# US 8,785,874 B2 · Ionization window

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,785,874 B2
- Document ID: US8785874B2
- Status: Granted
- Kind: B2
- Application number: 13/976,657
- Filed: 2010-12-30
- Published: 2013-10-17
- Granted: 2014-07-22
- Earliest claimed: 2010-12-30
- Assignees: Walter Kidde Portable Equipment, Inc.
- Applicants: Sameh Dardona; Timothy N. Obee; Marcin Piech; Joseph V. Mantese
- Inventors: Sameh Dardona; Timothy N. Obee; Marcin Piech; Joseph V. Mantese
- Web page: https://patentgrep.com/patent/US8785874B2

## CPC

- G01T 7/00: Details of radiation-measuring instruments
- G01N 27/64: using wave or particle radiation to ionise a gas, e.g. in an ionisation chamber
- G01T 1/185: with ionisation chamber arrangements
- H01J 5/18: Windows permeable to X-rays, gamma-rays, or particles
- H01J 33/04: Windows
- H01J 2235/18: Windows, e.g. for X-ray transmission
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

An exemplary ionization window assembly includes a support layer having a thickness between a first side and a second side. There is at least one opening in the support layer extending between the first and second sides. The opening has a first width dimension near the first side of the support layer and a second, larger width dimension near the second side of the support layer. A window layer is supported on the second side of the support layer. The window layer extends across the opening to allow ionizing radiation to pass through the opening in a direction from the first side toward the second side.

## Claims

### Claim 1

An ionization window assembly, comprising:
a support layer having a thickness between a first side and a second side, at least one opening in the support layer extending between the first and second sides, the at least one opening having a first width dimension near the first side of the support layer and a second, larger width dimension near the second side of the support layer; and
a window layer supported on the second side of the support layer, the window layer extending across the at least one opening to allow ionizing radiation to pass through the at least one opening in a direction from the first side toward the second side.

### Claim 2 (depends on 1)

The assembly of claim 1, wherein the window layer comprises at least one of a silicon oxide, a silicon nitride or a silicon oxynitride.

### Claim 3 (depends on 1)

The assembly of claim 1, wherein the window layer comprises ultra-nanocrystalline diamond.

### Claim 4 (depends on 1)

The assembly of claim 1, wherein the support layer comprises silicon.

### Claim 5 (depends on 4)

The assembly of claim 4, wherein the support layer comprises a silicon-on-insulator wafer having silicon on opposite sides of an oxide.

### Claim 6 (depends on 1)

The assembly of claim 1, wherein the support layer has a first thickness in the direction from the first side toward the second side and the window layer has a second, smaller thickness in the direction from the first side toward the second side.

### Claim 7 (depends on 1)

The assembly of claim 1, wherein the at least one opening has a progressively increasing width from the first side to the second side and wherein the second width is the largest width of the opening.

### Claim 8 (depends on 1)

The assembly of claim 1, wherein the support layer comprises a plurality of support members and a plurality of openings between support members, each support member having side surfaces facing toward an adjacent one of the openings, the side surfaces being aligned at an oblique angle relative to the first side of the support layer.

### Claim 9 (depends on 8)

The assembly of claim 8, wherein at least some of the support members have a cross-section that is shaped as an isosceles trapezoid.

### Claim 10 (depends on 8)

The assembly of claim 8, wherein the window layer comprises a continuous coating over the first side of the support members, the side surfaces of the support members and across the openings.

### Claim 11 (depends on 1)

The assembly of claim 1, wherein the at least one opening has a first cross-sectional area near the first side and a second, larger cross-sectional area near the second side.

### Claim 12 (depends on 1)

The assembly of claim 1, wherein the window layer maintains a desired pressure difference between a pressure on a first surface of the window layer near the first side and a second surface of the window layer that is closer to the second side than the first surface.

### Claim 13 (depends on 1)

The assembly of claim 1, wherein the window layer has a first surface aligned with the first side of the support layer.

### Claim 14 (depends on 1)

The assembly of claim 1, wherein the window layer comprises at least one of silicon dioxide, carbon, nitride, aluminum, titanium, beryllium, aluminum oxide, magnesium oxide, silicon carbide, silicon carbonitride, or beryllium oxide.

### Claim 15

A detector, comprising:
a pressurized chamber;
a source of ionizing radiation at least partially in the chamber;
an ionization window on at least one side of the chamber that allows the ionizing radiation to exit the chamber, the ionization window including
a support layer having a thickness between a first side and a second side, at least one opening in the support layer extending between the first and second sides, the at least one opening having a first width dimension near the first side of the support layer and a second, larger width dimension near the second side of the support layer; and
a window layer supported on the second side of the support layer, the window layer extending across the at least one opening to allow the ionizing radiation to pass through the at least one opening in a direction from the first side toward the second side and to exit the chamber.

### Claim 16 (depends on 15)

The detector of claim 15, wherein the window layer comprises at least one of a silicon oxide, a silicon nitride, a silicon oxynitride or ultra-nanocrystalline diamond.

### Claim 17 (depends on 15)

The detector of claim 15, wherein the support layer comprises a silicon-on-insulator wafer having silicon on opposite sides of an oxide.

### Claim 18 (depends on 15)

The detector of claim 15, wherein the support layer has a first thickness in a direction that the electrons exit the chamber and the window layer has a second, smaller thickness in the direction.

### Claim 19 (depends on 15)

The detector of claim 15, wherein the at least one opening has a progressively increasing width from the first side to the second side and wherein the second width is the largest width dimension of the opening.

### Claim 20 (depends on 15)

The detector of claim 15, wherein the support layer comprises a plurality of support members and a plurality of openings between support members, each support member having side surfaces facing toward an adjacent one of the openings, the side surfaces being aligned at an oblique angle relative to the first side of the support layer.

### Claim 21 (depends on 20)

The detector of claim 20, wherein at least some of the support members have a cross-section that is shaped as an isosceles trapezoid.

### Claim 22 (depends on 20)

The detector of claim 20, wherein the window layer comprises a continuous coating over the first side of the support members, the side surfaces of the support members and across the openings.

### Claim 23 (depends on 15)

The detector of claim 15, wherein the at least one opening has a first cross-sectional area near the first side and a second, larger cross-sectional area near the second side.

### Claim 24 (depends on 15)

The detector of claim 15, wherein the window layer maintains a desired pressure difference between a pressure on a first surface of the window layer near the first side and a second surface of the window layer that is closer to the second side than the first surface.

### Claim 25 (depends on 15)

The detector of claim 15, wherein the window layer has a first surface aligned with the first side of the support layer.

### Claim 26

A method of making an ionization window, comprising the steps of:
establishing a plurality of support members on a wafer with a plurality of spaces between the support members;
establishing a first width near one end of each the spaces;
establishing a second, larger width near a second end of each of the spaces;
coating the support members and the wafer in the spaces with a continuous ionization window layer; and
removing material of the wafer adjacent the ionization window layer at the spaces between the support members to leave only the ionization window layer across the openings near the one end of the spaces.

### Claim 27 (depends on 26)

The method of claim 26, comprising shaping the support members to have an isosceles trapezoid shaped cross section.