# US 9,354,509 B2 · Mask blank, transfer mask, method of manufacturing a transfer mask, and method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,354,509 B2
- Document ID: US9354509B2
- Status: Granted
- Kind: B2
- Application number: 14/222,794
- Filed: 2014-03-24
- Published: 2014-07-24
- Granted: 2016-05-31
- Earliest claimed: 2011-09-14
- Assignees: Hoya Corporation
- Applicants: Hoya Corporation
- Inventors: Noriyuki Sakaya; Osamu Nozawa
- Web page: https://patentgrep.com/patent/US9354509B2

## CPC

- G03F 1/26: Phase shift masks [PSM]; PSM blanks; Preparation thereof
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- G03F 1/28: with three or more diverse phases on the same PSM; Preparation thereof
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G03F 7/20: Exposure; Apparatus therefor (photographic printing apparatus for making copies G03B27/00)
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A mask blank is used for manufacturing a binary mask adapted to be applied with ArF excimer laser exposure light and has a light-shielding film for forming a transfer pattern on a transparent substrate. The light-shielding film has a laminated structure of a lower layer and an upper layer and has an optical density of 2.8 or more for the exposure light. The lower layer is made of a material containing tantalum and nitrogen and has a thickness of 33 nm or more. The upper layer is made of a material containing tantalum and oxygen and has a thickness of 3 nm or more. The phase difference between the exposure light transmitted through the light-shielding film and the exposure light transmitted in air for a distance equal to the thickness of the light-shielding film is 60 degrees or less.

## Claims

### Claim 1

A mask blank for manufacturing a binary mask adapted to be applied with ArF excimer laser exposure light, comprising:
a transparent substrate; and
a light-shielding film formed on the transparent substrate, the light-shielding film serving to form a transfer pattern;
wherein the light-shielding film has a laminated structure of a lower layer and an upper layer and has an optical density of 2.8 or more for the exposure light,
the lower layer has a refractive index n of less than 2.0 and an extinction coefficient k of 2.0 or more and has a thickness of 33 nm or more,
the upper layer has an extinction coefficient k of 1.3 or more and has a thickness of 3 nm or more, and
a phase difference between the exposure light transmitted through the light-shielding film and the exposure light transmitted in air for a distance equal to a thickness of the light-shielding film is 60 degrees or less.

### Claim 2 (depends on 1)

The mask blank according to claim 1, wherein the upper layer has a refractive index n of 2.5 or less.

### Claim 3 (depends on 1)

The mask blank according to claim 1, wherein the upper layer has an extinction coefficient k of less than 2.0.

### Claim 4 (depends on 1)

The mask blank according to claim 1, wherein the upper layer has a thickness of 15 nm or less.

### Claim 5 (depends on 1)

The mask blank according to claim 1, wherein the light shielding film has a front-surface reflectance of 40% or less for the exposure light.

### Claim 6 (depends on 1)

A method of manufacturing a transfer mask, comprising:
an etching step of patterning, by etching, the light-shielding film in the mask blank according to claim 1.

### Claim 7

A binary transfer mask adapted to be applied with ArF excimer laser exposure light, comprising:
a transparent substrate; and
a light-shielding film formed on the a transparent substrate, the light-shielding film having a transfer pattern;
wherein the light-shielding film has a laminated structure of a lower layer and an upper layer and has an optical density of 2.8 or more for the exposure light,
the lower layer has a refractive index n of less than 2.0 and an extinction coefficient k of 2.0 or more and has a thickness of 33 nm or more,
the upper layer has an extinction coefficient k of 1.3 or more and has a thickness of 3 nm or more, and
a phase difference between the exposure light transmitted through the light-shielding film and the exposure light transmitted in air for a distance equal to a thickness of the light-shielding film is 60 degrees or less.

### Claim 8 (depends on 7)

The binary transfer mask according to claim 7, wherein the upper layer has a refractive index n of 2.5 or less.

### Claim 9 (depends on 7)

The binary transfer mask according to claim 7, wherein the upper layer has an extinction coefficient k of less than 2.0.

### Claim 10 (depends on 7)

The binary transfer mask according to claim 7, wherein the upper layer has a thickness of 15 nm or less.

### Claim 11 (depends on 7)

The binary transfer mask according to claim 7, wherein the light shielding film has a front-surface reflectance of 40% or less for the exposure light.

### Claim 12 (depends on 7)

The binary transfer mask according to claim 7, wherein the transfer pattern of the light-shielding film includes a line & space pattern of half-pitch 45 nm or less.

### Claim 13 (depends on 7)

A method of manufacturing a semiconductor device, comprising:
exposing and transferring the transfer pattern to a resist film on a semiconductor substrate using the binary transfer mask according to claim 7.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the transfer pattern which is transferred to the resist film on the semiconductor substrate includes a line & space pattern of half-pitch 45 nm or less.