Rubber asphalt and preparation method thereof
OwnerQiqiang Zhouinventor
Life of this patent
Estimating the term…
Loading patent…
OwnerQiqiang Zhouinventor
Estimating the term…
A rubber asphalt and a preparation method thereof are disclosed. The rubber asphalt comprises matrix asphalt and rubber powder modifier in a ratio of 4:1-4, wherein the rubber powder modifier comprises waste tire rubber powder and hexanediol in a ratio of 94-96:6-4. The method comprises the following steps: mixing the hexanediol with the waste tire rubber powder according to the ratio and stirring and wetting to obtain the rubber powder modifier; placing the matrix asphalt into a reaction kettle and heating to 90-170° C.; adding the rubber powder modifier into the reaction kettle according to the ratio; and raising the temperature to 190-210° C. under the stirring state to obtain the rubber asphalt. The rubber asphalt has an extensibility of 13-19 cm at 5° C., a penetration of 68-75 at 25° C. and a softening point of 53-90° C. The asphalt-aggregate ratio of a mixed material on the subsequent work section can be reduced to 6-8 from 8-10. The rubber asphalt can be used for producing a mixture for highway construction and preventing water and leakage of roofing and tunnel.
A method of preparing rubber asphalt, comprising:
A method of preparing rubber asphalt, comprising:
Dependencies are inferred from the claim text.