# US 8,739,408 B2 · Shape memory material packer for subterranean use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,739,408 B2
- Document ID: US8739408B2
- Status: Granted
- Kind: B2
- Application number: 12/985,962
- Filed: 2011-01-06
- Published: 2012-07-12
- Granted: 2014-06-03
- Earliest claimed: 2011-01-06
- Assignees: Baker Hughes Incorporated
- Applicants: Ping Duan; Steve Rosenblatt
- Inventors: Ping Duan; Steve Rosenblatt
- Web page: https://patentgrep.com/patent/US8739408B2

## CPC

- E21B 33/1208: {characterised by the construction of the sealing or packing means (E21B33/1277 takes precedence)}
- E21B 23/06: for setting packers
- E21B 33/128: with a member expanded radially by axial pressure (E21B33/122, E21B33/124 take precedence)
- Y10T 29/49428: Gas and water specific plumbing component making
- Y10T 29/49895: Associating parts by use of aligning means [e.g., use of a drift pin or a "fixture"]
- Y10T 29/49938: Radially expanding part in cavity, aperture, or hollow body
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A shape memory polymer is initially fabricated to a size where its peripheral dimension will be at least as large as the borehole wall in which it is to be deployed. After the initial manufacturing the material temperature is elevated above the transition temperature and the material is stretched on a mandrel to retain its inside dimension as its outside dimension is reduced to size that will allow running the seal to a desired subterranean location without failing the material during the stretching. The material is allowed to cool below the transition temperature to hold the new shape. The material on the mandrel is then secured to a tubular string and delivered to the desired location. Wellbore fluid at given temperature raises the material again above the transition temperature, which causes the material to revert to its originally manufactured shape.

## Claims

### Claim 1

A method of using a seal for a subterranean location having a borehole dimension, comprising:
providing a shape memory element to a manufactured peripheral dimension at least as large as the borehole dimension and extending for at least a portion of the length of said element;
reducing said peripheral dimension to less than the borehole dimension before running in;
running in said element on a mandrel to the subterranean location;
allowing said element to revert to said manufactured peripheral dimension to seal at the subterranean location;
biasing said element with a biasing member supported on a mandrel and contacting said shape memory element, after said allowing said element to revert to said manufactured peripheral dimension, to enhance the seal at the subterranean location.

### Claim 2 (depends on 1)

The method of claim 1, comprising:
raising the temperature of said element to above its transition temperature before said reducing.

### Claim 3 (depends on 2)

The method of claim 2, comprising:
inserting said mandrel through a bore in said element before said raising the temperature of said element.

### Claim 4 (depends on 3)

The method of claim 3, comprising:
providing an axial tensile force to said element when said element is mounted to said mandrel to reduce said manufactured peripheral dimension.

### Claim 5 (depends on 1)

The method of claim 1, comprising:
inserting a mandrel through a bore in said element before said reducing said peripheral dimension.

### Claim 6 (depends on 5)

The method of claim 5, comprising:
providing an interference fit in said bore of said element for said inserting.

### Claim 7 (depends on 1)

The method of claim 1, comprising:
making said manufactured peripheral dimension larger than the subterranean location borehole dimension.

### Claim 8

A method of using a seal for a subterranean location having a borehole dimension, comprising:
providing a shape memory element to a manufactured peripheral dimension at least as large as the borehole dimension and extending for at least a portion of the length of said element;
reducing said peripheral dimension to less than the borehole dimension before running in;
running in said element on a mandrel to the subterranean location;
allowing said element to revert to said manufactured peripheral dimension to seal at the subterranean location;
raising the temperature of said element to above its transition temperature before said reducing;
inserting a mandrel through a bore in said element before said raising the temperature of said element;
providing an axial tensile force to said element when said element is mounted to said mandrel to reduce said manufactured peripheral dimension;
mounting a biasing member on said mandrel before providing said axial tensile force.

### Claim 9 (depends on 8)

The method of claim 8, comprising:
locating said biasing member outside said element adjacent at least one of opposed ends of said element.

### Claim 10 (depends on 8)

The method of claim 8, comprising:
locating said biasing member between said element and said mandrel.

### Claim 11 (depends on 8)

The method of claim 8, comprising:
providing a preload force on said element from said biasing member after the temperature of said element goes below the transition temperature said axial tensile force is released.

### Claim 12 (depends on 8)

The method of claim 8, comprising:
using a constant manufactured peripheral dimension for the length of said element.

### Claim 13 (depends on 8)

The method of claim 8, comprising:
using a variable manufactured peripheral dimension for said element that has a larger dimension between ends thereof

### Claim 14 (depends on 13)

The method of claim 13, comprising:
reducing said larger dimension during said reducing.

### Claim 15 (depends on 13)

The method of claim 13, comprising:
reducing the entirety of said variable manufactured peripheral dimension during said reducing.

### Claim 16

A method of using a seal for a subterranean location having a borehole dimension, comprising:
providing a shape memory element to a manufactured peripheral dimension at least as large as the borehole dimension and extending for at least a portion of the length of said element;
reducing said peripheral dimension to less than the borehole dimension before running in;
running in said element on a mandrel to the subterranean location;
allowing said element to revert to said manufactured peripheral dimension to seal at the subterranean location;
raising the temperature of said element to above its transition temperature before said reducing;
inserting a mandrel through a bore in said element before said raising the temperature of said element;
providing an axial tensile force to said element when said element is mounted to said mandrel to reduce said manufactured peripheral dimension;
mounting a biasing member on said mandrel before providing said axial tensile force;
locating said biasing member within said element.

### Claim 17

A method of using a seal for a subterranean location having a borehole dimension, comprising:
providing a shale memory element to a manufactured peripheral dimension at least as large as the borehole dimension and extending for at least a portion of the length of said element;
reducing said peripheral dimension to less than the borehole dimension before running in;
running in said element on a mandrel to the subterranean location;
allowing said element to revert to said manufactured peripheral dimension to seal at the subterranean location;
raising the temperature of said element to above its transition temperature before said reducing;
inserting a mandrel through a bore in said element before said raising the temperature of said element;
providing an axial tensile force to said element when said element is mounted to said mandrel to reduce said manufactured peripheral dimension;
mounting a biasing member on said mandrel before providing said axial tensile force;
manufacturing said biasing member from a shape memory polymer.

### Claim 18 (depends on 17)

The method of claim 17, comprising:
raising the temperature of said biasing member to above its transition temperature and reshaping said biasing member when above said transition temperature before mounting said biasing member to said mandrel;
applying a force to said element at the subterranean location due to reverting of said biasing member to said manufactured shape when the temperature of said biasing member is again raised above the transition temperature.

### Claim 19

A method of using a seal for a subterranean location having a borehole dimension, comprising:
providing a shape memory element to a manufactured peripheral dimension at least as large as the borehole dimension and extending for at least a portion of the length of said element;
reducing said peripheral dimension to less than the borehole dimension before running in;
running in said element on a mandrel to the subterranean location;
allowing said element to revert to said manufactured peripheral dimension to seal at the subterranean location;
using a variable manufactured peripheral dimension for said element that has a larger dimension between ends thereof;
inserting a mandrel in an interference fit in a bore through said element before said reducing;
locating a biasing member in an annular space between said mandrel and said larger dimension or in the element itself at said larger dimension.

### Claim 20 (depends on 19)

The method of claim 19, comprising:
using a shape memory alloy leaf spring as said biasing element;
initially reforming said shape memory alloy leaf spring to a flat condition when holding it above its transition temperature prior to mounting said leaf spring in said annular space or in the element itself and before said reducing.