# US 9,352,987 B2 · Method of manufacturing compositions for removing halogenated hydrocarbons from contaminated environments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,352,987 B2
- Document ID: US9352987B2
- Status: Granted
- Kind: B2
- Application number: 14/100,854
- Filed: 2013-12-09
- Published: 2014-04-03
- Granted: 2016-05-31
- Earliest claimed: 2002-07-12
- Assignees: Remediation Products, Inc.
- Applicants: Remediation Products, Inc.
- Inventors: Scott Noland; Bob Elliott
- Web page: https://patentgrep.com/patent/US9352987B2

## CPC

- C02F 1/58: by removing specified dissolved compounds (using ion-exchange C02F1/42; softening water C02F5/00)
- B01J 20/02: comprising inorganic material
- B01J 20/20: comprising free carbon; comprising carbon obtained by carbonising processes
- B01J 20/28057: {Surface area, e.g. B.E.T specific surface area}
- B01J 20/28064: {being in the range 500-1000 m2/g}
- B01J 20/28066: {being more than 1000 m2/g}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3204: {Inorganic carriers, supports or substrates}
- B01J 20/3236: {containing metal, other than zeolites, e.g. oxides, hydroxides, sulphides or salts}
- B01J 21/18: Carbon
- B01J 23/745: Iron
- B01J 37/082: {Decomposition and pyrolysis}
- B09C 1/002: {involving in-situ ground water treatment}
- B09C 1/08: chemically
- B09C 1/10: microbiologically, {biologically} or by using enzymes
- C02F 1/283: {using coal, charred products, or inorganic mixtures containing them}
- C02F 1/288: {using composite sorbents, e.g. coated, impregnated, multi-layered}
- C02F 1/705: {Reduction by metals}
- C02F 3/104: {Granular carriers}
- C02F 3/2806: {Anaerobic processes using solid supports for microorganisms}
- C02F 3/34: characterised by the microorganisms used
- C09K 17/02: containing inorganic compounds only
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/618: {more than 1000 m2/g}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/16: Reducing
- B09C 2101/00: In situ
- C02F 1/281: {using inorganic sorbents}
- C02F 2101/101: {Sulfur compounds}
- C02F 2101/32: Hydrocarbons, e.g. oil
- C02F 2101/36: containing halogen
- C02F 2103/06: Contaminated groundwater or leachate
- C02F 2305/06: Nutrients for stimulating the growth of microorganisms
- Y02E 50/30: Fuel from waste, e.g. synthetic alcohol or diesel
- Y02W 10/10: Biological treatment of water, waste water, or sewage
- Y10T 428/12181: Composite powder [e.g., coated, etc.]
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B09C: RECLAMATION OF CONTAMINATED SOIL (gatherers for removing stone or the like from the soil A01B43/00; sterilising soil by steam A01G11/00; removing undesirable matter, e.g. rubbish, from the land E01H15/00)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a supported reactant for in situ remediation of soil and/or groundwater contaminated with a halogenated hydrocarbon consisting essentially of an adsorbent impregnated with elemental iron, wherein the adsorbent is capable of adsorbing the halogenated hydrocarbon. In one embodiment, the adsorbent is activated carbon.

## Claims

### Claim 1

A method of preparing a supported reactant for remediation of soil, wastewater, or groundwater, comprising:
providing a quantity of an adsorbent material comprising activated carbon capable of absorbing halogenated hydrocarbon contaminants;
treating the adsorbent material with a solution of water soluble iron salt to produce an intermediate product with iron salt impregnated into pores of the adsorbent material; and
subjecting the intermediate product to reducing conditions including heating the intermediate product to a reducing temperature to form elemental iron free of surface oxides within the pores of the adsorbent material,
wherein the reducing temperature is between 700 and 800° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the treating step comprises spraying the solution of water soluble iron salt onto the adsorbent material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the step of subjecting the intermediate product to reducing conditions includes introducing a reducing gas into a reaction chamber containing the intermediate product.

### Claim 4 (depends on 3)

The method of claim 3, further comprising, prior to the step of subjecting the intermediate product to reducing conditions:
loading the intermediate product into the reaction chamber; and
drying the intermediate product at an intermediate temperature of at least about 150° C.

### Claim 5 (depends on 4)

The method of claim 4, further comprising, after the drying of the intermediate product, heating the dried intermediate product to a temperature greater than the intermediate temperature to decompose the water soluble iron salt into an oxide.

### Claim 6 (depends on 5)

The method of claim 5, wherein the heating of the dried intermediate product is performed for a period of time selected to decompose the water soluble iron salt into an oxide.

### Claim 7 (depends on 3)

The method of claim 3, wherein the reducing gas comprises methane gas or hydrogen gas.

### Claim 8 (depends on 1)

The method of claim 1, wherein the treating comprises suspending the adsorbent material in a volume of the solution of water soluble iron salt to generate a suspension.

### Claim 9 (depends on 8)

The method of claim 8, further comprising, prior to the step of subjecting the intermediate product to reducing conditions, de-aerating the suspension to produce the intermediate product.

### Claim 10 (depends on 1)

The method of claim 1, wherein the water soluble iron salt comprises one or more of the group consisting of: iron (II/III) sulfate, iron chloride, iron citrate, and iron nitrate.

### Claim 11 (depends on 1)

The method of claim 1, wherein the activated carbon is porous with a surface area from 800 to 2000 m2/g.

### Claim 12

A method of preparing a supported reactant for remediation of soil, wastewater, or groundwater contaminated with a halogenated hydrocarbon, comprising:
spraying an adsorbent, comprising activated carbon, with a solution of water soluble metal salt to produce an intermediate product; and
in reducing conditions, heating the intermediate product at temperatures between 550 and 800° C. to produce a reactant with pores impregnated with a non-toxic metal free of surface oxides,
wherein the activated carbon is porous with a surface area from 800 to 2000 m2/g, and
wherein the non-toxic metal comprises elemental iron.

### Claim 13 (depends on 12)

The method of claim 12, wherein the elemental iron has a purity of at least about 99 percent.

### Claim 14 (depends on 12)

The method of claim 12, wherein the produced reactant has a pH above 7.0.

### Claim 15 (depends on 12)

The method of claim 12, wherein the produced reactant comprises between about 1 and 20 percent by weight of the non-toxic metal.

### Claim 16 (depends on 12)

The method of claim 12, wherein the reducing conditions include an atmosphere comprising methane or hydrogen gas.

### Claim 17

A method of preparing a supported reactant for remediation of soil, wastewater, or groundwater, comprising:
providing a quantity of an adsorbent material comprising activated carbon capable of absorbing halogenated hydrocarbon contaminants;
treating the adsorbent material with a solution of water soluble iron salt to produce an intermediate product with iron salt impregnated into pores of the adsorbent material; and
under reducing conditions, heating the intermediate product to a reducing temperature between 700 to 800° C.,
wherein a reactant is produced with pores impregnated with a material comprising elemental iron free of surface oxides,
wherein the produced reactant comprises about 1 to 20 percent by weight of the elemental iron, and
wherein the activated carbon is porous with a surface area from 800 to 2000 m2/g.

### Claim 18 (depends on 17)

The method of claim 17, wherein the adsorbent material comprises activated carbon and the treating includes spraying the activated carbon with the solution of water soluble iron salt.

### Claim 19 (depends on 17)

The method of claim 17, wherein the elemental iron has a purity of about 99 percent.

### Claim 20 (depends on 1)

The method of claim 1, wherein the elemental iron has a surface area in the range of 50 to 400 m2/(gm-deposited iron).