Concrete with a low clinker content
AssigneeLafarge
InventorsArnaud Schwartzentruber, Myléne Martin, Philippe Benard, Serge Sabio
Life of this patent
Estimating the term…
Loading patent…
AssigneeLafarge
InventorsArnaud Schwartzentruber, Myléne Martin, Philippe Benard, Serge Sabio
Estimating the term…
A dry binder premix includes, in mass proportions: Portland clinker having a Blaine specific surface area comprised from 4500 to 9500 cm2/g, the minimum quantity of the clinker by mass percentage relative to the total mass of the premix being determined according to: [−6.10−3×BSSk]+75, in which BSSk is the Blaine specific surface area of the clinker given in cm2/g; fly ash; an alkali sulphate; one source of SO3; complementary materials having a Dv90 less than or equal to 200 μm selected from limestone powders, calcined shale, metakaolins, siliceous fillers, silica powders, pozzolans, slags, fly ash and mixtures thereof. A quantity of clinker+the quantity of fly ash is greater than or equal to 75% by mass percentage relative to the total mass of the premix and a total quantity of clinker in the premix is less than 60% by mass percentage relative to the total mass of the premix.
A dry binder premix comprising, in mass proportions:
Dependencies are inferred from the claim text.