# US 9,353,429 B2 · Aluminum alloy material for use in thermal conduction application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,429 B2
- Document ID: US9353429B2
- Status: Granted
- Kind: B2
- Application number: 12/527,283
- Filed: 2007-02-27
- Published: 2010-05-06
- Granted: 2016-05-31
- Earliest claimed: 2007-02-27
- Assignees: Nippon Light Metal Company, Ltd.
- Applicants: Hiroshi Horikawa; Masahiko Shioda
- Inventors: Hiroshi Horikawa; Masahiko Shioda
- Web page: https://patentgrep.com/patent/US9353429B2

## CPC

- C22F 1/043: of alloys with silicon as the next major constituent
- C22C 21/02: with silicon as the next major constituent
- F28F 21/084: {from aluminium or aluminium alloys}
- F28D 2021/0029: {Heat sinks}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)
- F28D: HEAT-EXCHANGE APPARATUS, NOT PROVIDED FOR IN ANOTHER SUBCLASS, IN WHICH THE HEAT-EXCHANGE MEDIA DO NOT COME INTO DIRECT CONTACT (fluid heaters having heat generating means and heat transferring means F24H; furnaces F27; details of heat-exchange apparatus of general)

## Abstract

An aluminum alloy material for use in thermal conduction to which improved castability has been imparted by silicon addition. It has improved thermal conductivity and improved strength. The material has a composition containing 7.5-12.5 mass % Si and 0.1-2.0 mass % Cu, the remainder being Al and unavoidable impurities, wherein the amount of copper in the state of a solid solution in the matrix phase is regulated to 0.3 mass % or smaller. The composition may further contain at least 0.3 mass % Fe and/or at least 0.1 mass % Mg, provided that the sum of (Fe content) and (content of Mg among the impurities)×2 is 1.0 mass % or smaller and the sum of (Cu content), (content of Mg among the impurities)×2.5, and (content of Zn among the impurities) is 2.0 mass % or smaller.

## Claims

### Claim 1

An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, less than 0.05 mass % of Mg as an impurity, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less and the solid solution content of Cu in the matrix phase is 0.3 mass % or less.

### Claim 2 (depends on 1)

A heat exchange element consisting of the aluminum alloy die cast of claim 1.

### Claim 3 (depends on 2)

The heat exchange element of claim 2, which is a heat dissipating element.

### Claim 4 (depends on 1)

The aluminum alloy die cast for use in a thermal conduction application of claim 1, wherein the aluminum alloy has been subjected to an aging treatment.

### Claim 5 (depends on 4)

The aluminum alloy die cast for use in a thermal conduction application of claim 4, wherein before said ageing treatment, said aluminum alloy is subjected to a solution treatment by holding at a temperature of 450 to 520° C. for 1 to 10 hours, then quenched by cooling at a cooling rate of at least 100° C./sec to a temperature of 100° C. or less.

### Claim 6 (depends on 4)

The aluminum alloy die cast for use in a thermal conduction application of claim 4, wherein said aluminum alloy is held at a temperature of 160 to 370° C. for 1 to 20 hours during said aging treatment.

### Claim 7 (depends on 6)

The aluminum alloy die cast for use in a thermal conduction application of claim 6, wherein before said ageing treatment, said aluminum alloy is subjected to a solution treatment by holding at a temperature of 450 to 520° C. for 1 to 10 hours, then quenched by cooling at a cooling rate of at least 100° C./sec to a temperature of 100° C. or less.

### Claim 8 (depends on 1)

The aluminum alloy die cast for use in a thermal conduction application of claim 1, wherein the amount of Cu is 0.5-1.2 mass %.

### Claim 9

An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, 0.1 to less than 0.2 mass % of Mg, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less, the relationship among the Cu content, the Mg content and the content of Zn included as an unavoidable impurity is such that the total of (Cu content)+(Mg content) times 2.5+(Zn content) is less than 1.8 mass %, and the solid solution content of Cu in the matrix phase is 0.3 mass % or less.

### Claim 10 (depends on 9)

A heat exchange element consisting of the aluminum alloy die cast of claim 9.

### Claim 11 (depends on 10)

The heat exchange element of claim 10, which is a heat dissipating element.

### Claim 12 (depends on 9)

The aluminum alloy die cast for use in a thermal conduction application of claim 9, wherein the aluminum alloy has been subjected to an aging treatment.

### Claim 13 (depends on 12)

The aluminum alloy die cast for use in a thermal conduction application of claim 12, wherein before said ageing treatment, said aluminum alloy is subjected to a solution treatment by holding at a temperature of 450 to 520° C. for 1 to 10 hours, then quenched by cooling at a cooling rate of at least 100° C./sec to a temperature of 100° C. or less.

### Claim 14 (depends on 12)

The aluminum alloy die cast for use in a thermal conduction application of claim 12, wherein said aluminum alloy is held at a temperature of 160 to 370° C. for 1 to 20 hours during said aging treatment.

### Claim 15 (depends on 14)

The aluminum alloy die cast for use in a thermal conduction application of claim 14, wherein before said ageing treatment, said aluminum alloy is subjected to a solution treatment by holding at a temperature of 450 to 520° C. for 1 to 10 hours, then quenched by cooling at a cooling rate of at least 100° C./sec to a temperature of 100° C. or less.

### Claim 16

An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, less than 0.05 mass % of Mg as an impurity, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less and the solid solution content of Cu in the matrix phase is 0.3 mass % or less, subject to an ageing treatment within the range of at 180-300° C. for 4-8 hours.

### Claim 17 (depends on 16)

The aluminum alloy die cast for use in a thermal conduction application of claim 16, wherein the amount of Cu is 0.5-1.2 mass %.

### Claim 18

An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, 0.1 to less than 0.2 mass % of Mg, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less, the relationship among the Cu content, the Mg content and the content of Zn included as an unavoidable impurity is such that the total of (Cu content)+(Mg content) times 2.5+(Zn content) is less than 1.8 mass %, and the solid solution content of Cu in the matrix phase is 0.3 mass % or less, subject to an ageing treatment within the range of at 180-300° C. for 4-8 hours.