# US 9,353,208 B2 · Method for preparing a sol-gel resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,208 B2
- Document ID: US9353208B2
- Status: Granted
- Kind: B2
- Application number: 14/259,884
- Filed: 2014-04-23
- Published: 2014-10-30
- Granted: 2016-05-31
- Earliest claimed: 2013-04-24
- Assignees: Hexion Inc.
- Applicants: Hexion Inc.
- Inventors: Stephen W. Arbuckle; Gabriele Badini; John Huggins; Sanjay Gangal
- Web page: https://patentgrep.com/patent/US9353208B2

## CPC

- C08G 8/24: with mixtures of two or more phenols which are not covered by only one of the groups C08G8/10 - C08G8/20
- C08G 8/22: Resorcinol
- C08J 3/12: Powdering or granulating
- C08L 61/12: with polyhydric phenols
- C08J 2361/08: with monohydric phenols
- C08J 2361/12: with polyhydric phenols
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Sol-gel resins can be prepared using one or two-step processes to produce small granules or pellets of resin that are easy to handle. The methods include agitating phenolic compounds and aldehydes in the presence of a catalyst and a solvent. The reactants are brought together over a period of time to avoid an undesirable buildup of heat within the reaction mass. Condensation of the material continues under agitation sufficient to knead the material as it gels. During this gelation, the material begins to form into smaller parts until particles, the shape of granules, are produced. The condensation continues to the degree that the material is no longer capable of sintering during packaging and storage. The material thus made can be easily discharged, packaged, portioned, and further processed.

## Claims

### Claim 1

A method for preparing a sol-gel resin comprising:
introducing a hydroxylated benzene and optionally a catalyst into a reactor;
introducing an aldehyde into the reactor with agitation to form a reaction mixture;
reacting the reaction mixture for a period of time sufficient to consume a portion of the hydroxylated benzene to form a liquid resin precursor;
transferring the liquid resin precursor from the reactor into a mixer; and
agitating the liquid resin precursor in the mixer for a period of time sufficient to form the sol-gel resin in a particulate form.

### Claim 2 (depends on 1)

The method of claim 1 wherein the reactor is configured to control the temperature of material therein.

### Claim 3 (depends on 1)

The method of claim 1 wherein the aldehyde is introduced into the reactor over a period of time sufficient to control a reaction exotherm.

### Claim 4 (depends on 3)

The method of claim 3 wherein the reaction exotherm is controlled for the period of time sufficient to consume more than above about 70% of the hydroxylated benzene.

### Claim 5 (depends on 3)

The method of claim 3 wherein the reaction exotherm is controlled for the period of time sufficient to consume from about 30% to about 90% of the aldehyde.

### Claim 6 (depends on 1)

The method of claim 1 wherein the resin precursor is agitated in the mixer at a temperature maintained between about 25° C. to about 120° C.

### Claim 7 (depends on 6)

The method of claim 6 wherein the temperature is maintained between about 40° C. to about 80° C.

### Claim 8 (depends on 1)

The method of claim 1 wherein the molar ratio of hydroxylated benzene to aldehyde is about 0.20 to about 0.75.

### Claim 9 (depends on 1)

The method of claim 1 wherein the resin precursor is agitated within the mixer under conditions sufficient to produce the sol-gel resin having an average particle size of from about 0.5 mm to about 20 mm.

### Claim 10 (depends on 1)

The method of claim 1 further comprising shaping the sol-gel resin into a desired geometry that does not sinter or agglomerate.

### Claim 11 (depends on 10)

The method of claim 10 wherein the shaped sol-gel resin is cured at a temperature of from about 50° C. to about 100° C.

### Claim 12 (depends on 1)

The method of claim 1 free of a step to isolate the sol-gel resin from a suspending liquid reaction media.

### Claim 13 (depends on 1)

The method of claim 1 free of reaction phases that are immiscible or insoluble with each other.

### Claim 14

A method for preparing a sol-gel resin comprising:
introducing a hydroxylated benzene and optionally a catalyst into a mixer;
introducing an aldehyde into the mixer with agitation to form a reaction mixture; and
agitating the reaction mixture for a period of time sufficient to form the sol-gel resin in a particulate form.

### Claim 15 (depends on 14)

The method of claim 14 wherein the mixer is configured to control the temperature of material therein.

### Claim 16 (depends on 14)

The method of claim 14 wherein the aldehyde is introduced into the mixer over a period of time sufficient to control a reaction exotherm.

### Claim 17 (depends on 16)

The method of claim 16 wherein the reaction exotherm is controlled for the period of time sufficient to consume more than above about 70% of the hydroxylated benzene.

### Claim 18 (depends on 16)

The method of claim 16 wherein the reaction exotherm is controlled for period of time sufficient to consume from about 30% to about 90% of the aldehyde.

### Claim 19 (depends on 14)

The method of claim 14 wherein the resin precursor is agitated in the mixer at a temperature maintained between about 25° C. to about 120° C.

### Claim 20 (depends on 19)

The method of claim 19 wherein the temperature is maintained between about 40° C. to about 80° C.

### Claim 21 (depends on 14)

The method of claim 14 wherein a molar ratio of hydroxylated benzene to aldehyde is about 0.20 to about 0.75.

### Claim 22 (depends on 14)

The method of claim 14 wherein the resin precursor is agitated within the mixer under conditions sufficient to produce the sol-gel resin having an average particle size of from about 0.5 mm to about 20 mm.

### Claim 23 (depends on 14)

The method of claim 14 further comprising shaping the sol-gel resin into a desired geometry that does not sinter or agglomerate.

### Claim 24 (depends on 23)

The method of claim 23 wherein the shaped sol-gel resin is cured at a temperature of from about 50° C. to about 100° C.

### Claim 25 (depends on 1)

The method of claim 1 free of a step to isolate the sol-gel resin from a suspending liquid reaction media.

### Claim 26 (depends on 14)

The method of claim 14 free of reaction phases that are immiscible or insoluble with each other.