# US 9,354,519 B2 · Methods of forming patterns

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,354,519 B2
- Document ID: US9354519B2
- Status: Granted
- Kind: B2
- Application number: 14/621,049
- Filed: 2015-02-12
- Published: 2016-03-17
- Granted: 2016-05-31
- Earliest claimed: 2014-09-16
- Assignees: SK hynix Inc.
- Applicants: SK hynix Inc.
- Inventors: Keun Do Ban; Cheol Kyu Bok; Jung Gun Heo; Hong Ik Kim
- Web page: https://patentgrep.com/patent/US9354519B2

## CPC

- C09D 153/00: Coating compositions based on block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Coating compositions based on derivatives of such polymers
- G03F 7/0002: {Lithographic processes using patterning methods other than those involving the exposure to radiation, e.g. by stamping}
- G03F 7/002: {using materials containing microcapsules; Preparing or processing such materials, e.g. by pressure; Devices or apparatus specially designed therefor}
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G03F 7/165: {Monolayers, e.g. Langmuir-Blodgett}
- G03F 7/322: {Aqueous alkaline compositions}
- G03F 7/325: {Non-aqueous compositions}
- G03F 7/40: Treatment after imagewise removal, e.g. baking
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/2043: {using an anti-reflective coating}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- C08F 293/00: Macromolecular compounds obtained by polymerisation on to a macromolecule having groups capable of inducing the formation of new polymer chains bound exclusively at one or both ends of the starting macromolecule (on to polymers modified by introduction of unsaturated end groups C08F290/02)
- C08L 53/005: {Modified block copolymers}
- H10P 95/08: {Planarisation of organic insulating materials}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method of forming patterns includes: forming guide patterns on an underlying layer, forming a self-assembling block copolymer (BCP) layer on the guide patterns and the underlying layer, annealing the self-assembling BCP layer to form first polymer block domains and second polymer block domains which are alternately and repeatedly arrayed, and selectively removing the first polymer block domains. The guide patterns are formed of a developable antireflective material. In addition, the guide patterns are spaced apart from each other such that a width of each of the guide patterns is less than a distance between the guide patterns.

## Claims

### Claim 1

A method of forming patterns, the method comprising:
forming a developable antireflective layer on an underlying layer disposed on a semiconductor substrate;
forming a photoresist layer on the developable antireflective layer;
selectively exposing portions of the photoresist layer and portions of the developable antireflective layer to light;
selectively removing non-exposed portions of the photoresist layer to form a photoresist pattern exposing non-exposed portions of the developable antireflective layer;
selectively removing the exposed portions of the developable antireflective layer to form guide patterns;
forming a neutral layer that fills a space between the guide patterns;
forming a self-assembling block copolymer (BCP) layer on the guide patterns and the neutral layer;
annealing the self-assembling BCP layer to form first polymer block domains and second polymer block domains, which are alternately and repeatedly arrayed; and
selectively removing the first polymer block domains.

### Claim 2 (depends on 1)

The method of claim 1, wherein the selectively removing non-exposed portions of the photoresist layer is performed using a negative tone developer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the selectively removing the exposed portions of the developable antireflective layer is performed using a positive tone developer.

### Claim 4 (depends on 3)

The method of claim 3, wherein the positive tone developer is an alkaline developer including a tetra-methyl ammonium hydroxide (TMAH) material.

### Claim 5

The method of claim
wherein add is generated in the exposed portions of the photoresist layer when the portions of the photoresist layer and the portions of the developable antireflective layer are exposed to the light; and
wherein the acid generated in the exposed portions of the photoresist layer is diffused into the exposed portions of the developable antireflective layer so that the exposed portions of the developable antireflective layer are dissolved by the positive tone developer.

### Claim 6 (depends on 5)

The method of claim 5, further comprising applying a post exposure bake (PEB) step to the exposed photoresist layer to accelerate the generation of acid in the exposed portions of the photoresist layer and accelerate diffusion of the acid into the exposed portions of the developable antireflective layer.

### Claim 7 (depends on 3)

The method of claim 3, wherein the photoresist pattern is removed while the exposed portions of the developable antireflective layer are selectively removed using the positive tone developer.

### Claim 8 (depends on 3)

The method of claim 3, further comprising removing a side surface portion of the photoresist pattern with an organic solvent to expose edge portions of the exposed portions of the developable antireflective layer.

### Claim 9 (depends on 1)

The method of claim 1, wherein the self-assembling BCP layer includes a first polymer block component and a second polymer block component, which are suitable for phase separation during the annealing of the self-assembling BCP layer; and
wherein the first polymer block domains are formed of the first polymer block component and the second polymer block domains are formed of the second polymer block component.

### Claim 10 (depends on 9)

The method of claim 9,
wherein the developable antireflective layer is formed material that has greater affinity to the first polymer block component than to the second polymer block component; and
wherein the first polymer block domains are formed on the guide patterns when the self-assembling BCP layer is annealed.

### Claim 11 (depends on 9)

The method of claim 9,
wherein the self-assembling BCP layer includes a polystyrene-poly(meta methyl acrylate) block copolymer (PS-b-PMMA) material; and
wherein the developable antireflective layer includes an organic material having a greater affinity to the PMMA polymer block component than to the PS polymer block component.

### Claim 12 (depends on 9)

The method of claim 9, wherein the neutral layer has substantially the same affinity to both the first and second polymer block components, so that the first polymer block domains and the second polymer block domains are alternately and repeatedly arrayed on the neutral layer.

### Claim 13 (depends on 9)

The method of claim 9, wherein forming the neutral layer includes:
preparing a polymer material having hydroxyl groups (—OH groups) that act as terminal groups to bond with the underlying layer, which is exposed by the guide patterns;
coating the polymer material having the hydroxyl groups on the guide patterns and the underlying layer;
annealing the polymer material to bond the hydroxyl groups of the polymer material with the underlying layer; and
selectively removing the polymer material on the guide patterns using a polymer brush process,
wherein the polymer brush process is performed using a solvent.

### Claim 14 (depends on 1)

The method of claim 1, wherein the neutral layer is formed to have a top surface that is substantially coplanar with top surfaces of the guide patterns.

### Claim 15 (depends on 1)

The method of claim 1, wherein the guide patterns are spaced apart from each other such that a distance between the guide patterns is “W×(2N−1)”; and
wherein, “N” denotes a natural number which is equal to or greater than 2 and “W” denotes a width of each of the guide patterns.

### Claim 16

A method of forming patterns, the method comprising forming a developable antireflective layer on an underlying layer disposed on a semiconductor substrate;
forming a photoresist layer on the developable antireflective layer;
selectively exposing portions of the photoresist layer and portions of the developable antireflective layer to light to define line-shaped non-exposed portions of the photoresist layer and the developable antireflective layer;
selectively removing the non-exposed portions of the photoresist layer to form a photoresist pattern that provides trenches exposing the non-exposed portions of the developable antireflective layer;
selectively removing the exposed portions of the developable antireflective layer to form line-shaped guide patterns having a width which is less than a distance between the line-shaped guide patterns;
forming a neutral layer that fills a space between the guide patterns;
forming a self-assembling block copolymer (BCP) layer on the guide patterns and the neutral layer;
annealing the self-assembling BCP layer to form line-shaped first polymer block domains and line-shaped second polymer block domains, which are alternately and repeatedly arrayed; and
selectively removing the first polymer block domains.

### Claim 17

A method of forming patterns, the method comprising:
forming a developable antireflective layer on an underlying layer disposed on a semiconductor substrate;
forming a photoresist layer on the developable antireflective layer;
selectively exposing portions of the photoresist layer and portions of the developable antireflective layer to light to define circular-shaped non-exposed portions of the photoresist layer and the developable antireflective layer;
selectively removing the non-exposed portions of the photoresist layer to form a photoresist pattern exposing the non-exposed portions of the developable antireflective layer;
selectively removing the exposed portions of the developable antireflective layer to form circular-shaped guide patterns having a width that is less than a distance between the circular-shaped guide patterns;
forming a neutral aye that fills a space between the guide patterns;
forming a self-assembling block copolymer (BCP) layer on the guide patterns and the neutral layer;
annealing the self-assembling BCP layer to form first polymer block domains and second polymer block domains surrounding sidewalls of the first polymer block domains; and
selectively removing the first polymer block domains to form holes.

### Claim 18 (depends on 17)

The method of claim 17, wherein the selectively removing the non-exposed portions of the photoresist layer is performed using a negative tone developer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the selectively removing the exposed portions of the developable antireflective layer is performed using a positive tone developer.

### Claim 20 (depends on 19)

The method of claim 19,
wherein acid is generated in the exposed portions of the photoresist layer while the portions of the photoresist layer and the portions of the developable antireflective layer are exposed to the light; and
wherein the acid generated in the exposed portions of the photoresist layer diffuses into the exposed portions of the developable antireflective layer such that the exposed portions of the developable antireflective layer are suitable for being dissolved by the positive tone developer.