# US 9,352,534 B2 · Ceramic plate structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,352,534 B2
- Document ID: US9352534B2
- Status: Granted
- Kind: B2
- Application number: 14/492,455
- Filed: 2014-09-22
- Published: 2016-03-24
- Granted: 2016-05-31
- Earliest claimed: 2014-09-22
- Assignees: Jen Long Vacuum Industrial Co., Ltd.
- Applicants: Jen Long Vacuum Industrial Co., Ltd.
- Inventors: Rong-Fu Wu
- Web page: https://patentgrep.com/patent/US9352534B2

## CPC

- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C03C 17/3417: {all coatings being oxide coatings}
- C03C 17/3435: {comprising a nitride, oxynitride, boronitride or carbonitride}
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C04B 37/008: {by means of an interlayer consisting of an organic adhesive, e.g. phenol resin or pitch}
- C04B 37/04: with articles made from glass
- B32B 2307/40: having particular optical properties
- B32B 2307/412: Transparent
- B32B 2457/208: Touch screens
- C03C 2217/212: TiO2
- C03C 2217/213: SiO2
- C03C 2217/214: Al2O3
- C03C 2217/281: Nitrides
- C03C 2217/29: Mixtures
- C03C 2217/78: Coatings specially designed to be durable, e.g. scratch-resistant
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- C04B 2237/062: based on silica or silicates
- C04B 2237/08: Non-oxidic interlayers
- C04B 2237/341: Silica or silicates
- C04B 2237/343: Alumina or aluminates
- C04B 2237/368: Silicon nitride
- C04B 2237/704: of one or more of the ceramic layers or articles
- C04B 2237/708: of one or more of the interlayers
- C04B 2237/72: Forming laminates or joined articles comprising at least two interlayers directly next to each other
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A ceramic plate structure includes a first transmittance-enhancing film layer disposed between a substrate and a first binding film layer, a conductive film layer disposed between the first binding film layer and a second binding film layer, and a second transmittance-enhancing film layer disposed between the second binding film layer and a ceramic layer. The ceramic layer renders the ceramic plate structure satisfactory in terms of transmittance gain, thermal conductivity coefficient, electrical insulation, rigidity, resistance to wear and tear, and resistance to wind erosion of the ceramic plate structure. The ceramic plate structure is suitable for use with touch panels to therefore enhance the cost-effectiveness of the manufacturing process of touch panels by cutting its material costs, reducing its power consumption, and shortening its production cycle. Accordingly, the anticipated benefits and objectives of the ceramic plate structure are attained.

## Claims

### Claim 1

A ceramic plate structure, comprising:
a substrate, a first transmittance-enhancing film layer, a first binding film layer, a conductive film layer, a second binding film layer, a second transmittance-enhancing film layer, and a ceramic layer;
wherein the substrate is a glass plate;
wherein the first transmittance-enhancing film layer is disposed between the substrate and the first binding film layer and adapted to provide transmittance gain to the ceramic plate structure;
wherein the conductive film layer is disposed on and attached to the first binding film layer and corresponds in position to the first transmittance-enhancing film layer to effectuate electrical conduction of the ceramic plate structure;
wherein the second binding film layer is disposed on and attached to the conductive film layer and corresponds in position to the first binding film layer;
wherein the second transmittance-enhancing film layer is disposed on and attached to the second binding film layer and corresponds in position to the conductive film layer to provide transmittance gain to the ceramic plate structure;
wherein the ceramic layer is disposed on and attached to the second transmittance-enhancing film layer and corresponds in position to the second binding film layer to augment transmittance gain, thermal conductivity coefficient, electrical insulation, rigidity, resistance to wear and tear, and resistance to wind erosion of the ceramic plate structure; and
wherein the ceramic layer features a polycrystalline transparent structure and comprises aluminum oxide.

### Claim 2 (depends on 1)

The ceramic plate structure of claim 1, wherein the first transmittance-enhancing film layer and the second transmittance-enhancing film layer each comprise one of a composite of silicon oxide, silicon oxide and silicon nitride and a composite of silicon oxide, silicon nitride, and silicon oxide.

### Claim 3 (depends on 2)

The ceramic plate structure of claim 2, wherein the first binding film layer and the second binding film layer each comprise one of an optically clear adhesive and a liquid optically clear adhesive.

### Claim 4 (depends on 3)

The ceramic plate structure of claim 3, further comprising an antifouling layer disposed on and attached to the ceramic layer and corresponding in position to the second transmittance-enhancing film layer, wherein the antifouling layer comprises one of organic fluoride and inorganic coating to render the ceramic plate structure less susceptible to fingerprints and smears.

### Claim 5 (depends on 4)

The ceramic plate structure of claim 4, wherein the antifouling layer comprises one of nano silicon dioxide, nano titanium dioxide, and nano aluminum oxide.

### Claim 6 (depends on 2)

The ceramic plate structure of claim 2, further comprising an antifouling layer disposed on and attached to the ceramic layer and corresponding in position to the second transmittance-enhancing film layer, wherein the antifouling layer comprises one of organic fluoride and inorganic coating to render the ceramic plate structure less susceptible to fingerprints and smears.

### Claim 7 (depends on 6)

The ceramic plate structure of claim 6, wherein the antifouling layer comprises one of nano silicon dioxide, nano titanium dioxide, and nano aluminum oxide.

### Claim 8 (depends on 1)

The ceramic plate structure of claim 1, wherein the first binding film layer and the second binding film layer each comprise one of an optically clear adhesive and a liquid optically clear adhesive.

### Claim 9 (depends on 8)

The ceramic plate structure of claim 8, further comprising an antifouling layer disposed on and attached to the ceramic layer and corresponding in position to the second transmittance-enhancing film layer, wherein the antifouling layer comprises one of organic fluoride and inorganic coating to render the ceramic plate structure less susceptible to fingerprints and smears.

### Claim 10 (depends on 9)

The ceramic plate structure of claim 9, wherein the antifouling layer comprises one of nano silicon dioxide, nano titanium dioxide, and nano aluminum oxide.

### Claim 11 (depends on 1)

The ceramic plate structure of claim 1, further comprising an antifouling layer disposed on and attached to the ceramic layer and corresponding in position to the second transmittance-enhancing film layer, wherein the antifouling layer comprises one of organic fluoride and inorganic coating to render the ceramic plate structure less susceptible to fingerprints and smears.

### Claim 12 (depends on 11)

The ceramic plate structure of claim 11, wherein the antifouling layer comprises one of nano silicon dioxide, nano titanium dioxide, and nano aluminum oxide.