# US 9,353,292 B2 · Asphalt modified with an SBS/MMWCNT nanocomposite and production method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,292 B2
- Document ID: US9353292B2
- Status: Granted
- Kind: B2
- Application number: 14/412,239
- Filed: 2013-08-21
- Published: 2015-07-02
- Granted: 2016-05-31
- Earliest claimed: 2012-08-22
- Assignees: Corporacion Para La Investigacion Y Desarrollo De Asfaltos En El Sector Transporte E Industrial-Corasfaltos
- Applicants: Corasfaltos—Corp. Para La Investigacion Y Desarrollo De Asfaltos En El Sector Transporte E Industrial
- Inventors: Luz Stella Quintero Rangel; Luis Enrique Sanabria Grajales
- Web page: https://patentgrep.com/patent/US9353292B2

## CPC

- C08K 3/04: Carbon
- C08J 3/005: {Processes for mixing polymers}
- C08J 3/226: {using a polymer as a carrier}
- C08K 3/041: {Carbon nanotubes}
- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C09D 7/62: modified by treatment with other compounds
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 7/70: {characterised by shape, e.g. fibres, flakes or microspheres}
- C09D 195/00: Coating compositions based on bituminous materials, e.g. asphalt, tar, pitch
- C08J 2395/00: Bituminous materials, e.g. asphalt, tar or pitch
- C08J 2453/02: of vinyl aromatic monomers and conjugated dienes
- C08K 2201/011: Nanostructured additives
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The invention relates to a method for modifying an asphalt binder using, as an additive, a nanocomposite of: functionalized multi-walled carbon nanotubes dispersed in a styrene-butadiene-styrene polymer matrix (SBS/MMWCNT). The asphalt modified with the SBS/MMWCNT nanocomposite has substantially improved mechanical resistance to deformations and to loads at high temperatures, such that the life of the flexible paving is improved. The asphalt mixtures produced with this novel modified asphalt binder have considerably less rutting, are classified as high-modulus asphalt mixtures when produced from asphalt of medium (60/70) or greater hardness, and are not sensitive to moisture effects.

## Claims

### Claim 1

A method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes comprising:
1) preparing a polymer nanocomposite additive comprising:
a) dispersing a multi-walled carbon nanotubes in a solvent by ultrasound and/or mechanical stirring in order to obtain a multi-walled carbon nanotubes dispersion;
b) dissolving a styrene-butadiene-styrene polymer in a solvent by mechanical stirring in order to obtain a styrene-butadiene-styrene solution;
c) mixing the multi-walled carbon nanotubes dispersion with the styrene-butadiene-styrene solution by ultrasound and/or mechanical stirring and obtaining a homogeneous viscous solution of styrene-butadiene-styrene polymer and multi-walled carbon nanotubes;
2) introducing the polymer nanocomposite additive to an asphalt base and mixing the polymer nanocomposite additive with the asphalt base in order to form the asphalt modified with the polymer nanocomposite comprising styrene-butadiene-styrene and multi-walled carbon nanotubes.

### Claim 2 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 1, wherein in the preparation stage of the polymer nanocomposite, the styrene-butadiene-styrene polymer is in the form of pellets or crumbs, and the multi-walled carbon nanotubes are functionalized.

### Claim 3 (depends on 2)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 2, wherein the multi-walled carbon nanotubes are functionalized with functional groups selected from the group consisting of hydroxyl groups, carboxylic acid groups, amino groups, phenol, and alkyl groups.

### Claim 4 (depends on 2)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 2, wherein the functionalized multi-walled carbon nanotubes are dispersed in the solvent by application of ultrasound for a period not greater than 24 hours.

### Claim 5 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 1, wherein the solvent is selected from the group consisting of xylenes, toluene, acetone, tetrahydrofuran, chloroform, cyclohexane, ethanol, methanol, propanol, dimethylformamide, and combinations thereof, with a solvent/polymer weight ratio between 1 and 20 and with a solvent/multi-walled carbon nanotubes weight ratio between 10 and 10,000.

### Claim 6 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 1, wherein the multi-walled carbon nanotubes have a diameter between 5-50 nm and a length between 1-30 μm.

### Claim 7 (depends on 1)

The method for preparing asphalt modified a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 1, wherein the styrene-butadiene-styrene polymer solution and the multi-walled carbon nanotubes dispersion are mixed and homogenized for a period not greater than 4 hours.

### Claim 8 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of claim 1, wherein the solutions prepared from styrene-butadiene-styrene and multi-walled carbon nanotubes are mixed by means of ultrasound and mechanical stirring until they are homogenized.

### Claim 9 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes of as claimed in claim 1, wherein the solvent is evaporated from the homogenized solution by means of a rotary evaporator, a dryer, an evaporator, a vacuum distillation system or any other means that allows the evaporation of the solvent until the solution becomes viscous.

### Claim 10 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes as claimed in claim 1, wherein the homogeneous viscous solution of styrene-butadiene-styrene and multi-walled carbon nanotubes is poured onto plates, metal strips or conveyor belts of glass or any material that is chemically stable with respect to the employed solvent, and the latter are fed into a vacuum furnace or convection furnace at a temperature between 30° C.-100° C. so as to evaporate the remaining solvent and produce the dry sheets of the polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes.

### Claim 11 (depends on 10)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes as claimed in claim 10, wherein the sheets of the Polymer nanocomposite are cut to pieces having a maximum size of 0.2 cm-4 cm.

### Claim 12 (depends on 11)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes nanocomposite as claimed in claim 11, wherein the asphalt base is heated at a temperature between 100° C. and 200° C. until it becomes fluid, following which the pieces of polymer nanocomposite are added.

### Claim 13 (depends on 1)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes as claimed in claim 1, wherein the mix of asphalt base and the polymer nanocomposite additive is homogenized by mechanical stirring for a period between 0.5 and 7 hours.

### Claim 14 (depends on 13)

The method for preparing asphalt modified with a polymer nanocomposite additive comprising styrene-butadiene-styrene and multi-walled carbon nanotubes as claimed in claim 13, wherein the concentration of the polymer nanocomposite additive in the asphalt base is between 3-7%.