Back to results
US 8,920,520 B2Granted
Methods of preparing polysaccharide sheets for esterification
AssigneeCelanese Acetate LLC
InventorsThomas S. Garrett, Lawton E. Kizer, Henry P. Stogner
Life of this patent
Estimating the term…
Abstract
Processing of cellulose, and more particularly, fiber opening and downstream processing and chemistry are provided. A process includes moistening a cellulose sheet stock to a water content in a range from about 20% to about 50%, attriting the moistened cellulose sheet to a wet pulp, flash drying the wet pulp to a floccule of cellulose having a moisture content from about 4% to about 8%, and esterifying the floccule of cellulose to provide a cellulose ester product.
Claims23
A process comprising:
- moistening a cellulose sheet stock to a water content in a range from about 20% to about 50%;
- attriting the moistened cellulose sheet to a wet pulp;
- flash drying said wet pulp to a floccule of cellulose having a moisture content from about 4% to about 8%, wherein flash drying is conducted in a flash dryer having an inlet temperature of about 105° C. to about 200° C. and an outlet temperature of about 60° C. to about 130° C.;
- and
- esterifying said floccule of cellulose to provide a cellulose ester product.
2 more elements
A process comprising:
- (a) moistening a cellulose sheet stock to a water content in a range from about 20% to about 50%;
- (b) attriting the moistened cellulose sheet to a wet pulp;
- (c) flash drying said wet pulp to a floccule of cellulose having a moisture content from about 5% to about 8%, wherein flash drying is conducted in a flash dryer having an inlet temperature of about 105° C. to about 200° C. and an outlet temperature of about 60° C. to about 130° C.;
- (d) esterifying said floccule of cellulose to provide a cellulose ester product;
- and
- (e) forming a fiber tow from said cellulose ester product.
3 more elements
A process comprising:
- moistening a cellulose sheet stock to a water content of the cellulose sheet stock is about 20% to about 50%;
- attriting the moistened cellulose sheet to a wet pulp, wherein a water content of the wet pulp is about 20% to about 50%;
- delivering the wet pulp to a flash dryer;
- flash drying said wet pulp to a floccule of cellulose, wherein a water content of the flocculate of cellulose is about 4% to about 8%, and wherein the flash dryer has an inlet temperature of about 105° C. to about 200° C. and an outlet temperature of about 60° C. to about 130° C.;
- and
- esterifying said floccule of cellulose to provide a cellulose ester product.
3 more elements