# US 9,352,999 B2 · Glass composition for producing high strength and high modulus fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,352,999 B2
- Document ID: US9352999B2
- Status: Granted
- Kind: B2
- Application number: 13/719,508
- Filed: 2011-06-30
- Published: 2013-05-16
- Granted: 2016-05-31
- Earliest claimed: 2010-06-30
- Assignees: OCV Intellectual Capital, LLC
- Applicants: Douglas A. Hofmann; Peter Bernard McGinnis
- Inventors: Douglas A. Hofmann; Peter Bernard McGinnis
- Web page: https://patentgrep.com/patent/US9352999B2

## CPC

- C03C 13/00: Fibre or filament compositions (manufacture of fibres or filaments C03B37/00)
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- B29K 2309/08: Glass
- B29L 2031/085: {Wind turbine blades}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 442/2934: Coating or impregnation contains vinyl polymer or copolymer
- Y10T 442/2951: Coating or impregnation contains epoxy polymer or copolymer or polyether
- Y10T 442/2992: Coated or impregnated glass fiber fabric
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass composition including SiO2 in an amount from about 69.5 to about 80.0% by weight, Al2O3 in an amount from about 5.0 to about 18.5% by weight, MgO in an amount from about 5.0 to about 14.75% by weight, CaO in an amount from 0.0 to about 3.0% by weight, Li2O in an amount from about 3.25 to about 4.0% by weight, and Na20 in an amount from 0.0 to about 2.0% by weight is provided. Glass fibers formed from the inventive composition may be used in applications that require high strength, high stiffness, and low weight. Such applications include, but are not limited to, woven fabrics for use in forming wind blades, armor plating, and aerospace structures.

## Claims

### Claim 1

A composition for preparing high strength, light weight glass fibers comprising:
SiO2 in an amount from about 69.5 to about 80.0%% by weight of the total composition,
Al2O3 in an amount from about 5.0 to about 18.5% by weight of the total composition,
CaO in an amount from 0.0 to about 3.0% by weight of the total composition,
MgO in an amount from 5.0 to about 14.75% by weight of the total composition,
Li2O in an amount from 3.25 to about 4.0% by weight of the total composition, and
Na2O in an amount from 0.0 to about 2.0% by weight of the total composition, wherein said composition comprises less than 1.0% by weight of B2O3 and wherein said composition is capable of producing glass fibers having a specific modulus of about 33.9 MJ/kg to about 35 MJ/kg.

### Claim 2 (depends on 1)

The glass composition of claim 1, wherein
Al2O3 is present in an amount from about 9.0 to about 15.4% by weight of the total composition, and
MgO is present in an amount from 5.0 to about 10.2% by weight of the total composition.

### Claim 3 (depends on 2)

The glass composition of claim 2, wherein
Al2O3 is present in an amount from about 9.5 to about 15.3% by weight of the total composition, and
MgO is present in an amount from 6.9 to about 10.2% by weight of the total composition.

### Claim 4 (depends on 1)

The glass composition of claim 1, wherein
SiO2 is present in an amount from about 69.5 to about 74.5% by weight of the total composition, and
Al2O3 is present in an amount from about 10.30 to about 18.5% by weight of the total composition.

### Claim 5 (depends on 1)

The glass composition of claim 1, wherein
SiO2 is present in an amount from about 69.5 to about 76.5% by weight of the total composition, and
Al2O3 is present in an amount from about 5.0 to about 15.4% by weight of the total composition.

### Claim 6 (depends on 1)

The composition of claim 1, wherein said composition is free of B2O3 and fluorine.

### Claim 7 (depends on 1)

The composition of claim 1, wherein said composition has a ΔT up to about 250° C.

### Claim 8 (depends on 1)

The composition of claim 1, wherein said composition has a ΔT of from about 100° C. to about 250° C.

### Claim 9 (depends on 1)

The composition of claim 1, wherein said composition has a log 3 temperature from about 1255° C. to about 1550° C.

### Claim 10 (depends on 1)

The composition of claim 1, wherein said composition has a liquidus temperature no greater than about 1510° C.

### Claim 11 (depends on 1)

The composition of claim 1, wherein components of said composition are melted in a refractory tank melter.

### Claim 12 (depends on 1)

A continuous high strength, light weight glass fiber produced from a composition according to claim 1.

### Claim 13 (depends on 12)

The glass fiber of claim 12, wherein said glass fiber has a specific strength from about 1.74 MJ/kg to about 2.09 MJ/kg.

### Claim 14 (depends on 12)

The glass fiber of claim 12, wherein said glass fiber has a pristine fiber tensile strength between about 4200 and about 5000 MPa, a modulus between about 80 and about 86 GPa, and a density between about 2.35 and about 2.46 g/cc.

### Claim 15 (depends on 12)

A method of preparing a reinforced composite product comprising combining at least one polymer matrix material and a plurality of glass fibers according to claim 12.

### Claim 16 (depends on 13)

The glass fiber of claim 13, wherein said glass fiber has a specific strength of greater than 2.01 MJ/Kg and less than or equal to about 2.09 MJ/kg.

### Claim 17 (depends on 1)

The glass fiber of claim 1, wherein said glass fiber has a specific modulus of greater than 34.1 MJ/Kg and less than or equal to about 35.0 MJ/kg.

### Claim 18 (depends on 1)

A method of forming a continuous high performance glass fiber comprising:
providing a molten glass composition including a composition according to claim 1; and
drawing said molten glass composition through orifices in a bushing to form a continuous glass fiber.

### Claim 19 (depends on 18)

The method of claim 18, wherein said glass fiber has a specific strength from about 1.74 MJ/kg to about 2.09 MJ/kg.

### Claim 20 (depends on 18)

The method of claim 18, wherein said glass fiber has a specific modulus of greater than 34.1 MJ/Kg and less than or equal to about 35.0 MJ/kg.

### Claim 21 (depends on 19)

The method of claim 19, wherein said glass fiber has a specific strength of greater than 2.01 MJ/Kg and less than or equal to about 2.09 MJ/kg.

### Claim 22 (depends on 18)

The method of claim 18, wherein said glass fiber has a pristine fiber tensile strength between about 4200 and about 5000 MPa, a modulus between about 80 and about 86 GPa, and a density between about 2.35 and about 2.46 g/cc.

### Claim 23 (depends on 18)

A method of preparing a reinforced composite product comprising:
preparing a plurality of glass fibers according to the method of claim 18 and combining said plurality of glass fibers with at least one polymer matrix material.

### Claim 24

A reinforced composite product comprising:
a polymer matrix; and
a plurality of glass fibers, said glass fibers being produced from a composition comprising:
SiO2 in an amount from about 69.5 to about 80.0%% by weight of the total composition,
Al2O3 in an amount from about 5.0 to about 18.5% by weight of the total composition,
CaO in an amount from 0.0 to about 1.8% by weight of the total composition,
MgO in an amount from 5.0 to about 14.75% by weight of the total composition,
Li2O in an amount from 3.25 to about 4.0% by weight of the total composition, and
Na2O in an amount from 0.0 to about 2.0% by weight of the total composition, wherein said composition has less than 1.0% by weight of B2O3.

### Claim 25 (depends on 24)

The composite product of claim 24, wherein said polymer matrix is a thermoplastic polymer selected from polyesters, polypropylene, polyamide, polyethylene terephtalate, polybutylene and combinations thereof.

### Claim 26 (depends on 24)

The composite product of claim 24, wherein said polymer matrix is a thermoset polymer selected from epoxy resins, unsaturated polyesters, phenolics, vinylesters and combinations thereof.