Method and a device for the refining of glass
AssigneeSchott AG
InventorsErich Rodek, Wolfgang Schmid-Bauer, Hilgegard Römer, Günter Weidmann, Werner Kiefer
Life of this patent
Estimating the term…
Abstract
A device for the refining of a glass melt at high temperatures according to the skull pot principle is provided. The device includes a skull crucible having walls that are constructed from a plurality of pipes, a high-frequency coil for coupling electrical energy into the contents of the skull crucible, and an inlet and an outlet of the skull crucible being arranged in a melt surface region of the glass melt, wherein the inlet and the outlet are essentially arranged lying opposite one another.
Claims3
A method for the refining of a glass melt, which is heated by irradiation of high-frequency energy, by high temperatures in a core of a skull crucible, the method comprising:
- introducing the glass melt through an inlet in an upper region of the skull crucible;
- coupling the high-frequency energy into the glass melt in the skull crucible via a high frequency coil to heat the glass melt to a temperature of between 1,750 to 3,000° C.;
- refining the glass melt in the skull crucible at a temperature between 1,750 to 3,000° C.;
- discharging the glass melt through an outlet in the upper region of the skull crucible, the outlet being at a place essentially lying opposite the inlet;
- and
- preventing a short-circuit flow of the glass melt between the inlet and the outlet by increasing, via the high frequency coil, a temperature difference between the glass melt flowing into the skull crucible through the inlet and the glass melt in the core of the skull crucible.
A method for the refining of a glass melt, which is heated by irradiation of high-frequency energy, by high temperatures in a core of a skull crucible, the method comprising:
- introducing the glass melt through an inlet in an upper region of the skull crucible;
- coupling the high-frequency energy into the glass melt in the skull crucible to heat the glass melt to a temperature of between 1,750 to 3,000° C.;
- refining the glass melt in the skull crucible at a temperature between 1,750 to 3,000° C.;
- discharging the glass melt through an outlet in the upper region of the skull crucible, the outlet being at a place essentially lying opposite the inlet;
- and
- preventing a short-circuit flow of the glass melt between the inlet and the outlet by increasing a temperature difference between the glass melt flowing into the skull crucible through the inlet and the glass melt in the core of the skull crucible by coupling the high-frequency energy into the glass melt in the core of the skull crucible.
A method for the refining of a glass melt, which is heated by irradiation of high-frequency energy, by high temperatures in a core of a skull crucible, the method comprising:
- introducing a crude glass melt through an inlet in an upper region of the skull crucible, the skull crucible having an outlet in the upper region lying essentially opposite the inlet;
- preventing a short-circuit flow of the crude glass melt from the inlet to the outlet by increasing a temperature difference between the crude glass melt flowing into the upper region and the glass melt in the core of the skull crucible, wherein the preventing step comprises coupling the high-frequency energy into the skull crucible to refine the crude glass melt into a refined glass melt at a temperature between 1,750 to 3,000° C.;
- and
- discharging the refined glass melt through the outlet.
Dependencies are inferred from the claim text.