a surface of the metal layer to form a metal oxide layer such that a part of the metal layer adjacent to the magnetic layer remains in a metal state without being oxidized and ensures perpendicular magnetic anisotropy of the magnetic layer as a result of oxidizing only a surface of the metal layer to form a metal oxide layer that transforms a phase of the magnetic layer into a L10-crystalline phase structure; and
wherein annealing is performed between 400° C. to 900° C. and the partial oxygen pressure in the annealing is between 10−10 bar to 1 bar,
wherein, as a result of annealing, the magnetic layer is transformed to have an L10-crystalline structure by tensile stress applied in parallel with the surface of the magnetic layer by the metal layer which is transformed into a metal oxide, the c axis of the magnetic layer is aligned perpendicular to the direction in which the film plane of the magnetic layer is extended, and the metal layer is transformed into a metal oxide layer.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
providing an insulating layer located between the base layer and the magnetic layer; and
forming an electrode layer on the metal oxide layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein
the metal oxide layer is selected from a group of TiO2, Ta2O5, Al2O3, Cr2O3, ZrO2, ZnO, Cu2O, and NiO;
the insulating layer includes an MgO layer and the thickness of the MgO layer is 2 nm or less; and
the magnetic layer contains a compound having a chemical formula of A100-xBx, the A is at least one element selected from a group of Fe(iron), Co(cobalt), Ni(nickel), Mn(manganese) or Cr(chromium), the B is at least one element selected from a group of Pt(platinum), Pd(palladium), Ni(nickel), Rh(rhodium), Au(gold), Hg(mercury) or Al(aluminum), and the x is 25 at % to 75 at %.