# US 9,353,252 B2 · Soft polypropylene with improved optical properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,252 B2
- Document ID: US9353252B2
- Status: Granted
- Kind: B2
- Application number: 14/387,768
- Filed: 2013-03-25
- Published: 2015-02-19
- Granted: 2016-05-31
- Earliest claimed: 2012-03-29
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Markus Gahleitner; Martina Sandholzer; Klaus Bernreitner
- Web page: https://patentgrep.com/patent/US9353252B2

## CPC

- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08J 5/18: Manufacture of films or sheets
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08J 2323/14: Copolymers of propene (C08J2323/16 takes precedence)
- Y10T 428/1397: Single layer [continuous layer]
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Polymer composition comprising a propylene copolymer and a styrenic based elastomer.

## Claims

### Claim 1

Polymer composition comprising:
(a) a propylene copolymer (A) having:
(a1) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of more than 2.0 to 15.0 g/10 min,
(a2) a comonomer content in the range of more than 7.5 to 16.5 wt. %, and
(a3) a xylene cold soluble content (XCS) determined according to ISO 16152 (25° C.) in the range of 25.0 to 55.0 wt. %, wherein,
(a4) the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of 14.0 to 30.0 wt. %, and
(a5) an intrinsic viscosity (IV) of the xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of equal or more than 1.5 to equal or below 3.0 dl/g, wherein the intrinsic viscosity (IV) is determined according to DIN ISO 1628/1 (in Decalin at 135° C.), and
(b) styrenic based elastomer(s) (B) having a styrene content in the range of 5 to equal or below 15 wt. %,
wherein further the weight ratio of propylene copolymer (A) and the styrenic based elastomer(s) (B) [(A)/(B)] is in the range of 9/1 to 3/2.

### Claim 2 (depends on 1)

Polymer composition according to claim 1, wherein the propylene copolymer (A):
(a) has a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of more than 2.5 to below 5.0 g/10 min, and/or
(b) fulfills inequation (I):
0.3
≤
Co
⁢
⁢
(
total
)
Co
⁢
⁢
(
XCS
)
≤
0.7
wherein, Co (total) is the comonomer content [wt. %] of the propylene copolymer (A),
Co (XCS) is the comonomer content [wt. %] of the xylene cold soluble fraction (XCS) of the propylene copolymer (A), and/or
(c) fulfills inequation (II):
Co
⁢
⁢
(
total
)
XCS
≤
0.30
wherein, Co (total) is the comonomer content [wt. %] of the propylene copolymer (A),
XCS is the content of the xylene cold soluble fraction (XCS) [wt. %] of the propylene copolymer (A).

### Claim 3 (depends on 1)

Polymer composition according to claim 1, wherein the xylene cold insoluble (XCI) fraction of the propylene copolymer (A) has a comonomer content in the range of 1.5 to 6.0 wt. %.

### Claim 4 (depends on 1)

Polymer composition according to claim 1, wherein the propylene copolymer (A) is a heterophasic propylene copolymer (RAHECO) comprising a matrix (M) and an elastomeric propylene copolymer (E) dispersed in said matrix (M), wherein said matrix (M) is a random propylene copolymer (R-PP).

### Claim 5 (depends on 4)

Polymer composition according to claim 4, wherein:
(a) the weight ratio between the matrix (M) and the elastomeric propylene copolymer (E) is 50/50 to 90/10, and/or
(b) the comonomer content of the random propylene copolymer (R-PP) is in the range of 3.0 to 12.0 wt. %, and/or
(c) the random propylene copolymer (R-PP) has a xylene cold soluble (XCS) fraction in the range of 5.0 to 50.0 wt. %.

### Claim 6 (depends on 4)

Polymer composition according to claim 4, wherein the elastomeric propylene copolymer (E) has a comonomer content in the range of 14.0 to 35.0 wt. %.

### Claim 7 (depends on 1)

Polymer composition according to claim 1, wherein the styrenic based elastomer(s) (B) is(are) (a) styrene-ethylene/butylene-styrene (SEBS) block copolymer(s) (B-1) and/or (a) hydrogenated styrene-vinyl isoprene (SIS) block rubber(s) (B-2).

### Claim 8 (depends on 1)

Polymer composition according to claim 1, wherein the polymer composition comprises as styrenic based elastomer(s) (B) only (a) styrene-ethylene/butylene-styrene (SEBS) block copolymer(s) (B-1) and/or (a) hydrogenated styrene-vinyl isoprene (SIS) block rubber(s) (B-2).

### Claim 9 (depends on 1)

Polymer composition according to claim 1, wherein the styrenic based elastomer (B) has a melt flow rate MFR2 (230° C.) of below 10.0 g/10 min.

### Claim 10 (depends on 1)

Polymer composition according to claim 1, wherein the styrenic based elastomer(s) (B) has a density of below 0.905 g/m3.

### Claim 11 (depends on 1)

A film, comprising the polymer composition as defined in claim 1.

### Claim 12

A container, comprising a film, the film including a polymer composition, the polymer composition comprising:
(a) a propylene copolymer (A) having:
(a1) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of more than 2.0 to 15.0 g/10 min,
(a2) a comonomer content in the range of more than 7.5 to 16.5 wt. %, and
(a3) a xylene cold soluble content (XCS) determined according to ISO 16152 (25° C.) in the range of 25.0 to 55.0 wt. %, wherein,
(a4) the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of 14.0 to 30.0 wt. %, and
(a5) an intrinsic viscosity (IV) of the xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of equal or more than 1.5 to equal or below 3.0 dl/g, wherein the intrinsic viscosity (IV) is determined according to DIN ISO 1628/1 (in Decalin at 135° C.), and
(b) styrenic based elastomer(s) (B) having a styrene content in the range of 5 to equal or below 15 wt. %,
wherein further the weight ratio of propylene copolymer (A) and the styrenic based elastomer(s) (B) [(A)/(B)] is in the range of 9/1 to 3/2.

### Claim 13 (depends on 12)

The container according to claim 12, wherein the container or the film has been subjected to a sterilisation treatment.