# US 9,353,430 B2 · Lightweight, crash-sensitive automotive component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,430 B2
- Document ID: US9353430B2
- Status: Granted
- Kind: B2
- Application number: 14/222,648
- Filed: 2014-03-23
- Published: 2014-07-24
- Granted: 2016-05-31
- Earliest claimed: 2005-10-28
- Assignees: Shipston Aluminum Technologies (Michigan), Inc.
- Applicants: Shipston Aluminum Technologies (Michigan), Inc.
- Inventors: Jen C. Lin; Moustapha Mbaye; Jan Ove Loland; Russell S. Long; Xinyan Yan
- Web page: https://patentgrep.com/patent/US9353430B2

## CPC

- C22C 21/02: with silicon as the next major constituent
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B22D 25/02: by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)}
- B22D 25/06: by its physical properties (B22D27/00 takes precedence)
- B62D 21/15: having impact absorbing means, e.g. a frame designed to permanently or temporarily change shape or dimension upon impact with another body (bumpers B60R19/02; shock absorbers in general F16F)
- B62D 29/008: {predominantly of light alloys, e.g. extruded}
- C22C 21/04: Modified aluminium-silicon alloys
- C22F 1/043: of alloys with silicon as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- B62D: MOTOR VEHICLES; TRAILERS (steering, or guiding on a desired track, of agricultural machines or implements A01B69/00; wheels, castors, axles, increasing wheel adhesion B60B; vehicle tyres, tyre inflation or tyre changing B60C; connections between vehicles of a train or the like B60D; vehicles for use on rail and road, amphibious or convertible vehicles B60F; suspension arrangements B60G; heating, cooling, ventilating or other air treating devices B60H; windows, windscreens, non-fixed roofs, doors or similar devices, protective coverings for vehicles not in use B60J; propulsion plant arrangements, auxiliary drives, transmissions, controls, instrumentation or dashboards B60K; electric equipment or propulsion of electrically-propelled vehicles B60L; power supply for electrically-propelled vehicles B60M; passenger accommodation not otherwise provided for B60N; adaptations for load transportation or to carry special loads or objects B60P; arrangement of signalling or lighting devices, the mounting or supporting thereof or circuits therefor, for vehicles in general B60Q; vehicles, vehicle fittings or vehicle parts not otherwise provided for B60R; servicing, cleaning, repairing, supporting, lifting, or manoeuvring, not otherwise provided for, B60S; brake arrangements, brake control systems or parts thereof B60T; air-cushion vehicles B60V; motor-cycles, accessories therefor B62J, B62K; testing of vehicles G01M)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The present invention provides a casting having increased crashworthiness including an an aluminum alloy of about 6.0 wt % to about 8.0 wt % Si; about 0.12 wt % to about 0.25 wt % Mg; less than or equal to about 0.35 wt % Cu; less than or equal to about 4.0 wt % Zn; less than or equal to about 0.6 wt % Mn; and less than or equal to about 0.15 wt % Fe, wherein the cast body is treated to a T5 or T6 temper and has a tensile strength ranging from 100 MPa to 180 MPa and has a critical fracture strain greater than 10%. The present invention further provides a method of forming a casting having increased crashworthiness.

## Claims

### Claim 1

A method of casting an aluminum alloy into a crash-sensitive automotive component having a desired critical fracture strain for collision impact, the method comprising:
selecting a crash-sensitive automotive component to cast;
providing a melt having an alloy comprising:
about 6.0 wt % to about 7.8 wt % Si;
about 0.10 wt % to about 0.18 wt % Mg;
less than or equal to about 0.35 wt % Cu;
less than or equal to about 0.6 wt % Mn;
less than or equal to about 0.15 wt % Fe;
and, a balance of aluminum and impurities;
casting the melt into a cast body of the crash-sensitive automotive component; and,
heat treating the cast body, the treating including a solution heating at 450° C. to 550° C. for about ½ hour to about 6 hours; quenching, and aging at a temperature of about 150° C. to about 250° C. for about ½ hour to about 10 hours;
wherein, the crash-sensitive automotive component has a critical fracture strain of at least about 10%.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heat treating comprises processing to a T6 temper.

### Claim 3 (depends on 1)

The method of claim 1, wherein the processing comprises a solution heat treatment of the crash-sensitive automotive component at 450° C. to 550° C. for a time period ranging from approximately a ½ hour to approximately 6 hours, quenching, and aging; the processing creating a tensile yield strength in the cast body ranging from 190 MPa to 240 MPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the Mn content is less than 0.15 wt %, and the casting of the cast body includes using a vacuum riserless casting/pressure riserless process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the casting of the cast body includes using a sand core in combination with a vacuum riserless casting/pressure riserless process to provide a wall thickness as thin as 2.0 mm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the cast body is in T6 temper and has a tensile yield strength ranging from 100 MPa to 180 MPa.

### Claim 7 (depends on 1)

The method of claim 1, wherein the Mn content of the cast body is less than about 0.05 wt % Mn.

### Claim 8 (depends on 1)

The method of claim 1, wherein the heat treating comprises T6 or T7 to further provide an elongation that exceeds 14%.

### Claim 9 (depends on 1)

The method of claim 1, the melt having about 7.0 wt % Si and from about 0.10 wt % to about 0.18 wt % Mg.

### Claim 10 (depends on 1)

The method of claim 1, the melt having about 0.12 wt % Mg and from about 6.0 wt % to about 7.8 wt % Si.

### Claim 11

A method of making a vehicle with a crash-sensitive automotive component having a desired performance during collision, the performance measured using critical fracture strain, the method comprising:
obtaining a crash-sensitive automotive component that was produced using a process including;
providing a melt having an alloy comprising:
about 6.0 wt % to about 7.8 wt % Si;
about 0.10 wt % to about 0.18 wt % Mg;
less than or equal to about 0.35 wt % Cu;
less than or equal to about 0.6 wt % Mn;
less than or equal to about 0.15 wt % Fe;
and, a balance of aluminum and impurities;
casting the melt into a cast body of the crash-sensitive automotive component; and,
heat treating the cast body, the heat treating including a solution heating at 450° C. to 550° C. for about ½ hour to about 6 hours; quenching, and aging at a temperature of about 150° C. to about 250° C. for about ½ hour to about 10 hours;
and,
employing the crash-sensitive component in the vehicle to provide a critical fracture strain of at least about 10% in the crash-sensitive component.

### Claim 12 (depends on 11)

The method of claim 11, wherein the crash-sensitive automotive component is a part of a vehicle frame construction.

### Claim 13 (depends on 11)

The method of claim 11, wherein the crash-sensitive automotive component is a part of a body structure.

### Claim 14 (depends on 11)

The method of claim 11, wherein the crash-sensitive automotive component is selected from a group consisting of a bracket, a node, a crashbox, a crossmember, a subframe, and an engine cradle.

### Claim 15 (depends on 11)

The method of claim 11, wherein the heat treating comprises processing the cast body to a T6 temper.

### Claim 16 (depends on 11)

The method of claim 11, wherein the heat treating comprises a solution heat treatment of the cast body at 450° C. to 550° C. for a time period ranging from approximately a ½ hour to approximately 6 hours, quenching, and aging; the processing creating a tensile yield strength in the cast body ranging from 190 MPa to 240 MPa.