# US 9,352,968 B2 · Graphene materials having randomly distributed two-dimensional structural defects

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,352,968 B2
- Document ID: US9352968B2
- Status: Granted
- Kind: B2
- Application number: 14/025,572
- Filed: 2013-09-12
- Published: 2014-01-16
- Granted: 2016-05-31
- Earliest claimed: 2011-05-12
- Assignees: Northwestern University
- Applicants: Northwestern University
- Inventors: Harold H. Kung; Xin Zhao; Cary M. Hayner; Mayfair C. Kung
- Web page: https://patentgrep.com/patent/US9352968B2

## CPC

- C01B 32/23: Oxidation
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/192: starting from graphitic oxides
- H01B 1/04: mainly consisting of carbon-silicon compounds, carbon or silicon
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Graphene-based storage materials for high-power battery applications are provided. The storage materials are composed of vertical stacks of graphene sheets and have reduced resistance for Li ion transport. This reduced resistance is achieved by incorporating a random distribution of structural defects into the stacked graphene sheets, whereby the structural defects facilitate the diffusion of Li ions into the interior of the storage materials.

## Claims

### Claim 1

A method, comprising:
a) exposing one or more graphene sheets to an acid creating at least one defect pore formed from a carbon vacancy disposed within the one or more graphene sheets;
b) removing the acid from the one or more graphene sheets; and
c) exposing the one or more graphene sheets to a first elevated temperature to thereby form a structure in which at least a portion of the one or more graphene sheets comprise crystalline graphite.

### Claim 2 (depends on 1)

The method of claim 1 wherein the at least one defect pore within the one or more graphene sheets has an average diameter of about 1 nm to about 100 nm.

### Claim 3 (depends on 1)

The method of claim 1 wherein the at least one defect pore comprises a plurality of defect pores having an average diameter and an average separation distance that extends between adjacent defect pores, wherein the defect pores have an average density within one graphene sheet of at least 3, wherein the average defect pore density is measured by a ratio of the average separation distance between adjacent defect pores to the average pore diameter within the graphene sheet.

### Claim 4 (depends on 1)

The method of claim 1 wherein the step of exposing the one or more graphene sheets to the acid comprises exposing one or more exfoliated, oxidized graphene sheets to the acid.

### Claim 5 (depends on 1)

The method of claim 1 further comprising attaching a carboxylate group to a respective perimeter of the at least one defect pore.

### Claim 6 (depends on 1)

The method of claim 1 wherein lithium ions are capable of diffusing through the at least one defect pore within the one or more graphene sheets.

### Claim 7 (depends on 1)

The method of claim 1 wherein the at least one defect pores is a two-dimensional defect pore disposed within a plane of the one or more graphene sheets.

### Claim 8 (depends on 1)

The method of claim 1 wherein the acid comprises HNO3.

### Claim 9 (depends on 1)

The method of claim 1 further comprising exposing the one or more graphene sheets to the first elevated temperature to reduce the one or more graphene sheets from a graphene oxide to graphene.

### Claim 10 (depends on 9)

The method of claim 9 further comprising:
a) mixing the one or more graphene sheets with electrochemically active particles, wherein the one or more graphene sheets have at least one defect pore formed from a carbon vacancy disposed therewithin, and wherein the electrochemically active particles are dispersed between adjacent graphene sheets; and
b) exposing the mixture of the one or more graphene sheets and electrochemically active particles to a second elevated temperature, thereby forming a material structure having a network of graphitic regions, wherein the network of graphitic regions has at least one crystalline structure portion and at least one disordered structure portion.

### Claim 11 (depends on 10)

The method of claim 10 wherein the electrochemically active particles are dispersed between, and in electrochemical contact with, the one or more graphene sheets that comprise the disordered structure portion.

### Claim 12 (depends on 10)

The method of claim 10 wherein the electrochemically active particles comprise silicon.

### Claim 13 (depends on 10)

The method of claim 10 wherein the first and second elevated temperatures are at least about 700° C.

### Claim 14

A method, comprising:
a) exposing a plurality of graphene sheets to an acid creating at least one defect pore formed from a carbon vacancy disposed within at least one of the plurality of graphene sheets;
b) mixing the plurality of graphene sheets with electrochemically active particles, wherein the electrochemically active particles are dispersed between adjacent graphene sheets;
c) removing the acid from the plurality of graphene sheets; and
d) exposing the mixture of graphene sheets and electrochemically active particles to an elevated temperature, thereby forming a material structure having a network of graphitic regions, wherein the network of graphitic regions has at least one crystalline structure portion and at least one disordered structure portion.

### Claim 15 (depends on 14)

The method of claim 14 wherein the electrochemically active particles are dispersed between, and in electrochemical contact with, the graphene sheets that comprise the at least one disordered structure portion.

### Claim 16 (depends on 14)

The method of claim 14 wherein the electrochemically active particles comprise silicon.

### Claim 17 (depends on 14)

The method of claim 14 wherein the at least one defect pore comprises a diameter that ranges from about 1 nm to about 100 nm.

### Claim 18 (depends on 4)

The method of claim 4 wherein the at least one defect pore comprises a plurality of defect pores having an average diameter and an average separation distance that extends between adjacent defect pores, wherein the defect pores have an average density within one graphene sheet of at least 3, wherein the average defect pore density is measured by a ratio of the average separation distance between adjacent defect pores to the average pore diameter within the graphene sheet.

### Claim 19 (depends on 14)

The method of claim 14 wherein the elevated temperature is at least about 700° C.

### Claim 20 (depends on 14)

The method of claim 14 wherein the acid comprises HNO3.

### Claim 21 (depends on 14)

The method of claim 14 wherein the step of exposing the one or more graphene sheets to the acid comprises exposing one or more exfoliated, oxidized graphene sheets to the acid.

### Claim 22 (depends on 14)

The method of claim 14 wherein the step of removing the acid occurs before the step of mixing the plurality of graphene sheets with electrochemically active particles.

### Claim 23 (depends on 14)

The method of claim 14 wherein exposing the mixture of reduced graphene sheets and electrochemically active particles to the elevated temperature causes at least a portion of the plurality of graphene sheets to reduce from a graphene oxide to graphene.