# US 9,353,199 B2 · Golf ball resin composition and golf ball

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,199 B2
- Document ID: US9353199B2
- Status: Granted
- Kind: B2
- Application number: 13/728,644
- Filed: 2012-12-27
- Published: 2013-07-04
- Granted: 2016-05-31
- Earliest claimed: 2011-12-28
- Assignees: Dunlop Sports Co. Ltd.
- Applicants: Dunlop Sports Co., Ltd.
- Inventors: Kazuyoshi Shiga; Ryo Murakami; Takahiro Shigemitsu
- Web page: https://patentgrep.com/patent/US9353199B2

## CPC

- C08F 22/02: Acids; Metal salts or ammonium salts thereof {, e.g. maleic acid or itaconic acid}
- A63B 37/0051: {Materials other than polybutadienes; Constructional details}
- A63B 37/0054: {Substantially rigid, e.g. metal}
- A63B 37/0059: {Ionomer}
- A63B 37/006: {Physical properties}
- A63B 37/0073: {Solid, i.e. formed of a single piece}
- C08K 5/098: Metal salts of carboxylic acids
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

An object of the present invention is to provide a golf ball excellent in a shot feeling and resilience. The present invention provides a golf ball resin composition comprising (A) at least one resin component selected from the group consisting of (a-1) a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms, (a-2) an ionomer resin consisting of a metal ion-neutralized product of the binary copolymer, (a-3) a ternary copolymer composed of the binary copolymer components and an α,β-unsaturated carboxylic acid ester, and (a-4) an ionomer resin consisting of a metal ion-neutralized product of the ternary copolymer components; and (B) a basic metal salt of a fatty acid, and having a spin-lattice relaxation time (T1) of 13C nucleus of 5.56 seconds or shorter measured by a High resolution solid state nuclear magnetic resonance (NMR) method.

## Claims

### Claim 1

A golf ball resin composition comprising:
(A) at least one resin component selected from the group consisting of
(a-1) a binary copolymer composed of an olefin and an α, β-unsaturated carboxylic acid having 3 to 8 carbon atoms,
(a-2) an ionomer resin consisting of a metal ion-neutralized product of a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8carbon atoms,
(a-3) a ternary copolymer composed of an olefin, an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester, and
(a-4) an ionomer resin consisting of a metal ion-neutralized product of a ternary copolymer composed of an olefin, an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester; and
(B) a basic metal salt of a fatty acid, and having a spin-lattice relaxation time (T1) of 13C nucleus measured by a high resolution solid state nuclear magnetic resonance (NMR) method of 5.56 seconds or shorter,
wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 100 parts by mass with respect to 100 parts by mass of (A) the resin component, and
wherein the basic metal salt of the fatty acid is represented by the following general formula (1):
mM1O.M2(RCOO)2 (1)
wherein m ranges from 0.8 to 2.0, RCOO represents a residue of the fatty acid, and M1 and M2 are magnesium, respectively.

### Claim 2 (depends on 1)

The golf ball resin composition according to claim 1, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of a fatty acid having 8 to 30 carbon atoms.

### Claim 3 (depends on 2)

The golf ball resin composition according to claim 2, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of an unsaturated fatty acid.

### Claim 4 (depends on 3)

The golf ball resin composition according to claim 3, wherein the unsaturated fatty acid component of (B) the basic metal salt of the fatty acid is at least one component selected from the group consisting of oleic acid, erucic acid, linoleic acid, linolenic acid, arachidonic acid, eicosapentaenoic acid, docosahexaenoic acid, stearidonic acid, nervonic acid, vaccenic acid, gadoleic acid, elaidic acid, eicosenoic acid, eicosadienoic acid, docosadienoic acid, pinolenic acid, eleostearic acid, mead acid, adrenic acid, clupanodonic acid, nishinic acid, and tetracosapentaenoic acid.

### Claim 5 (depends on 1)

The golf ball resin composition according to claim 1, wherein the golf ball resin composition has a slab hardness in a range from 20 to 65 in Shore D hardness.

### Claim 6 (depends on 1)

The golf ball resin composition according to claim 1, wherein the golf ball resin composition has a melt flow rate (190° C., 2.16 kg) in a range from 0.01 g/10 min to 100 g/10 min.

### Claim 7 (depends on 1)

The golf ball resin composition according to claim 1, wherein the golf ball resin composition has a rebound resilience of 40% or more.

### Claim 8 (depends on 1)

The golf ball resin composition according to claim 1, wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 70.2 parts by mass with respect to 100 parts by mass of (A) the resin component.

### Claim 9

A golf ball comprising a core composed of at least one layer and a cover covering the core, wherein at least one layer of the core is formed from a golf ball resin composition comprising:
(A) at least one resin component selected from the group consisting of
(a-1) a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms,
(a-2) an ionomer resin consisting of a metal ion-neutralized product of a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms,
(a-3) a ternary copolymer composed of an olefin, an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester, and
(a-4) an ionomer resin consisting of a metal ion-neutralized product of a ternary copolymer composed of an olefin, an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester; and
(B) a basic metal salt of a fatty acid, and having a spin-lattice relaxation time (T1) of 13C nucleus measured by a high resolution solid state nuclear magnetic resonance (NMR) method of 5.56 seconds or shorter,
wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 100 parts by mass with respect to 100 parts by mass of (A) the resin component, and
wherein the basic metal salt of the fatty acid is represented by the following general formula (1):
mM1O.M2(RCOO)2 (1)
wherein m ranges from 0.8 to 2.0, RCOO represents a residue of the fatty acid, and M1 and M2 are magnesium, respectively.

### Claim 10 (depends on 9)

The golf ball according to claim 9, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of a fatty acid having 8 to 30 carbon atoms.

### Claim 11 (depends on 9)

The golf ball according to claim 9, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of an unsaturated fatty acid.

### Claim 12 (depends on 11)

The golf ball according to claim 11, wherein the unsaturated fatty acid component of (B) the basic metal salt of the fatty acid is at least one component selected from the group consisting of oleic acid, erucic acid, linoleic acid, linolenic acid, arachidonic acid, eicosapentaenoic acid, docosahexaenoic acid, stearidonic acid, nervonic acid, vaccenic acid, gadoleic acid, elaidic acid, eicosenoic acid, eicosadienoic acid, docosadienoic acid, pinolenic acid, eleostearic acid, mead acid, adrenic acid, clupanodonic acid, nishinic acid, and tetracosapentaenoic acid.

### Claim 13 (depends on 9)

The golf ball according to claim 9, wherein the golf ball resin composition has a slab hardness in a range from 20 to 65 in Shore D hardness, a melt flow rate (190° C., 2.16 kg) in a range from 0.01 g/10 min to 100 g/10 min, and a rebound resilience of 40% or more.

### Claim 14 (depends on 9)

The golf ball according to claim 9, wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 70.2 parts by mass with respect to 100 parts by mass of (A) the resin component.

### Claim 15

A one-piece golf ball comprising a golf ball body formed from a golf ball resin composition, wherein the golf ball resin composition comprises:
(A) at least one resin component selected from the group consisting of
(a-1) a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms,
(a-2) an ionomer resin consisting of a metal ion-neutralized product of a binary copolymer composed of an olefin and an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms,
(a-3) a ternary copolymer composed of an olefin, an α,β-unsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester, and
(a-4) an ionomer resin consisting of a metal ion-neutralized product of a ternary copolymer composed of an olefin, an α,βunsaturated carboxylic acid having 3 to 8 carbon atoms and an α,β-unsaturated carboxylic acid ester; and
(B) a basic metal salt of a fatty acid, and has a spin-lattice relaxation time (T1) of 13C nucleus measured by a high resolution solid state nuclear magnetic resonance (NMR) method of 5.56 seconds or shorter,
wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 100 parts by mass with respect to 100 parts by mass of (A) the resin component, and
wherein the basic metal salt of the fatty acid is represented by the following general formula (1):
mM1O.M2(RCOO)2 (1)
wherein m ranges from 0.8 to 2.0, RCOO represents a residue of the fatty acid, and M1 and M2 are magnesium, respectively.

### Claim 16 (depends on 15)

The one-piece golf ball according to claim 15, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of a fatty acid having 8 to 30 carbon atoms.

### Claim 17 (depends on 15)

The one-piece golf ball according to claim 15, wherein (B) the basic metal salt of the fatty acid is a basic metal salt of an unsaturated fatty acid.

### Claim 18 (depends on 17)

The one-piece golf ball according to claim 17, wherein the unsaturated fatty acid component of (B) the basic metal salt of the fatty acid is at least one component selected from the group consisting of oleic acid, erucic acid, linoleic acid, linolenic acid, arachidonic acid, eicosapentaenoic acid, docosahexaenoic acid, stearidonic acid, nervonic acid, vaccenic acid, gadoleic acid, elaidic acid, eicosenoic acid, eicosadienoic acid, docosadienoic acid, pinolenic acid, eleostearic acid, mead acid, adrenic acid, clupanodonic acid, nishinic acid, and tetracosapentaenoic acid.

### Claim 19 (depends on 15)

The one-piece golf ball according to claim 15, wherein the golf ball resin composition has a slab hardness in a range from 20 to 65 in Shore D hardness, a melt flow rate (190° C., 2.16 kg) in a range from 0.01 g/10 min to 100 g/10 min, and a rebound resilience of 40% or more.

### Claim 20 (depends on 15)

The one-piece golf ball according to claim 15, wherein (B) the basic metal salt of the fatty acid is present in an amount range of from 25 parts to 70.2 parts by mass with respect to 100 parts by mass of (A) the resin component.