# US 9,353,458 B2 · Base substrate for epitaxial diamond film, method for producing the base substrate for epitaxial diamond film, epitaxial diamond film produced with the base substrate for epitaxial diamond film, and method for producing the epitaxial diamond film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,458 B2
- Document ID: US9353458B2
- Status: Granted
- Kind: B2
- Application number: 12/225,570
- Filed: 2007-02-05
- Published: 2009-07-09
- Granted: 2016-05-31
- Earliest claimed: 2006-03-31
- Assignees: Atsuhito Sawabe
- Applicants: Atsuhito Sawabe; Hitoshi Noguchi; Shintaro Maeda
- Inventors: Atsuhito Sawabe; Hitoshi Noguchi; Shintaro Maeda
- Web page: https://patentgrep.com/patent/US9353458B2

## CPC

- C30B 23/02: Epitaxial-layer growth
- C23C 16/272: {using DC, AC or RF discharges}
- C30B 25/105: {by irradiation or electric discharge}
- C30B 25/18: characterised by the substrate
- C30B 29/02: Elements
- C30B 29/04: Diamond
- H01J 37/32009: {Arrangements for generation of plasma specially adapted for examination or treatment of objects, e.g. plasma sources (plasma generation in general H05H1/24)}
- H01J 37/34: operating with cathodic sputtering (H01J37/36 takes precedence {; methods of cathodic sputtering C23C14/34})
- H01J 37/3447: {Collimators, shutters, apertures}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3241: {being conductive materials}
- H10P 14/3258: {Crystal orientation}
- H10P 14/3406: {Carbon, e.g. diamond-like carbon}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a base substrate for epitaxial diamond film capable of epitaxially growing a large area of high quality diamond, having a diameter of 1 inch (2.5 cm) or more, on an iridium base by using the CVD method, a method for producing the base substrate for epitaxial diamond film, an epitaxial diamond film produced with the base substrate for epitaxial diamond film and a method for producing the epitaxial diamond film. An iridium (Ir) film is formed by epitaxial growth on a single crystal magnesium oxide (MgO) substrate or a single crystal sapphire (α-Al2O3) substrate by means of a vacuum deposition method or a sputtering method, and a bias nucleus generation process of forming epitaxial diamond nuclei is applied to the surface of the iridium (Ir) base formed as a film by exposing an ion-containing direct current plasma to the surface of the iridium (Ir) base formed as a film.

## Claims

### Claim 1

A method for producing a base substrate for epitaxial diamond film, comprising:
forming an iridium (Ir) base by epitaxial growth of an iridium (Ir) film on a surface of a single crystal magnesium oxide (MgO) substrate; and
applying to a surface of the iridium (Ir) base a bias enhanced nucleation process for forming epitaxial diamond nuclei by exposing an ion-containing direct current plasma using a parallel plate electrode type direct current plasma generator; and wherein
said bias enhanced nucleation process is conducted with a direct current plasma using the parallel plate electrode type direct current plasma generator under such conditions that
a diameter of an anode thereof is set at 7 to 25 mm,
a separation between the anode and the substrate is set at 5 to 11 mm,
a discharge gas used is composed of H2 and CH4,
a concentration of CH4 is set at 2%,
a discharge gas pressure is set at 100 to 150 Torr,
a discharge current density is set at 150 to 250 mA/cm2,
a discharge voltage is set at 250 to 760 V,
a substrate temperature is set at a temperature from greater than 850° C. to 1100° C., and
a discharge time is set at 30 to 120 seconds.

### Claim 2 (depends on 1)

The method of claim 1, wherein an epitaxial diamond film produced on said substrate has a size of at least 2.5 cm.

### Claim 3 (depends on 2)

The method of claim 2, wherein the epitaxial diamond film has a thickness of at least 60 microns.

### Claim 4

A method for producing an epitaxial diamond film, comprising:
forming an iridium (Ir) base on a surface of a single crystal magnesium oxide (MgO) substrate by epitaxial growth of an iridium (Ir) film;
applying to a surface of the iridium (Ir) base a bias enhanced nucleation process for forming epitaxial diamond nuclei by exposing an ion-containing plasma using a parallel plate electrode type direct current plasma generator,
said bias enhanced nucleation process being conducted with a direct current plasma using the parallel plate electrode type direct current plasma generator under such conditions that
a diameter of an anode thereof is set at 7 to 25 mm,
a separation between the anode and the substrate is set at 5 to 11 mm,
a discharge gas used is composed of H2 and CH4,
a concentration of CH4 is set at 2%,
a discharge gas pressure is set at 100 to 150 Torr,
a discharge current density is set at 150 to 250 mA/cm2,
a discharge voltage is set at 250 to 760 V,
a substrate temperature is set at a temperature from greater than 850° C. to 1100° C., and
a discharge time is set at 30 to 120 seconds; and
obtaining a free-standing epitaxial diamond film on said substrate by using a multiple electrode type direct current plasma CVD apparatus, said substrate having thereon said base which is formed by said epitaxial growth and on which the epitaxial diamond film is to be formed, and said free-standing epitaxial diamond film being obtained such that a vacuum chamber, which is provided therein with a movable shutter that is disposed above the substrate so as to face cathodes and is switchable between being grounded and being on a floating electric potential, is evacuated to introduce therein a discharge gas H2, and while discharge current of each of the cathodes is being slowly increased up to 1000 mA, a discharge is made between the cathodes and the shutter, and then discharge gas CH4 is introduced into said vacuum chamber to further increase the discharge current at the cathodes, and thereafter the shutter is opened to change the discharge to a discharge that is between the cathodes and the substrate.

### Claim 5 (depends on 4)

The method of claim 4, wherein the free-standing epitaxial diamond film has a size of at least 2.5 cm.

### Claim 6 (depends on 5)

The method of claim 5, wherein the free-standing epitaxial diamond film has a thickness of at least 60 microns.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate temperature is set at a temperature from greater than 920° C. to 1100° C.

### Claim 8 (depends on 4)