A conductive paste containing a conductive powder (A) having a dendrite structure, a vinyl chloride-vinyl acetate resin (B), a polyester resin and/or polyurethane resin (C), a blocked isocyanate (D) blocked with an active methylene compound, and an organic solvent (E),
- wherein
- the resin (C) has a glass transition temperature of −50° C. to 20° C.,
- a sum of amounts of the resin (C) is 50 to 400 parts by weight relative to 100 parts by weight of the resin (B), and
- a sum of amounts of the resin (B), the resin (C) component, and the blocked isocyanate (D) is 10 to 60 parts by weight relative to 100 parts by weight of the conductive powder (A).