Hydrogenated norbornene-based ring-opening polymerization polymer, resin composition, and molded object
AssigneeZeon Corporation
InventorsNobuhiro Kudo, Koichi Ikeda
Life of this patent
Estimating the term…
Loading patent…
AssigneeZeon Corporation
InventorsNobuhiro Kudo, Koichi Ikeda
Estimating the term…
A hydrogenated norbornene ring-open polymer obtained by hydrogenating 80% or more of main-chain carbon-carbon double bonds of a ring-open polymer obtained by ring-opening polymerization of 2-norbornene. The hydrogenated norbornene ring-open polymer has a weight average molecular weight determined by gel permeation chromatography (GPC) of 50,000 to 200,000, a molecular weight distribution of 1.5 to 10.0, and a melting point of 110 to 145° C. A hydrogenated norbornene ring-open polymer obtained by hydrogenating 80% or more of carbon-carbon double bonds of a ring-open polymer obtained by ring-opening copolymerization of 2-norbornene and a substituent-containing norbornene monomer, wherein the proportion of a repeating unit (A) derived from the 2-norbornene with respect to all repeating units is 90 to 99 wt % and the proportion of a repeating unit (B) derived from the substituent-containing norbornene monomer with respect to all repeating units is 1 to 10 wt %. A resin composition and a molding material.
A medical supply packing material having at least one resin layer which is a layer of a hydrogenated norbornene ring-open polymer obtained by hydrogenating 80% or more of carbon-carbon double bonds of a ring-open homopolymer of 2-norbornene or a polymer which is obtained by ring-opening polymerization of a monomer mixture of 2-norbornene and a substituent-containing norbornene monomer, the proportion of a repeating unit (A) derived from the 2-norbornene with respect to all repeating units being 90 to 100 wt % and the proportion of a repeating unit (B) derived from the substituent-containing norbornene monomer with respect to all repeating units being 0 to 10 wt %, and the hydrogenated norbornene ring-open polymer having a melting point of 110 to 145° C.
Dependencies are inferred from the claim text.