Process for the preparation of a polyolefin polymer with improved wax deposition
AssigneeBasell Polyolefine GmbH
InventorsGerhardus Meier, Reinhard Kuehl, Harald Prang, Michael Aulbach
Life of this patent
Estimating the term…
Loading patent…
AssigneeBasell Polyolefine GmbH
InventorsGerhardus Meier, Reinhard Kuehl, Harald Prang, Michael Aulbach
Estimating the term…
Process for the preparation of a polyolefin polymer by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1 to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising a) withdrawing a suspension of solid polyolefin particles in a suspension medium from the polymerization reactor, wherein the suspension has a temperature of from 65° C. to 120° C.; b) feeding the suspension withdrawn from the polymerization reactor to a moderating vessel; c) keeping the suspension in the moderating vessel at a temperature of from 60° C. to 85° C. for a time sufficiently long that the mean residence time of the suspension in the moderating vessel is at least 5 min; d) withdrawing suspension from the moderating vessel; e) cooling the suspension withdrawn from the moderating vessel to a temperature of from 20° C. to 55° C.; and f) mechanically separating the solid polyolefin particles from the liquid suspension medium, and method for controlling the content of hydrocarbons with from 14 to 300 carbon atoms in a polyolefin polymer prepared by polymerizing one or more olefin monomers in suspension.
A process for the preparation of a polyolefin polymer by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising
A method for controlling the content of hydrocarbons with from 14 to 300 carbon atoms in a polyolefin polymer prepared by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1 to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising
Dependencies are inferred from the claim text.