# US 9,353,308 B2 · Modified cement composition, preparation and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,308 B2
- Document ID: US9353308B2
- Status: Granted
- Kind: B2
- Application number: 14/452,596
- Filed: 2014-08-06
- Published: 2014-11-27
- Granted: 2016-05-31
- Earliest claimed: 2011-01-26
- Assignees: Research Institute of Petroleum Industry
- Applicants: Research Institute of Petroleum Industry
- Inventors: Hamid Soltanian; Ali Reza Mortazavi; Mohammad Javad Modjtahedi; Mahmoud Reza Badamaki; Ali Mesbah; Ali Reza Khoshniyat; Mohammad Reza Kamali
- Web page: https://patentgrep.com/patent/US9353308B2

## CPC

- C04B 14/04: Silica-rich materials; Silicates
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C04B 14/062: {Microsilica, e.g. colloïdal silica (preparing microsilica slurries or suspensions C04B18/148)}
- C04B 22/064: {of the alkaline-earth metals}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 28/04: Portland cements
- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- C09K 8/487: Fluid loss control additives; Additives for reducing or preventing circulation loss
- C09K 8/493: Additives for reducing or preventing gas migration
- E21B 33/14: for cementing casings into boreholes
- C04B 2111/00008: {Obtaining or using nanotechnology related materials}
- C04B 2111/00474: {Uses not provided for elsewhere in C04B2111/00}
- C04B 2111/40: Porous or lightweight materials
- C04B 2201/50: for the mechanical strength
- C09K 2208/10: Nanoparticle-containing well treatment fluids
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

Light to ultra-light cement compositions with modified rheological properties. The cement composition includes cement, hydrophobic nano-silica, at least one additive and a sufficient amount of water to make a cement slurry with high compressive strength, low porosity, low free water, and low fluid loss with a quick thickening time.

## Claims

### Claim 1

A modified cement composition comprising cement, hydrophobic nano-silica, at least one additive and a sufficient amount of water to make a cement slurry.

### Claim 2 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica includes a surface area of from about 110 m2/g to about 260 m2/g.

### Claim 3 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica includes a surface area of from about 240 m2/g to about 260 m2/g.

### Claim 4 (depends on 1)

The modified cement composition of claim 1, wherein water is present in an amount of from about 30% by weight of blend cement to about 170% by weight of blend cement.

### Claim 5 (depends on 1)

The modified cement composition of claim 1, wherein water is present in an amount of from about 30% by weight of blend cement to about 80% by weight of blend cement.

### Claim 6 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica includes a particle size of from about 1 nm to about 100 nm.

### Claim 7 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica includes a particle size of from about 1 nm to about 60 nm.

### Claim 8 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica includes a particle size of from about 1 nm to about 6 nm.

### Claim 9 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica is present in an amount of from about 1% BWOC to about 15% BWOC.

### Claim 10 (depends on 1)

The modified cement composition of claim 1, wherein the hydrophobic nano-silica is present in an amount of from about 1% BWOC to about 9% BWOC.

### Claim 11 (depends on 1)

The modified cement composition of claim 1, wherein the at least one additive comprises at least one of light weight additive, an anti-foaming agent, a retardant, an accelerator, a dispersant, a fluid loss controlling agent, a surfactant, and a gas migration controlling agent.

### Claim 12 (depends on 11)

The modified cement composition of claim 11, wherein the gas migration controlling agent comprises at least one of (i) a composition including at least about 90% SiO2, from about 0.5% to about 2.0% Al2O3, from about 0.2% to about 1.5% Fe2O3, from about 0.1% to about 0.5% CaO, from about 0.1% to about 1.5% Na2O, from about 0.5% to about 2.0% K2O, from about 0.5% to about 2.0% MgO, from about 0.1% to about 0.4% SO3, and from about 0.5% to about 2.5% C and (ii) a composition including at least latex particles.

### Claim 13 (depends on 1)

The modified cement composition of claim 1, wherein the cement, hydrophobic nano-silica, and the at least one additive include a particle size to maximize a packing volume fraction.

### Claim 14 (depends on 1)

The modified cement composition of claim 1, wherein the cement includes a particle size of from about 10 μm to about 50 μm and the at least one additive includes a particle size of from about 51 μm to about 370 μm.

### Claim 15 (depends on 1)

The modified cement composition of claim 1, wherein the additive is present in an amount of from about 0.1% BWOC to about 150% BWOC.

### Claim 16 (depends on 1)

The modified cement composition of claim 1 comprising a 24-hour compressive strength of about 4450 psi.

### Claim 17

A modified cement composition comprising cement, hydrophobic nano-silica, and at least one additive and water to make a cement slurry having a 24-hour compressive strength of about 4450 psi.

### Claim 18 (depends on 17)

The modified cement composition of claim 17, wherein water is present in an amount of about 127% or less by weight of blend cement.

### Claim 19

A modified cement composition comprising cement with a particle size of from about 10 μm to about 50μm, hydrophobic nano-silica with a surface area of from about 110 m2/g to about 260 m2/g, at least one additive with a particle size of from about 51 μm to about 370 μm, and a sufficient amount of water to make a cement slurry.

### Claim 20 (depends on 1)

A method for making a well structure resistant to damaging and corrosive fluids and securement of a well casing to a well borehole wall comprising the steps of applying the modified cement composition of claim 1 to a location.