# US 9,353,014 B2 · Process for sintering silicon carbide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,353,014 B2
- Document ID: US9353014B2
- Status: Granted
- Kind: B2
- Application number: 14/321,215
- Filed: 2014-07-01
- Published: 2015-01-01
- Granted: 2016-05-31
- Earliest claimed: 2013-07-01
- Applicants: Dale Adams
- Inventors: Dale Adams
- Web page: https://patentgrep.com/patent/US9353014B2

## CPC

- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C01B 32/956: Silicon carbide
- C04B 20/002: {Hollow or porous granular materials}
- C04B 35/575: obtained by pressure sintering
- C04B 35/634: Polymers (C04B35/636 takes precedence)
- C04B 35/638: Removal thereof
- C04B 38/00: Porous mortars, concrete, artificial stone or ceramic ware; Preparation thereof (treating slag with gases or gas generating material C04B5/06 {; expanded graphite C04B35/536})
- C04B 38/009: {Porous or hollow ceramic granular materials, e.g. microballoons (C04B18/027, C04B20/002 take precedence)}
- C04B 2235/6023: Gel casting
- C04B 2235/606: Drying
- C04B 2235/6587: Influencing the atmosphere by vaporising a solid material, e.g. by using a burying of sacrificial powder
- C04B 2235/72: Products characterised by the absence or the low content of specific components, e.g. alkali metal free alumina ceramics
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A process for sintering silicon carbide is provided which includes the steps of providing a silicon carbide powder of silicon carbide granules; purifying the silicon carbide powder; subjecting the purified silicon carbide powder to a gel-casting process; removing the gel-cast part from the mold; drying the gel-cast part; obtaining a dried cast ceramic part (a green body) which is capable of green machining into a final desired shape; firing the green body in an oven at temperatures ranging from about 100° C. to about 1900° C. to remove or burn out any polymer remaining in the ceramic; and sintering the green body at temperatures ranging from about 1600° C. to less than about 2200° C.

## Claims

### Claim 1

A process for sintering silicon carbide comprising:
a) providing a silicon carbide powder of silicon carbide granules;
b) purifying the silicon carbide powder by
b. 1) washing the silicon carbide powder with a solution of hydrofluoric acid,
b. 2) rinsing the silicon carbide powder in distilled water; and
b. 3) drying the silicon carbide powder to obtain a pure silicon carbide powder, wherein granules which form the silicon carbide powder are substantially free of a silicon dioxide shell; and
c) subjecting the purified silicon carbide powder to a gel-casting process comprising the following steps:
c. 1) mixing the silicon carbide powder with water or a non-aqueous solvent, a dispersant, and gel-forming organic monomers to obtain a ceramic slurry;
c. 2) exposing the ceramic slurry to a partial vacuum to remove air from the ceramic slurry;
c. 3) adding a polymerization initiator to the ceramic slurry to commence a gel-forming chemical reaction;
c. 4) pouring the ceramic slurry into a mold and casting the ceramic slurry into a desired workpiece shape; and
c. 5) heating the mold in a curing oven or setting the mold with a catalyst;
d) removing a gel-cast part from the mold;
e) drying the gel-cast part to remove the water or the non-aqueous solvent and obtain a dried cast ceramic part;
f) firing the dried cast ceramic part in an oven at temperatures ranging from about 100° C. to about 1600° C.; and,
g) sintering the dried cast ceramic part at temperatures ranging from about 1600° C. to less than about 2200° C., wherein the dried cast ceramic part is sintered within a capped crucible of pressurized molten liquid, wherein the pressure is obtained by capping of the crucible and application of vibratory forces to the molten liquid.

### Claim 2 (depends on 1)

The process of claim 1, wherein ultrasonic vibrations are applied during step c. 4).

### Claim 3 (depends on 1)

The process of claim 1, wherein ultrasonic vibrations are applied during step c. 5).

### Claim 4 (depends on 3)

The process of claim 3, wherein the mold is subjected to a de-airing step during vibration of step c. 5) to drive air out and orientate the silicon carbide particles to each other.

### Claim 5 (depends on 4)

The process of claim 4, wherein the de-airing step comprises application of low pressure to the mold, wherein the pressure is less than about 1000 psi.

### Claim 6 (depends on 1)

The process of claim 1, wherein ultrasonic vibrations are applied during step c. 1).

### Claim 7 (depends on 1)

The process of claim 1, wherein ultrasonic vibrations are applied during step c. 2).

### Claim 8 (depends on 1)

The process of claim 1, wherein ultrasonic vibrations are applied during steps b), c.1), c.2), c. 4), and c. 5).

### Claim 9 (depends on 1)

The process of claim 1, wherein vibratory forces are applied to the dried cast ceramic part during step g).

### Claim 10 (depends on 9)

The process of claim 9, wherein the dried cast ceramic part is heated within a capped graphite crucible containing the molten liquid through induction heating.

### Claim 11 (depends on 10)

The process of claim 10, wherein the vibratory forces are applied to the dried cast ceramic part through application of a pulsating electric current to the molten liquid.

### Claim 12 (depends on 11)

The process of claim 11, wherein the vibratory forces compact the silicon carbide granules to achieve a particle size of approximately one micron.

### Claim 13 (depends on 11)

The process of claim 11, wherein the molten liquid is conductive.

### Claim 14 (depends on 13)

The process of claim 13, wherein the molten liquid is fluorite.

### Claim 15 (depends on 14)

The process of claim 14, wherein the molten liquid is induction heated to a temperature ranging from about 1600° C. to about 2100° C.

### Claim 16 (depends on 15)

The process of claim 15, wherein the dried cast ceramic part is cored during the gel-casting process of step c) with a wax that will burnout during the drying and sintering process.

### Claim 17 (depends on 16)

The process of claim 16, wherein the dried cast ceramic part is sufficiently vented to allow an influx of the molten liquid into chambers within the gel-cast part allowing pressure to be evenly distributed on every surface of the dried cast ceramic part for obtaining a hollow silicon carbide part.

### Claim 18 (depends on 17)

The process of claim 17, wherein sintering takes place in a high carbon flame (rich fuel/air mixture) to facilitate the formation of silicon carbide.

### Claim 19 (depends on 18)

The process of claim 18, wherein the hollow silicon carbide parts are filled with urethane and para-aramid synthetic fibers.

### Claim 20 (depends on 18)

The process of claim 18, wherein the hollow silicon carbide part is porous and may be used as a fuel diffuser which is capable of retaining an air/fuel mixture within the interior of silicon carbide part and of diffusing the retained air/fuel mixture outside of the porous silicon carbide part for combustion.

### Claim 21 (depends on 10)

The process of claim 10, wherein the crucible is held within an inert atmosphere to keep from being consumed as fuel at sintering temperatures, wherein the inert atmosphere comprises nitrogen gas.