# US 9,353,578 B2 · Hardfacing compositions, methods of applying the hardfacing compositions, and tools using such hardfacing compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,578 B2
- Document ID: US9353578B2
- Status: Granted
- Kind: B2
- Application number: 12/728,932
- Filed: 2010-03-22
- Published: 2010-09-23
- Granted: 2016-05-31
- Earliest claimed: 2009-03-20
- Assignees: Smith International, Inc.
- Applicants: Sike Xia; Zhou Yong
- Inventors: Sike Xia; Zhou Yong
- Web page: https://patentgrep.com/patent/US9353578B2

## CPC

- E21B 10/50: the bit being of roller type
- C22C 29/005: {comprising a particular metallic binder}
- C22C 29/08: based on tungsten carbide
- B22F 2005/001: {Cutting tools, earth boring or grinding tool other than table ware}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A hardfacing composition comprising an iron-based binder alloy; and a carbide phase comprising a sintered carbide and a cast tungsten carbide, wherein the cast carbide is present in a quantity of at least 22% by weight, based on the total weight of the carbide phase, and the cast carbide comprises particles having sizes in the range of from 30 to 60 mesh. Also provided is a hardfacing composition comprising an iron-based binder alloy; and a carbide phase comprising a super dense sintered carbide and one or more additional carbide materials, wherein the super dense sintered carbide is present in a quantity of at least 10 percent by weight (% w), based on the total weight of the carbide phase, and comprises particles having sizes in the range of from 16 to 40 mesh. Included are methods of manufacturing such hardfacing compositions and downhole tools having such improved hardfacing compositions applied thereon.

## Claims

### Claim 1

A hardfacing composition comprising:
an iron-based binder alloy; and
a carbide phase comprising a sintered carbide and a cast tungsten carbide, wherein the cast carbide is present in a quantity of at least 22% and no greater than 40% by weight, based on the total weight of the carbide phase, wherein the cast carbide comprises particles having sizes in the range of from 30 to 60 mesh, and wherein the sintered carbide comprises particles having sizes in the range of from 16 to 50 mesh, and wherein only a portion of the sintered carbide particles comprise a super dense sintered carbide having a predominantly closed porosity or are free of pores, and wherein a first quantity of the super dense sintered carbide particles have sizes in the range of from 16 to 25 mesh (−16/+25 mesh) and a second quantity of the super dense sintered carbide particles have sizes in the range of from 25 to 50 mesh (−25/+50 mesh).

### Claim 2 (depends on 1)

The hardfacing composition of claim 1, wherein the cast tungsten carbide comprises crushed cast tungsten carbide.

### Claim 3 (depends on 1)

The hardfacing composition of claim 1, wherein the quantity of cast carbide is in the range of from 22.5% to 40% by weight, based on the total weight of the carbide phase.

### Claim 4 (depends on 1)

The hardfacing composition of claim 1, wherein the particles of cast carbide have sizes in the range of from 40 to 60 mesh.

### Claim 5 (depends on 1)

The hardfacing composition of claim 1, wherein the cast tungsten carbide has a core of cast tungsten carbide and a shell of monotungsten carbide.

### Claim 6 (depends on 5)

The hardfacing composition of claim 5, wherein said cast carbide comprises tungsten carbide particles having a bound carbon content in the range from 4% by weight to 6% by weight based on a total weight of the particles.

### Claim 7 (depends on 1)

The hardfacing composition of claim 1, wherein the quantity of sintered carbide is in the range of from 10% to 70% by weight, based on the total weight of the carbide phase.

### Claim 8 (depends on 1)

The hardfacing composition of claim 1, wherein the quantity of sintered carbide is in the range of from 30% to 65% by weight, based on the total weight of the carbide phase, and has particles with sizes in the range of from 16 to 40 mesh.

### Claim 9 (depends on 1)

The hardfacing composition of claim 1, wherein the carbide phase further comprises a filler carbide in a quantity of from 5% to 15% by weight, based on the total weight of the carbide phase, and the filler carbide particles have sizes in the range of from 200 to 625 mesh.

### Claim 10 (depends on 1)

The hardfacing composition of claim 1, wherein the amount of cast carbide is at least 1% w greater than the second quantity of sintered carbide, based on the weight percentages calculated based on the total weight of the carbide phase.

### Claim 11 (depends on 1)

The hardfacing composition of claim 1, wherein the first quantity and second quantity of sintered carbide is super dense sintered carbide having a predominantly closed porosity or is free of pores.

### Claim 12 (depends on 11)

The hardfacing composition of claim 11, wherein the first quantity of sintered carbide has particles with sizes in the range of from 16 to 20 mesh (−16/+20 mesh) and a second quantity of sintered carbide has particles with sizes in the range of from 30 to 40 mesh (−30/+40 mesh).

### Claim 13 (depends on 1)

The hardfacing composition of claim 1, wherein the carbide phase is present in an amount of from 50% to 75% by weight, based on the total weight of the hardfacing composition.

### Claim 14 (depends on 1)

The hardfacing composition of claim 1, wherein the binder alloy is present in an amount of from 25% to 50% by weight, based on the total weight of the hardfacing composition.

### Claim 15 (depends on 1)

The hardfacing composition of claim 1, wherein the sintered carbide is spherical and comprises tungsten carbide and cobalt.

### Claim 16 (depends on 1)

The hardfacing composition of claim 1, wherein the cast carbide is present in a quantity of 25% to 40% by weight.

### Claim 17 (depends on 1)

The hardfacing composition of claim 1, wherein the cast carbide is present in a quantity of 25% to 35% by weight.

### Claim 18 (depends on 1)

The hardfacing composition of claim 1, wherein the cast carbide is present in a quantity of 24% to 34% by weight.

### Claim 19

A hardfacing composition comprising:
an iron-based binder alloy; and
a carbide phase comprising a super dense sintered carbide and one or more additional carbides, wherein the super dense sintered carbide comprises particles having sizes in the range of from 16 to 40 mesh, wherein the carbide phase comprises a first quantity of super dense sintered carbide having particles with sizes in the range of from 16 to 25 mesh, said first quantity of super dense sintered carbide being in the range of 10% w to 70% w of the total weight of the carbide phase, and a second quantity of super dense sintered carbide having a particles with sizes of at least 25 mesh.

### Claim 20 (depends on 19)

The hardfacing composition of claim 19, wherein the second quantity of super dense sintered carbide has particles with sizes in the range of from 25 to 75 mesh.

### Claim 21 (depends on 20)

The hardfacing composition of claim 20, wherein the first quantity is greater than the second quantity by no greater than 15%.

### Claim 22

A hardfacing composition comprising:
an iron-based binder alloy; and
a carbide phase comprising a sintered carbide phase including a super dense sintered carbide and wherein the carbide phase comprises one or more additional carbides, wherein the sintered carbide phase comprises a first quantity of the sintered carbide particles have sizes in the range of from 16 to 25 mesh (−16/+25 mesh) and a second quantity of the sintered carbide particles have sizes in the range of from 25 to 50 mesh (−25/+50 mesh), wherein the first quantity of sintered carbide is present in an amount of at least 10% w, wherein the first quantity larger than the second quantity, and wherein the super dense sintered carbide is present in a quantity of 22.5% w to 47.5% w based on the total weight of the carbide phase.