# US 9,218,954 B2 · Defect capping method for reduced defect density epitaxial articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,218,954 B2
- Document ID: US9218954B2
- Status: Granted
- Kind: B2
- Application number: 13/872,821
- Filed: 2013-04-29
- Published: 2013-09-12
- Granted: 2015-12-22
- Earliest claimed: 2010-03-12
- Assignees: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Applicants: Sinmat, Inc.
- Inventors: Rajiv K. Singh; Arul Chakkaravarthi Arjunan
- Web page: https://patentgrep.com/patent/US9218954B2

## CPC

- H10P 90/12: {Preparing bulk and homogeneous wafers}
- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 29/36: Carbides
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/276: {Lateral overgrowth}
- H10P 14/2901: {Materials}
- H10P 14/2904: {Silicon carbide}
- H10P 14/2908: {Nitrides}
- H10P 14/3202: {Materials thereof}
- H10P 14/3216: {Nitrides}
- H10P 14/3402: {characterised by the chemical composition}
- H10P 14/3408: {Silicon carbide}
- H10P 14/3416: {Nitrides}
- H10P 50/644: {Anisotropic liquid etching (H10P50/61 takes precedence)}
- H10P 50/648: {Anisotropic liquid etching}
- H10P 52/402: {of semiconductor materials}
- H10D 62/8325: {Silicon carbide}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for forming an epitaxial layer on a substrate surface having crystalline defect or amorphous regions and crystalline non-defect regions includes preferential polishing or etching the crystalline defect or amorphous regions relative to the crystalline non-defect regions to form a decorated substrate surface having surface recess regions. A capping layer is deposited on the decorated substrate surface to cover the crystalline non-defect regions and to at least partially fill the surface recess regions. The capping layer is patterned by removing the capping layer over the crystalline non-defect regions to form exposed non-defect regions while retaining the capping layer in at least a portion of the surface recess regions. Selective epitaxy is then used to form the epitaxial layer, wherein the capping layer in the surface recess regions restricts epitaxial growth of the epitaxial layer over the surface recess regions.

## Claims

### Claim 1

A method for forming an epitaxial layer on a substrate comprising a substrate surface having crystalline defect or amorphous regions and crystalline non-defect regions, comprising:
preferential polishing said crystalline defect or amorphous regions relative to said crystalline non-defect regions using chemical mechanical polishing (CMP) to form a decorated substrate surface comprising surface recess regions;
depositing a capping layer on said decorated substrate surface to cover said crystalline non-defect regions and to at least partially fill said surface recess regions;
patterning said capping layer by removing said capping layer over said crystalline non-defect regions to form exposed non-defect regions while retaining said capping layer in at least a portion of said surface recess regions, and
selective epitaxy to form said epitaxial layer, wherein said capping layer in said surface recess regions restricts epitaxial growth of said epitaxial layer over said surface recess regions.

### Claim 2 (depends on 1)

The method of claim 1, further comprising chemical mechanical polishing (CMP) after said selective epitaxy to a top surface of said epitaxial layer to provide atomic level smoothness.

### Claim 3 (depends on 1)

The method of claim 1, further comprising chemical mechanical polishing (CMP) said decorated substrate surface to provide an atomic scale finish before said depositing.

### Claim 4 (depends on 1)

The method of claim 1, wherein said depositing comprises a blanket deposition, and said capping layer provides a masking function for restricting said epitaxial growth of said epitaxial layer over said surface recess regions.

### Claim 5 (depends on 4)

The method of claim 4, wherein said depositing comprises physical, chemical or vapor deposition, or electrochemical or electroless deposition.

### Claim 6 (depends on 1)

The method of claim 1, wherein said patterning comprises chemical mechanical polishing (CMP).

### Claim 7 (depends on 1)

The method of claim 1, wherein said epitaxial layer is a homoepitaxial layer.

### Claim 8 (depends on 1)

The method of claim 1 wherein said epitaxial layer is a heteroepitaxial layer.

### Claim 9 (depends on 1)

The method of claim 1, wherein said substrate comprises silicon having a 10 Angstrom to 1 mm thick first Group III-nitride semiconductor layer thereon and said epitaxial layer comprises a second Group III-nitride semiconductor layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein said substrate surface comprises SiC or AlN.

### Claim 11 (depends on 1)

The method of claim 1, wherein an average crystalline defect density throughout said epitaxial layer is ≦108 cm−2.

### Claim 12 (depends on 1)

The method of claim 1, wherein said epitaxial layer comprises a group IV, II-VI, III-V material, or a binary ternary or quaternary alloy of said group II-VI material or said III-V material.

### Claim 13 (depends on 1)

The method of claim 1, wherein a surface of said epitaxial layer has an atomic scale finish with a surface roughness less than 5 Å.

### Claim 14 (depends on 1)

The method of claim 1, wherein said CMP comprises using a slurry including a mixture of chemicals and particles.