# US 8,784,716 B2 · Method and apparatus for longitudinal orientation of thermoplastic film material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,784,716 B2
- Document ID: US8784716B2
- Status: Granted
- Kind: B2
- Application number: 12/740,203
- Filed: 2008-10-30
- Published: 2011-04-28
- Granted: 2014-07-22
- Earliest claimed: 2007-10-31
- Applicants: Ole-Bendt Rasmussen
- Inventors: Ole-Bendt Rasmussen
- Web page: https://patentgrep.com/patent/US8784716B2

## CPC

- B29C 55/18: by squeezing between surfaces, e.g. rollers
- B29C 55/065: {in several stretching steps}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

Method and apparatus for longitudinal orientation of thermoplastic film material (4) comprises a width-reduction zone upstream of the longitudinal stretching zone, through which the width of the film is gradually reduced so as to allow longitudinal stretching without necking. The width-reduction zone comprises at least one, preferably several, pairs of pleating rollers (16, 17) comprising intermeshing grooves or discs for pleating the material, the length of said width reduction zone preferably being less than 3 times the original width of the film. The width-reducing zone has upstream (14) and downstream (15) rollers or roller assemblies, with curved axes and optionally also conveyor belts for providing smooth width reduction. Longitudinal stretching is preferably between at least two, and preferably more than two, pairs of stretching rollers (9, 10, 11, 12) which are relatively close together. The pleats may be provided in several stages with increasing pleats per stage, while guiding means preferably lay all the pleats to one side. The method allows achievement of high tensile strength, yield point, resistance to tear propagation and puncture resistance, especially for polyethylene and polypropylene films.

## Claims

### Claim 1

A process of supplying a thermoplastic polymer film with longitudinal orientation comprising the steps of:
reducing a width of a film in a reduction zone comprising at least one pair of curved mutually intermeshing grooved rollers or curved intermeshing sets of discs to form a regular pattern of longitudinally extending pleats, where the width reduction occurs gradually within the reduction zone, where a length of the reduction zone is no shorter than half of an original width of the film, and where the reduction zone length is limited by an upstream roller or roller assembly and a downstream roller or roller assembly installed having varying directions of their respective axis of rotation from a central direction at the middle of the film forming an angle of 90° with a machine direction and gradually changing towards edges of the film to forward the film in a converging manner within the reduction zone, and
solid state stretching in one or more short zones between and/or on two or more stretching rollers or bars, where the stretching zones are adapted to fully straighten out the pleats by the inherent tendency in the polymer material making up the film to contract transversely, while being stretched longitudinally.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the film mainly comprises HDPE, PP or blends of these polymers.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the reduction zone is no longer than 3 times the original film width.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the film is in the form of a lay-flat tube.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the stretching takes place at a temperature no higher than 60° C.

### Claim 6 (depends on 1)

The process according to claim 1, wherein the downstream roller or roller assembly comprises at least one banana roller with its convex side pointing towards the upstream roller or roller assembly.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the downstream roller assembly comprises many short rollers mounted individually and together forming part of the circumference of a polygon for the desired pattern of pleating.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the film while leaving the last roller or roller assembly of the downstream part of the reduction zone is guided in a direction deviating no more than 10° from being perpendicular to its movement within the reduction zone.

### Claim 9 (depends on 1)

The process according to claim 1, wherein the upstream roller or roller assembly comprises a banana roller or several parallel banana rollers with the concave side pointing towards the downstream roller or roller assembly.

### Claim 10 (depends on 9)

The process according to claim 9, wherein the banana roller or rollers form arcs the tangents of which at any location are perpendicular to the film tension created by the downstream roller or roller assembly.

### Claim 11 (depends on 1)

The process according to claim 1, wherein the film is forwarded towards the first upstream roller in a direction deviating no more than 10° from being perpendicular to its movement within the width-reduction zone.

### Claim 12 (depends on 1)

The process according to claim 1, wherein the upstream roller or roller assembly is a crown-shaped roller or an assembly of short rollers which together form a crown-shape on a straight shaft, the short rollers being connected with a common shaft through bearings to be able to rotate independently of each other.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the gradual reduction of the width within the reduction zone is assisted by mutually intermeshing discs, in the form of pairs of grooved banana rollers installed between the upstream roller or roller assembly and the downstream roller or roller assembly.

### Claim 14 (depends on 13)

The process according to claim 13, wherein the banana roller comprises discs of different external diameters in alternating succession or of short roller segments supplied with grooves, the discs or roller segments being mounted on a bent shaft.

### Claim 15 (depends on 13)

The process according to claim 13, wherein some or all of the intermeshing discs are individually adjustable in their intermeshing.

### Claim 16 (depends on 13)

The process according to claim 13, wherein the gradual reduction of width is assisted by at least one pair of mutually intermeshing grooved banana rollers, wherein the intermeshing is variable by means of an adjustable force acting to move the two rollers together.

### Claim 17 (depends on 1)

The process according to claim 1, wherein the gradual reduction of width within the reduction zone is assisted by a set of narrow conveyor belts following and guiding the film through at least a part of this zone, the two sets of narrow belts gradually intermeshing more and more with each other during the conveying advancement in the zone.

### Claim 18 (depends on 1)

The process according to claim 1, wherein the pleating is carried out in several steps with several sets of grooved rollers, the pitch of the grooves in the sets being mutually different to develop from a coarser to a finer pleating.

### Claim 19 (depends on 1)

The process according to claim 1, wherein when the film, is in a pleated state before being permanently elongated, passes over a smooth banana roller or a smooth straight roller, there are guiding means acting immediately upstream of and in close proximity to this roller, to counter act the roller's random rising of the pleating.

### Claim 20 (depends on 19)

The process according to claim 19, wherein these means are screwed tracks adapted to fold all pleats over to the same side.

### Claim 21 (depends on 1)

The process according to claim 1, wherein the reduction zone is no longer than 2 times the original film width.

### Claim 22 (depends on 1)

The process according to claim 1, wherein the reduction zone is no more than equal to the original film width.

### Claim 23 (depends on 1)

The process according to claim 1, wherein the reduction zone comprises at least two pair of curved mutually intermeshing grooved rollers or curved intermeshing sets of discs.

### Claim 24 (depends on 23)

The process according to claim 23, wherein the second pair of rollers or discs are located half way between the first pair of rollers or discs and the downstream roller or roller assembly.

### Claim 25 (depends on 1)

The process according to claim 1, wherein the reduction zone comprises at least three pair of curved mutually intermeshing grooved rollers or curved intermeshing sets of discs.

### Claim 26 (depends on 25)

The process according to claim 25, wherein the second pair of rollers or discs are located half way between the first pair of rollers or discs and the downstream roller or roller assembly.

### Claim 27 (depends on 26)

The process according to claim 26, wherein the third pair of rollers or discs are located half way between the second pair of rollers or discs and the downstream roller or roller assembly.