Aqueous copolymer dispersion and coating composition
AssigneeRohm and Haas Company
InventorsHuiling Yang, Xiangting Dong, Siyuan Jiang, Qianqian Li
Life of this patent
Estimating the term…
Abstract
The present invention relates to an aqueous copolymer dispersion comprising an emulsion copolymer and two hydrophobic aromatic ketones, wherein the aromatic ketones are, based on the dry weight of the copolymer, from 0.1 to 3 wt % benzophenone and from 0.1 to 4 wt % a benzophenone derivative; wherein the dispersion comprises 0 or less than 0.1 wt % hydrophilic aromatic ketone. The copolymer dispersion is suitable for preparation of aqueous coating compositions which yields a relatively hard surface to provide not only short term but also long term dirt pick up resistance effects, after exposure to ultraviolet radiation.
Claims15
An aqueous copolymer dispersion comprising:
- an emulsion copolymer, wherein the emulsion copolymer comprises, as a copolymerized unit, based on the dry weight of the copolymer, at least 90 wt % an ethylenically unsaturated nonionic monomer, and up to 10 wt % an ethylenically unsaturated stabilizer monomer, and wherein the emulsion copolymer is not a multi-stage emulsion copolymer comprising at least two stages;
- and
- two hydrophobic aromatic ketones, wherein the aromatic ketones are, based on the dry weight of the copolymer, from 0.6 to 3 wt % benzophenone and from 0.5 to 3 wt % of a benzophenone derivative;
- and
- wherein the dispersion comprises 0 or less than 0.1 wt % hydrophilic aromatic ketone.
An aqueous coating composition comprising:
- an emulsion copolymer, two hydrophobic aromatic ketones, and a coating adjuvant,
- wherein the aromatic ketones are, based on the dry weight of the copolymer, from 0.6 to 3 wt % benzophenone and from 0.5 to 3 wt % of a benzophenone derivative;
- wherein the emulsion copolymer comprises, as a copolymerized unit, based on the dry weight of the copolymer, at least 90 wt % an ethylenically unsaturated nonionic monomer, and up to 10 wt % an ethylenically unsaturated stabilizer monomer, and wherein the emulsion copolymer is not a multi-stage emulsion copolymer comprising at least two stages;
- and
- wherein the coating composition comprises 0 or less than 0.1 wt % hydrophilic aromatic ketone.
An aqueous copolymer dispersion comprising:
- an emulsion copolymer;
- and
- two hydrophobic aromatic ketones, wherein the aromatic ketones are, based on the dry weight of the copolymer, from 0.6 to 3 wt % benzophenone and from 0.5 to 3 wt % of a benzophenone derivative, wherein the dispersion comprises 0 or less than 0.1 wt % hydrophilic aromatic ketone, and
- wherein a coating film made from the aqueous copolymer dispersion exhibits a CIE delta b of less than or equal to 0.10 after:
- exposure for 7 days to 23° C. and 50% relative humidity;
- exposure for 3 days to 40° C.;
- exposure for 4 hours to UV light having an irradiance of 0.77 W/m2/nm in a QUV Weathering Tester, Model QUV, with UVA-340 nm lamps;
- application of Premix GB (China national standard coal ash slurry in water) to the coating and exposure for 2 hours to 23° C. and 50% relative humidity followed by a rinse with deionized water;
- and
- repeat of the coal slurry application and rinse four times.