# US 9,353,250 B2 · Hinge polymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,250 B2
- Document ID: US9353250B2
- Status: Granted
- Kind: B2
- Application number: 14/205,628
- Filed: 2014-03-12
- Published: 2014-09-18
- Granted: 2016-05-31
- Earliest claimed: 2013-03-14
- Assignees: NOVA Chemicals (International) S.A.
- Applicants: NOVA Chemicals (International) S.A.
- Inventors: Jason Michael Rycroft; Gilbert Alexander Arnould; Matthew Zaki Botros; Mark Rejman
- Web page: https://patentgrep.com/patent/US9353250B2

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- G01N 3/32: by applying repeated or pulsating forces
- G01N 3/36: generated by pneumatic or hydraulic means
- C08L 2205/02: containing two or more polymers of the same C08L -group
- G01N 2203/0023: Bending
- G01N 2203/0464: with provisions for testing more than one specimen at the time
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A polymer suitable for use in a thin film hinge (living hinge) comprising from about 0.1 to about 5 weight % of a C4-8 comonomer and the balance ethylene, said composition having a density as determined according to ASTM D 792 from about 0.945 to about 0.965 g/cm3; a melt index as determined according to ASTM D1238 (2.16 kg/190° C.) from about 10 to about 20 g/10 min; a weight average molecular weight (Mw) from about 45,000 to about 55,000 g/mol; a polydispersity from about 2.5 to about 3.1 and when molded into a strip having a length of about 13 cm and gross thickness from about 50 to about 70 mil (about 1 to about 2 mm) and completely bent over end to end four times to create a thinned region or crease having a thickness from about 15 to about 30 mil (about 0.3 to about 0.7 mm) tested by bending and releasing the deformed thinned region of the strip through a radius of curvature from about 180 to about 190° about a rounded plate goes through not less than 500 cycles without breaking.

## Claims

### Claim 1

A polyethylene composition consisting of:
i) from 60 to 80 weight % of a polyethylene consisting of: from 0.1 to 0.5 weight of 1-butene and the balance ethylene, said composition having a density as determined according to ASTM D 792 from 0.948 to 0.952 g/cm3; a melt index as determined according to ASTM D1238 (2.16 kg 190° C.) from 16 to 18 g/10 min; a weight average molecular weight (Mw) from 48,000 to 52,000 g/mol; a polydispersity from 2.7 to 3.0 and;
ii) from 40 to 20 wt. % of a polyethylene homopolymer having a density from 0.960 g/cm3 to 0.965 g/cm3; a melt index as determined according to ASTM D1238 (2.16 kg 190° C.) from 12 to 14 g/10 min, a weight average molecular weight (Mw) from 55,000 to 63,000 and a polydispersity from 3.0 to 3.3;
wherein said polyethylene composition has a density according to ASTM 792 from 0.950 to 0.960 g/cm3, a tensile strength at yield from 24 to 28 MPa, and when molded into a strip having a length of 13 cm and gross thickness from 50 to 70 mil (1 to 2 mm) and completely bent over end to end four times to create a creased strip having a thinned region having a thickness from 15 to 30 mil (0.3 to 0.3 mm); said creased strip is tested in a bending and releasing cycle until breaking; wherein said thinned region is bent and released through a radius of curvature of 180° to 190° about a rounded plate until said creased strap breaks; wherein said creased strip goes through from about 650 to 2510 cycles prior to breaking.

### Claim 2 (depends on 1)

The polyethylene composition according to claim 1, wherein said creased strip goes through from about 750 to 2510 bending and releasing cycles prior to breaking.

### Claim 3 (depends on 1)

The polyethylene composition according to claim 1, wherein the polyethylene composition has a lower comonomer content at higher molecular weight.

### Claim 4 (depends on 1)

The polyethylene composition according to claim 1, wherein component i) and component ii) are solution polymerized.

### Claim 5 (depends on 1)

The polyethylene composition according to claim 1, wherein said creased strip through from about 900 to 2510 bending and releasing cycles prior to breaking.