# US 9,353,196 B2 · Bimodal polymerization process utilizing chromium/silica catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,196 B2
- Document ID: US9353196B2
- Status: Granted
- Kind: B2
- Application number: 14/085,198
- Filed: 2013-11-20
- Published: 2015-05-21
- Granted: 2016-05-31
- Earliest claimed: 2013-11-20
- Assignees: Equistar Chemicals, LP
- Applicants: Equistar Chemicals, LP
- Inventors: Michael W. Lynch; Sebastian Joseph
- Web page: https://patentgrep.com/patent/US9353196B2

## CPC

- C08F 4/78: selected from chromium, molybdenum or tungsten
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 2410/06: Catalyst characterized by its size
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to novel methods for producing a bimodal or broad distribution of molecular weight polyolefin polymers using Cr/silica catalysts. In some aspects the methods utilize different pressures of hydrogen to tailor the properties of the polymer. In particular aspects, a method of preparing a polyolefin having a bimodal molecular weight distribution, comprising: (a) preparing a reaction mixture comprising a monomer, a catalyst, and an organic solvent; (b) heating the reaction mixture under a first set of reaction conditions to effect a first polymerization comprising the polymerization of a first fraction of the monomer; and (c) heating the reaction mixture under a second set of reaction conditions to effect a second polymerization comprising the polymerization of a second fraction of the monomer.

## Claims

### Claim 1

A method of preparing a polyolefin having a bimodal molecular weight distribution, comprising:
(a) preparing a reaction mixture comprising a monomer, a catalyst, and an organic solvent,
(b) heating the reaction mixture under a first set of reaction conditions to effect a first polymerization comprising the polymerization of a first fraction of the monomer; and
(c) heating the reaction mixture under a second set of reaction conditions to effect a second polymerization comprising the polymerization of a second fraction of the monomer;
wherein the monomer is a terminal alkene(C2-8), the catalyst comprises an oxide-supported chromium catalyst, and the first or second set of reaction conditions comprises the presence of hydrogen, provided that the first set of reaction conditions and the second set of reaction conditions are not the same; and whereby the method produces a polyolefin having a bimodal molecular weight distribution; and
wherein the catalyst comprises 0.1 to 2% by weight chromium.

### Claim 2 (depends on 1)

The method of claim 1, wherein the terminal alkene(C2-8 ) is ethylene.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polyolefin is polyethylene.

### Claim 4 (depends on 1)

The method of claims 1, wherein the organic solvent is isobutane.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first mode of the molecular weight distribution is from 80,000 Dalton to 130,000 Daltons and wherein the second mode of the molecular weight distribution is from about 84,000 Daltons ref 300,000 Daltons, provided that the first and the second modes differ by at least 4,000 Daltons.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first set of reaction conditions comprises a temperature from 85° C. to 110° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second set of reaction conditions comprises a temperature from 70° C. to 110° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the catalyst further comprises one or more of the elements titanium, aluminum, fluorine, boron, and phosphorus.

### Claim 9 (depends on 8)

The method of claim 8, wherein the catalyst further comprises 0.1 to 4% by weight titanium.

### Claim 10 (depends on 1)

The method of claim 1, wherein the catalyst has a surface area from 250 m2 /g to 900 m2/g and a pore volume from 1.5 mL/g to 3.0 mL/g.

### Claim 11 (depends on 1)

The method of claim 1, wherein the hydrogen concentration of the first set of reaction conditions is from 0.1 to 2 mole %.

### Claim 12 (depends on 1)

The method of claim 1, wherein the hydrogen concentration of the second set of reaction conditions is from 0.1 to 2 mole %.

### Claim 13 (depends on 1)

The method of claim 1, further comprising reducing hydrogen concentration between steps (b) and (c) using a hydrogen disengagement vessel.

### Claim 14 (depends on 1)

The method of claim 1, wherein the first or second polymerization further comprises a copolymerization of the monomer with a comonomer, wherein the comonomer is a terminal alkene (C2-8), provided that monomer and the comonomer are not the same.

### Claim 15 (depends on 14)

The method of claim 14, wherein the comonomer is 1-hexene.

### Claim 16 (depends on 1)

The method of claim 1 wherein the reaction mixture further comprises a cocatalyst.

### Claim 17 (depends on 16)

The method of claim 16, wherein the cocatalyst is an alkyl metal of the formula M(R)n, wherein M is Al3+, B3+, Zn2+, or Li+; R is alkyl(C≦8); and n is the number of alkyl groups, which corresponds to the oxidation state of M.

### Claim 18 (depends on 17)

The method of claim 17, wherein the cocatalyst is triethyl boron.

### Claim 19 (depends on 1)

The method of claim 1, wherein the polyolefin has a melt index from 0.02 g/10 minutes to 2 g/10 minutes, a high load melt index from 2 g/10 minutes to 100 g/10 minutes, or a high load melt index to melt index ratio from 80 to 250.