# US 9,355,631 B2 · Multilayer interlayer having sound damping properties over a broad temperature range

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,631 B2
- Document ID: US9355631B2
- Status: Granted
- Kind: B2
- Application number: 14/514,641
- Filed: 2014-10-15
- Published: 2016-04-21
- Granted: 2016-05-31
- Earliest claimed: 2014-10-15
- Assignees: Solutia Inc.
- Applicants: Solutia Inc.
- Inventors: Jun Lu
- Web page: https://patentgrep.com/patent/US9355631B2

## CPC

- G10K 11/168: Plural layers of different materials, e.g. sandwiches
- B32B 7/022: Mechanical properties
- B32B 17/10761: {containing vinyl acetal}
- B32B 27/08: of synthetic resin
- B32B 27/22: using plasticisers
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- B32B 2250/02: 2 layers
- B32B 2250/24: All layers being polymeric
- B32B 2250/246: All polymers belonging to those covered by groups B32B27/32 and B32B27/30
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/102: Insulating
- B32B 2307/536: Hardness
- B32B 2307/56: Damping, energy absorption
- B32B 2419/00: Buildings or parts thereof
- B32B 2605/006: Transparent parts other than made from inorganic glass, e.g. polycarbonate glazings
- G10K: SOUND-PRODUCING DEVICES; METHODS OR DEVICES FOR PROTECTING AGAINST, OR FOR DAMPING, NOISE OR OTHER ACOUSTIC WAVES IN GENERAL; ACOUSTICS NOT OTHERWISE PROVIDED FOR
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

A polymer interlayer having improved sound insulation is disclosed. The polymer interlayer comprises at least one soft layer wherein the soft layer comprises: a first poly(vinyl butyral) resin having a first residual hydroxyl content and a first glass transition temperature (Tg); a second poly(vinyl butyral) resin having a second residual hydroxyl content and a second glass transition temperature (Tg), wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 1.0 weight percent; wherein the difference between the first glass transition temperature (Tg) the second glass transition temperature (Tg) is at least 1.5° C.; and a plasticizer; at least one stiffer layer comprising a third poly(vinyl butyral resin) having a third residual hydroxyl content; and a plasticizer, wherein the polymer interlayer has a damping loss factor (η) (as measured by Mechanical Impedance Measurement according to ISO 16940) of at least about 0.16 measured at two or more different temperatures selected from 10° C., 20° C. and 30° C.

## Claims

### Claim 1

A polymer interlayer having improved sound insulation, the polymer interlayer comprising:
at least one soft layer wherein the soft layer comprises a blend of two or more poly(vinyl butyral) resins comprising:
a first poly(vinyl butyral) resin having a first residual hydroxyl content and a first glass transition temperature (Tg);
a second poly(vinyl butyral) resin having a second residual hydroxyl content and a second glass transition temperature (Tg),
wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 1.0 weight percent;
wherein the difference between the first glass transition temperature (Tg) and the second glass transition temperature (Tg) is at least 1.5° C.; and
a plasticizer, wherein the first poly(vinyl butyral) resin, the second poly(vinyl butyral) resin and the plasticizer are mixed and melt-extruded to form the at least one soft layer;
at least one stiffer layer comprising a third poly(vinyl butyral) resin having a third residual hydroxyl content; and
a plasticizer,
wherein the polymer interlayer has a damping loss factor (η) (as measured by Mechanical Impedance Measurement according to ISO 16940) of at least about 0.16 measured at two or more different temperatures selected from 10° C., 20° C. and 30° C.

### Claim 2 (depends on 1)

The polymer interlayer of claim 1, wherein the second poly(vinyl butyral) resin is present in an amount of from about 5 weight percent to about 50 weight percent.

### Claim 3 (depends on 1)

The polymer interlayer of claim 1, wherein the second poly(vinyl butyral) resin is present in an amount of from about 25 weight percent to about 50 weight percent.

### Claim 4 (depends on 1)

The polymer interlayer of claim 1, wherein each plasticized resin in the soft layer of the polymer interlayer has a glass transition temperature (Tg) less than 20.0° C.

### Claim 5 (depends on 1)

The polymer interlayer of claim 1, wherein the residual hydroxyl content of the third poly(vinyl butyral) resin is the same as the residual hydroxyl content of the first poly(vinyl butyral) resin or the second poly(vinyl butyral) resin.

### Claim 6 (depends on 1)

The polymer interlayer of claim 1, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 2.0 weight percent.

### Claim 7 (depends on 1)

The polymer interlayer of claim 1, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 3.0 weight percent.

### Claim 8 (depends on 1)

The polymer interlayer of claim 1, wherein the difference between the glass transition temperatures (Tg) of the first poly(vinyl butyral) resin and the second poly(vinyl butyral) resin is at least 3.0° C.

### Claim 9

A polymer interlayer having improved sound insulation, the polymer interlayer comprising:
at least one soft layer wherein the soft layer comprises a blend of two or more poly(vinyl butyral) resins comprising:
a first poly(vinyl butyral) resin having a first residual hydroxyl content and a first glass transition temperature (Tg);
a second poly(vinyl butyral) resin having a second residual hydroxyl content and a second glass transition temperature (Tg),
wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 1.0 weight percent;
wherein the difference between the first glass transition temperature (Tg) and the second glass transition temperature (Tg) is at least 1.5° C.; and
a plasticizer, wherein the first poly(vinyl butyral) resin, the second poly(vinyl butyral) resin and the plasticizer are mixed and melt-extruded to form the at least one soft layer;
at least one stiffer layer comprising a third poly(vinyl butyral) resin having a third residual hydroxyl content; and
a plasticizer,
wherein the polymer interlayer has a damping loss factor (η) (as measured by Mechanical Impedance Measurement according to ISO 16940) of at least about 0.16 measured at two or more different temperatures selected from 10° C., 20° C. and 30° C., and wherein the second poly(vinyl butyral) resin is present in an amount of from about 5 weight percent to about 50 weight percent.

### Claim 10 (depends on 9)

The polymer interlayer of claim 9, wherein each plasticized resin in the soft layer of the polymer interlayer has a glass transition temperature (Tg) less than 20.0° C.

### Claim 11 (depends on 9)

The polymer interlayer of claim 9, wherein the residual hydroxyl content of the third poly(vinyl butyral) resin is the same as the residual hydroxyl content of the first poly(vinyl butyral) resin or the second poly(vinyl butyral) resin.

### Claim 12 (depends on 9)

The polymer interlayer of claim 9, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 2.0 weight percent.

### Claim 13 (depends on 9)

The polymer interlayer of claim 9, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 3.0 weight percent.

### Claim 14 (depends on 9)

The polymer interlayer of claim 9, wherein difference between the glass transition temperatures (Tg) of the first poly(vinyl butyral) resin and the second poly(vinyl butyral) resin is at least 3.0° C.

### Claim 15

A polymer interlayer having improved sound insulation, the polymer interlayer comprising:
at least one soft layer wherein the soft layer comprises a blend of two or more poly(vinyl butyral) resins comprising:
a first poly(vinyl butyral) resin having a first residual hydroxyl content and a first glass transition temperature (Tg);
a second poly(vinyl butyral) resin having a second residual hydroxyl content and a second glass transition temperature (Tg),
wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 1.0 weight percent,
wherein the difference between the first glass transition temperature (Tg) and the second glass transition temperature (Tg) is at least 1.5° C.; and
a plasticizer, wherein the first poly(vinyl butyral) resin, the second poly(vinyl butyral) resin and the plasticizer are mixed and melt-extruded to form the at least one soft layer;
at least one stiffer layer comprising a third poly(vinyl butyral) resin having a third residual hydroxyl content; and
a plasticizer,
wherein each plasticized resin in the soft layer of the polymer interlayer has a glass transition temperature (Tg) less than 20.0° C.

### Claim 16 (depends on 15)

The polymer interlayer of claim 15, wherein the second poly(vinyl butyral) resin is present in an amount of from about 5 weight percent to about 50 weight percent.

### Claim 17 (depends on 15)

The polymer interlayer of claim 15, wherein the second poly(vinyl butyral) resin is present in an amount of from about 25 weight percent to about 50 weight percent.

### Claim 18 (depends on 15)

The polymer interlayer of claim 15, wherein the difference between the glass transition temperatures (Tg) of the first poly(vinyl butyral) resin and the second poly(vinyl butyral) resin is at least 3.0° C.

### Claim 19 (depends on 15)

The polymer interlayer of claim 15, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 2.0 weight percent.

### Claim 20 (depends on 15)

The polymer interlayer of claim 15, wherein the difference between the first residual hydroxyl content and the second residual hydroxyl content is at least 3.0 weight percent.