# US 9,353,215 B2 · Production method of polycarbonate resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,215 B2
- Document ID: US9353215B2
- Status: Granted
- Kind: B2
- Application number: 14/041,397
- Filed: 2013-09-30
- Published: 2014-01-30
- Granted: 2016-05-31
- Earliest claimed: 2011-03-31
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Masashi Yokogi; Shingo Namiki; Takehito Nagao; Masanori Yamamoto
- Web page: https://patentgrep.com/patent/US9353215B2

## CPC

- B29B 7/002: {Methods (chemical aspects C08J3/00)}
- C08G 64/083: {containing phosphorus}
- B29B 7/16: with paddles or arms
- B29B 7/28: for measuring, controlling or regulating, e.g. viscosity control {(B29B7/242 takes precedence)}
- B29B 7/72: Measuring, controlling or regulating
- B29B 7/7461: {Combinations of dissimilar mixers}
- B29B 7/748: {Plants (B29B7/7433, B29B7/7485, B29B7/7495 take precedence)}
- B29B 7/7485: {with consecutive mixers, e.g. with premixing some of the components}
- B29B 7/82: Heating or cooling
- B29B 7/845: {Venting, degassing or removing evaporated components in devices with rotary stirrers}
- B29B 9/06: in the form of filamentary material, e.g. combined with extrusion
- B29C 48/37: Gear pumps
- B29C 48/397: {using a single screw}
- B29C 48/40: using two or more parallel screws {or at least two parallel non-intermeshing screws}, e.g. twin screw extruders
- B29C 48/57: provided with kneading disc-like elements, e.g. with oval-shaped elements
- C08G 64/305: {and alcohols}
- C08G 64/38: using other monomers
- C08J 5/18: Manufacture of films or sheets
- B29B 7/86: for working at sub- or superatmospheric pressure {(B01F33/70 takes precedence)}
- B29K 2069/00: Use of PC, i.e. polycarbonates {or derivatives thereof}, as moulding material
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention is a method for producing a polycarbonate resin, comprising performing polycondensation through a transesterification reaction by using a catalyst and using a dihydroxy compound and a carbonic acid diester as raw material monomers, and feeding the produced polycarbonate resin to an extruder, wherein the dihydroxy compound contains at least a dihydroxy compound having a moiety represented by formula (1) in a part of the structure, the dihydroxy compound having a moiety represented by formula (1) contains a compound having a cyclic ether structure, and the temperature at the time of feeding the polycarbonate resin to the extruder is from 180° C. to less than 250° C., with the proviso excluding the case where the moiety represented by formula (1) is a part of —CH2—O—H CH2—O (1).

## Claims

### Claim 1

A method for producing a polycarbonate resin, comprising performing polycondensation through a transesterification reaction with a catalyst and with a dihydroxy compound and a carbonic acid diester, and continuously feeding the produced polycarbonate resin to an extruder,
wherein
the polycarbonate is not solidified after the polycondensation and before being fed to the extruder,
the dihydroxy compound contains a dihydroxy compound having a moiety represented by the following formula (1) in a part of the structure,
the dihydroxy compound having a moiety represented by the following formula (1) contains a compound having a cyclic ether structure, and
the temperature at the time of feeding the polycarbonate resin to the extruder is from 180° C. to less than 250° C.:
CH2—O (1)
with the proviso excluding the case where the moiety represented by formula (1) is a part of —CH2—O—H,
wherein a barrel constituting the extruder has a plurality of heaters and all of the heaters are set to a temperature of 100° C. to less than 250° C.

### Claim 2 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the glass transition temperature of the polycarbonate resin obtained via the extruder is from 80° C. to less than 145° C.

### Claim 3 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein each of the heaters is set to a temperature not higher than the preset temperature of the heater adjacent to the polycarbonate resin feed side of the extruder.

### Claim 4 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the polycarbonate resin produced by polycondensation through a transesterification reaction is fed in a molten state to the extruder.

### Claim 5 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the extruder comprises a screw and wherein the screw of the extruder is composed of a plurality of elements, at least one of the elements is a kneading disc, and the total length of the kneading disc is 20% or less of the length of the screw as a whole.

### Claim 6 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein assuming that the weight of the resin extruded per hour from the extruder is W (kg/h) and the cross-sectional area of the barrel of the extruder is S (m2), the following formula (5) is satisfied:
12000≦W/S≦60000 (5).

### Claim 7 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the reduced viscosity (ηsp/c) of the polycarbonate resin obtained via the extruder, as measured in methylene chloride under the conditions of a concentration of 0.6 g/dL and a temperature of 20.0° C.±0.1° C., is from 0.3 to 1.2 dL/g.

### Claim 8 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the glass transition temperature of the polycarbonate resin obtained via the extruder is from 90 to 140° C.

### Claim 9 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the content of an aromatic monohydroxy compound contained in said polycarbonate resin obtained via said extruder is less than 0.1 wt %.

### Claim 10 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the raw material monomers are filtered through a filter for raw material filtration before polycondensation.

### Claim 11 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein said extruder kneads a heat stabilizer.

### Claim 12 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein said catalyst is a compound of at least one metal selected from the group consisting of metals belonging to Group 2 of the long-form periodic table and lithium.

### Claim 13 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein the dihydroxy compound having a moiety represented by formula (1) is isosorbide.

### Claim 14 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein an alicyclic dihydroxy compound is further used as said dihydroxy compound.

### Claim 15

A method for producing a polycarbonate resin pellet, comprising performing polycondensation through a transesterification reaction with a catalyst and with a dihydroxy compound and a carbonic acid diester, and continuously feeding the produced polycarbonate resin to an extruder, wherein
said polycarbonate is not solidified after said polycondensation and before being fed to said extruder
said dihydroxy compound contains at least a dihydroxy compound having a moiety represented by the following formula (1) in a part of the structure,
the glass transition temperature of the polycarbonate resin fed to said extruder is from 80° C. to less than 145° C., and
the temperature at the time of feeding said polycarbonate resin to said extruder is from 180° C. to less than 250° C.:
CH2—O (1)
with the proviso excluding the case where the moiety represented by formula (1) is a part of —CH2—O—H,
wherein a barrel constituting the extruder has a plurality of heaters and all of the heaters are set to a temperature of 100° C. to less than 250° C.

### Claim 16

A method for producing a polycarbonate resin, comprising performing polycondensation through a transesterification reaction with a catalyst and with a dihydroxy compound and a carbonic acid diester as raw material monomers, and continuously feeding the produced polycarbonate resin to an extruder, wherein
said polycarbonate is not solidified after said polycondensation and before being fed to said extruder,
said dihydroxy compound contains at least a dihydroxy compound having a moiety represented by the following formula (1) in a part of the structure,
the dihydroxy compound having a moiety represented by formula (1) is a compound having a cyclic ether structure,
the barrel constituting said extruder has a plurality of heaters, and all of the heaters is set to a temperature of 100° C. to less than 250° C.:
CH2—O (1)
with the proviso excluding the case where the moiety represented by the formula (1) is a part of —CH2—O—H.

### Claim 17 (depends on 1)

The method for producing a polycarbonate resin according to claim 1, wherein
the glass transition temperature of the polycarbonate resin fed to said extruder is from 80° C. to less than 145° C., and
the glass transition temperature of the polycarbonate resin obtained from said extruder is from 80° C. to less than 145° C.