# US 9,353,259 B2 · Method for producing thermoplastic resin composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,259 B2
- Document ID: US9353259B2
- Status: Granted
- Kind: B2
- Application number: 14/540,711
- Filed: 2014-11-13
- Published: 2015-05-21
- Granted: 2016-05-31
- Earliest claimed: 2013-11-18
- Assignees: Konica Minolta, Inc.
- Applicants: Konica Minolta, Inc.
- Inventors: Yiqiang Yu; Masashi Mamino; Ryuji Kitani
- Web page: https://patentgrep.com/patent/US9353259B2

## CPC

- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C08J 3/00: Processes of treating or compounding macromolecular substances
- C08J 3/005: {Processes for mixing polymers}
- C08J 3/20: Compounding polymers with additives, e.g. colouring
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08J 2367/00: Characterised by the use of polyesters obtained by reactions forming a carboxylic ester link in the main chain; Derivatives of such polymers
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08L 2201/02: Flame or fire retardant/resistant
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

Provided is a thermoplastic resin composition having high flame resistance and high fluidity during injection molding, and improved impact resistance in a molded article. A method for producing a thermoplastic resin composition, the method including the step (1) of obtaining a polyester resin mixture by melt-kneading 50 to 80 parts by weight of crystalline polyester resin and 20 to 50 parts by weight of amorphous polyester resin with an extruder, and the step (2) of mixing the polyester resin mixture, a polycarbonate resin, a flame retardant, a dripping inhibitor and a toughening agent, wherein the cylinder temperature of the extruder is 250 to 280° C.

## Claims

### Claim 1

A method for producing a thermoplastic resin composition comprising: the step (1) of obtaining a polyester resin mixture by melt-kneading 50 to 80 parts by weight of crystalline polyester resin and 20 to 50 parts by weight of amorphous polyester resin with an extruder; and the step (2) of mixing the polyester resin mixture, polycarbonate resin, a flame retardant, a dripping inhibitor and a toughening agent, wherein the cylinder temperature of the extruder is 250 to 280° C., wherein the amount of heat release (ΔHA) in the DSC melting curve of the polyester resin mixture is 70% or less with respect to the amount of heat release (ΔHB) in the DSC melting curve of the crystalline polyester resin (ΔHA/ΔHB≦0.7).

### Claim 2 (depends on 1)

The production method according to claim 1, wherein the crystalline polyester resin is at least one kind of polyethylene terephthalate and polybutylene terephthalate, and the amorphous polyester resin is at least one kind of PETG resin, PCTG resin and PCTA resin.

### Claim 3 (depends on 1)

The production method according to claim 1, wherein in the step (1), a metal-based catalyst is added in an amount of 0.05 weight % or less with respect to a total of 100 weight % of the crystalline polyester resin and the amorphous polyester resin.

### Claim 4 (depends on 1)

The production method according to claim 1, wherein in the step (2), 10 to 90 parts by weight of polyester resin mixture, 10 to 90 parts by weight of polycarbonate resin, 1 to 40 parts by weight of flame retardant, 0.1 to 1 part by weight of dripping inhibitor and 1 to 20 parts by weight of toughening agent are mixed.

### Claim 5 (depends on 1)

The production method according to claim 1, wherein the molecular weight (Mw) of the polycarbonate resin is 20,000 to 70,000.