# US 9,355,362 B2 · Quantum bits and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,355,362 B2
- Document ID: US9355362B2
- Status: Granted
- Kind: B2
- Application number: 13/294,473
- Filed: 2011-11-11
- Published: 2013-05-16
- Granted: 2016-05-31
- Earliest claimed: 2011-11-11
- Assignees: Northrop Grumman Systems Corporation
- Applicants: Patrick B. Shea; Erica C. Folk; Daniel J. Ewing; John J. Talvacchio
- Inventors: Patrick B. Shea; Erica C. Folk; Daniel J. Ewing; John J. Talvacchio
- Web page: https://patentgrep.com/patent/US9355362B2

## CPC

- H10N 60/12: Josephson-effect devices
- H10N 60/0912: {of Josephson-effect devices}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Methods are provided of forming a Josephson junction (JJ) quantum bit (qubit). In one embodiment, the method comprises forming a JJ trilayer on a substrate. The JJ trilayer is comprised of a dielectric layer sandwiched between a bottom superconductor material layer and a top superconductor material layer. The method further comprises performing a thermal hardening process on the JJ trilayer to control diffusion of the dielectric layer into the bottom superconductor material layer and the top superconductor material layer, and etching openings in the JJ trilayer to form one or more JJ qubits.

## Claims

### Claim 1

A method of forming Josephson junction (JJ) quantum bits (qubit)s, the method comprising:
forming a JJ trilayer on a substrate, the JJ trilayer being comprised of a dielectric layer sandwiched between a bottom superconductor material layer and a top superconductor material layer;
performing a thermal hardening process on the JJ trilayer to control diffusion of the dielectric layer into the bottom superconductor layer and the top superconductor material layer, wherein the thermal hardening process comprises annealing the JJ trilayer in an inert environment; and
etching openings in the JJ trilayer to form one or more JJ qubits.

### Claim 2 (depends on 1)

The method of claim 1, wherein the JJ trilayer is annealed at a temperature between about 150° C. to about 400° C. for a time period between about 15 minute to about 120 minutes.

### Claim 3 (depends on 1)

The method of claim 1, wherein the thermal hardening process tunes the critical current density from a first critical current density defined by the respective dimensions of the associated one or more qubits to a second current density defined by the thermal hardening process, wherein the controlled diffusion mitigates further deleterious effects caused by subsequent semiconductor processes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the dielectric layer is aluminum oxide (Al2O3), and each of the bottom and top superconductor material layers are aluminum (Al) or aluminum-copper (Al—Cu).

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
depositing a protective barrier layer over the JJ trilayer;
curing the protective barrier layer;
depositing a photoresist material layer over the protective barrier layer;
irradiating and developing the photoresist material layer to form an opening pattern in the photoresist material layer;
etching the protective barrier layer to form openings in the protective barrier layer based on the opening pattern;
etching the JJ trilayer based on the openings in the protective barrier layer to form openings in the JJ trilayer layer that define a first set of superconductor material raised portions; and
stripping the photoresist material layer and the protective barrier layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the protective barrier layer is cured at a temperature of about 150° C. to about 180° C. for about 60 to about 120 seconds.

### Claim 7 (depends on 5)

The method of claim 5, wherein the top superconductive material layer is aluminum and developer utilized to develop the photoresist material layer contains sodium hydroxide, such that the protective barrier layer protects the aluminum from the sodium hydroxide during developing of the photoresist material layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein a protective barrier layer is employed for separate etching steps for both the top and bottom superconductor material layers.

### Claim 9

A method of forming Josephson junction (JJ) quantum bits (qubits), the method comprising:
depositing a first superconductor material layer over a substrate;
forming a dielectric layer over the first superconductor material layer;
depositing a second superconductor material layer over the dielectric layer, the first superconductor material layer, the dielectric layer and the second superconductor material layer forming a JJ trilayer;
annealing the JJ trilayer in an inert environment at a temperature between about 150° C. to about 400° C. for a time period between about 15 minute to about 120 minutes to control diffusion of the dielectric layer into the first superconductor material layer and the second superconductor material layer; and
etching openings in the JJ trilayer to form one or more JJ qubits.

### Claim 10 (depends on 9)

The method of claim 9, wherein annealing shifts the critical current density from a first critical current density defined by the respective dimensions of the associated one or more JJ qubits to a second current density defined by the annealing, wherein the controlled diffusion mitigates further deleterious effects caused by subsequent semiconductor processes.

### Claim 11 (depends on 9)

The method of claim 9, wherein the dielectric layer is aluminum oxide (Al2O3), and each of the first and second superconductor material layers are aluminum (Al) or aluminum-copper (Al—Cu).

### Claim 12 (depends on 9)

The method of claim 9, wherein the annealing is performed after the formation of the one or more JJ qubits.

### Claim 13 (depends on 9)

The method of claim 9, further comprising:
depositing a protective barrier layer over the JJ trilayer;
curing the protective barrier layer;
depositing a photoresist material layer over the protective barrier layer;
irradiating and developing the photoresist material layer to form an opening pattern in the photoresist material layer;
etching the protective barrier layer to form openings in the protective barrier layer based on the opening pattern;
etching the JJ trilayer based on the openings in the protective barrier layer to form openings in the JJ trilayer layer that define a first set of superconductor material raised portions; and
stripping the photoresist material layer and the protective barrier layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the protective barrier layer is cured at a temperature of about 150° C. to about 180° C. for about 60 to about 120 seconds.

### Claim 15 (depends on 13)

The method of claim 13, wherein a protective barrier layer is employed for separate etching steps for both the first and second superconductor material layer.