Abstract
A method includes casting a friction reducing layer on a carrier, and casting an adhesive layer overlying the friction reducing layer to form a multilayer cast film. The method further includes laminating the multilayer cast film to the load bearing substrate with the load bearing substrate to form a composite and shaping the composite. The load bearing substrate is closer to the adhesive layer than to the friction reducing layer.
Claims12
A method comprising
- casting first and second friction reducing layers on first and second sides of a polyimide carrier;
- casting first and second intermediate layers adjacent to and in direct contact with the first and second friction reducing layers, wherein the first and second intermediate layers consists of
- a fluoropolymer, the fluoropolymer selected from polytetrafluoroethylene (PTFE), fluorinated ethylene-propylene (FEP), polyvinylidenfluoride (PVDF), polychlorotrifluoroethylene (PCTFE), ethylene chlorotrifluoroethylene (ECTFE), ethylene tetrafluoroethylene (ETFE), perfluoroalkoxypolymer (PFA), and any combination thereof, and
- a filler, the filler selected from the group consisting of a friction reducing filler, a pigment, a scent producing filler, a noise producing filler, and a combination thereof;
- casting first and second adhesive layers, wherein the first and second adhesive layers includes a melt-processible fluoropolymer, the first and second adhesive layers overlying the first and second intermediate layers to form first and second multilayer cast films;
- layering first and second load bearing substrates from a feed spool, the first and second load bearing substrates comprising a continuous metal sheet, onto first and second multilayer cast films;
- laminating the first and second multilayer cast films to first and second load bearing substrates with each load bearing substrate closer to the corresponding adhesive layer than to the corresponding friction reducing layer to form first and second composites, wherein a thickness of each of the load bearing substrates is greater than a thickness of each of first and second adhesive layers and the thickness of each of the load bearing substrates is greater than a thickness of each of the first and second friction reducing layers;
- removing the polyimide carrier from the first and second multilayer cast films and the loadbearing substrates;
- and
- applying a first and second coating layers onto the first and second friction reducing layers, wherein the first and second coating layers are opposite to the loadbearing substrate, wherein the first and second coating layers comprise a lubricant;
- and
- shaping the composites.
9 more elements
A method comprising
- casting first and second friction reducing layers on first and second sides of a polyimide carrier;
- casting first and second adhesive layers to form first and second multilayer cast films, the first and second adhesive layers overlying the first and second friction reducing layers, wherein the first and second adhesive layers includes a melt-processible fluoropolymer consisting of
- an ethylene tetrafluoroethylene copolymer (ETFE), a fluorinated ethylene propylene copolymer (FEP), a perfluoroalkoxy (PFA), or any combination thereof, and
- a functional group selected from —C═O, —C—O—R, —COH, —COOH, —COOR, —CF2=CF—OR, or any combination thereof, where R is a cyclic or linear organic group containing between 1 and 20 carbon atoms;
- layering first and second load bearing substrates from a feed spool, the first and second load bearing substrates comprising a continuous metal sheet, onto first and second multilayer cast film;
- laminating the first and second multilayer cast films to first and second load bearing substrates with each load bearing substrate closer to the corresponding adhesive layer than to the corresponding friction reducing layer to form first and second composites, wherein a thickness of each of the load bearing substrates is greater than a thickness of each of first and second adhesive layers and the thickness of each of the load bearing substrates is greater than a thickness of each of the first and second friction reducing layers;
- removing the polyimide carrier from the first and second multilayer cast films and the loadbearing substrates;
- and
- applying a first and second coating layers onto the first and second friction reducing layers, wherein the first and second coating layers are opposite to the loadbearing substrate, wherein the first and second coating layers comprise a lubricant;
- and
- shaping the composites.
8 more elements