# US 9,352,976 B2 · Methods for preparing trimanganese tetroxide with low bet specific surface area, methods for controlling particle size of trimanganese tetroxide and trimanganese tetroxide product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,352,976 B2
- Document ID: US9352976B2
- Status: Granted
- Kind: B2
- Application number: 14/883,173
- Filed: 2015-10-14
- Published: 2016-02-04
- Granted: 2016-05-31
- Earliest claimed: 2012-06-26
- Assignees: Guizhou Redstar Developing Co., Ltd.
- Applicants: Guizhou Redstar Developing Co., Ltd.
- Inventors: Zhiguang Jiang; Dong Hua; Zhengtao Liu; Kaiwen Zeng
- Web page: https://patentgrep.com/patent/US9352976B2

## CPC

- C01G 45/028: Trimanganese tetraoxide
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/16: Oxides
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/12: Surface area
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides methods for preparing trimanganese tetroxide with low BET specific surface area and methods for controlling particle size of trimanganese tetroxide and trimanganese tetroxide product.

## Claims

### Claim 1

A method for preparing trimanganese tetroxide, comprising:
(1) a process for purifying air comprising purifying air by spraying dilute aqueous ammonia;
(2) a pretreatment of removing impurities from MnSO4 solution comprising adjusting pH value of the MnSO4 solution with a concentration in a range of 150˜200 g/L to 5.5-6.0, introducing H2S gas into the MnSO4 solution until pH value reaches 2.5-3.0, separating the mixture by solid-liquid separation to obtain a filtrate and a solid, purifying the filtrate by removing impurities with oxidization of H2O2, adjusting pH value of the filtrate to 5-6 with a base, and separating the obtained mixture by solid-liquid separation to obtain a filtrate and a solid, so as to obtain MnSO4 solution as filtrate for use;
(3) a process for preparing seed crystal comprising cooling the MnSO4 solution obtained in the process (2) from MnSO4 solution to a temperature of less than 40° C., and introducing liquid NH3 into the cooled MnSO4 solution until pH value reaches 10.5-11.0, separating the mixture by solid-liquid separation to obtain a filtrate and a solid; washing the obtained solid, adding deionized water to the washed solid and forming a slurry, introducing the purified air obtained in the process (1) into the slurry, and oxidizing the slurry into Mn3O4; separating the mixture by solid-liquid separation to obtain filtrate and solid, so as to obtain Mn3O4 seed crystal as solid for use; and
(4) a process for obtaining the final product by controlling oxidization comprising adding the MnSO4 solution obtained in the process (2) from MnSO4 solution into an oxidization reactor, adding Mn3O4 seed crystal obtained in the process for preparing seed crystal (3) according to the proportion of (0.012-0.040) kg of Mn3O4 seed crystal per cubic meter of the MnSO4 solution, adding the liquid ammonia, introducing the purified air obtained in the process for purifying air (1) into a reactor and turning on the recycle pump, controlling the temperature of the system in a range of 25±5° C., controlling pH value of the reaction system in a range of 6.5-7.5, which makes the MnSO4 solution circulate more than 6 times per hour so as to carry out circulatory oxidization reaction, not stopping the reaction until MnSO4 content of the reaction solution equal to or is less than 1.5 g/L, separating the mixture by solid-liquid separation to obtain a filtrate and a solid, washing and drying the solid to obtain Mn3O4 product.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in the process for purifying air (1), the air is purified by spraying dilute aqueous ammonia with a concentration of 0.5˜1.0 mol/L according to the proportion of 8˜10 L of the dilute aqueous ammonia per cubic meter of air.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in pretreatment (2), said MnSO4 solution is obtained from absorption of SO2 fume; H2O2 solution is added according to the proportion of 2.5 L H2O2 with weight content of 27.5 wt % per cubic meter of the MnSO4 solution.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, in the pretreatment (2), before the H2S gas is introduced into the MnSO4 solution, aqueous ammonia with a concentration of 10 mol/L is added to the MnSO4 solution so as to adjust pH value of the solution to 5.5-6.0.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, in the process for preparing seed crystal (3), D50 particle size of the obtained Mn3O4 seed crystal is 0.75-0.90 μm, preferably 0.82 μm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, in the process for preparing seed crystal (3), the liquid NH3 is introduced into the cooled MnSO4 solution until pH value reaches 11.0, and then the mixture is separated by solid-liquid separation to obtain filtrate and solid; the obtained solid is washed, and then deionized water is added to the washed solid and slurry is made; NH4HCO3 is added to the obtained filtrate so as to recovery manganese element.

### Claim 7 (depends on 1)

The method according to claim 1, wherein, in the process for preparing obtaining the final product (4), said drying is maintained for 24 hours in a temperature range of 140-150° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein, in the process for preparing obtaining the final product (4), the temperature of the system is controlled in a range of 25±5° C. by cool water jacket.

### Claim 9 (depends on 8)

The method according to claim 8, wherein, in the process for preparing obtaining the final product (4), the temperature of the system is controlled at 25° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein, in the process for preparing obtaining the final product (4), the Al element containing salt is added to the MnSO4 solution and is reacted with the purified air obtained in the process (1) together with MnSO4 solution and liquid ammonia.